Main
Brand
Germany
1.0000 - 1.0799 (Non-alloy Steels)
1.0300 - 1.0399 (Steels with Average C < 0,12% or Rm < 400 MPa)
1.0304 (C9D)
Classification
Country
Section
Category
Germany
Non-alloy Steels
Steels with Average C < 0,12% or Rm < 400 MPa
Chemical composition
Standard
Fe, %
Si, %
Mn, %
Cr, %
Cu, %
Ni, %
P, %
C, %
S, %
Mo, %
EN 10016-2
> 97.99
< 0.3
< 0.6
< 0.2
< 0.35
< 0.25
< 0.035
< 0.16
< 0.035
< 0.08
Information on suppliers
Wish to advertise here?
Properties
Property
According to EN 10016-2 note Mechanical properties: by agreement
Density: 7.86 g / cm3
Analogues
Germany
CIS, Russia, Ukraine
USA
D 8-2
10
SAE 1010
Standards
Standard
Description
EN 10016-2
DIN EN 10016-2:1995
DIN EN ISO 16120-2:2011
DIN EN ISO 16120-2:2017
Description of chemical elements
Element
Units of measurement
Description
Fe
%
Iron
Si
%
Silicon
Mn
%
Manganese
Cr
%
Chrome
Cu
%
Copper
Ni
%
Nickel
P
%
Phosphorus
C
%
Carbon
S
%
Sulfur
Mo
%
Molybdenum
Aloro
EN
Ago
Forward
Search
Brand
Brands by region
CIS, Russia, Ukraine
CIS, Russia, Ukraine
Aluminum, aluminum alloys
Brass (copper-zinc alloy)
Bronze
Cast iron
Copper, copper alloys
Corrosion-resistant alloys and steels
Electrical steel
Ferroalloys
Heat resistant steels and alloys
Magnesium
Materials for welding and soldering
Metals and alloys
Nickel, nickel alloys
Powder metallurgy
Precious metals
Precision alloys
Rare earth metals and their alloys
Refractory metals, carbide
Steels and alloys for castings
Steels for special purposes
Structural steel
Tin, lead, babity
Titanium, titanium alloys
Tool steel
Germany
Germany
0.0000 - 0.9999
1.0000 - 1.0799
1.0800 - 1.0999
1.1000 - 1.1999
1.2000 - 1.2999
1.3000 - 1.3999
1.4000 - 1.4999
1.5000 - 1.5999
1.6000 - 1.6999
1.7000 - 1.7999
1.8000 - 1.8999
1.9000 - 1.9999
2.0000 - 2.9999
3.0000 - 3.9999
4.0000 - 4.9999
5.0000 - 5.9999
9.0000 - 9.9999
USA
USA
A00001 - A99999
C00001 - C99999
D00001 - D99999
E00001 - E99999
F00001 - F99999
G00001 - G99999
J00001 - J99999
K00001 - K99999
L00001 - L99999
M00001 - M99999
N00001 - N99999
P00001 - P99999
R00001 - R99999
S00001 - S99999
T00001 - T99999
W00001 - W99999
Z00001 - Z99999
Grades Comparison
Calculator steel
Purchase
Language —
English
Select the language
Deutsch
English
Русский
А−
А
А+