Main
Brand
Germany
1.1000 - 1.1999 (Non-alloy Special Steels)
1.1100 - 1.1199 (Structural Pressure Vessel and Engineering Steels with C < 0,5%)
1.1104 (P275NL2)
Particularly strong at low temperatures
Classification
Country
Section
Category
Germany
Non-alloy Special Steels
Structural Pressure Vessel and Engineering Steels with C < 0,5%
Chemical composition
Standard
Fe, %
Si, %
Mn, %
Cr, %
Ti, %
Cu, %
Ni, %
V, %
Al, %
P, %
C, %
S, %
Nb, %
Nd, %
Mo, %
N, %
96.518–99.2
< 0.4
0.8–1.5
< 0.3
< 0.03
< 0.3
< 0.5
< 0.05
< 0.02
< 0.02
< 0.16
< 0.01
< 0.05
< 0.05
< 0.08
< 0.012
Information on suppliers
Wish to advertise here?
Mechanical properties at 20 °C
Rolling
Standard
Size, mm
Tension
Classifiers
$$\sigma _{U}$$
,
$$MPa$$
$$\sigma_{Y}$$
,
$$MPa$$
$$\epsilon_L$$
, %
$$KV_{L}$$
,
$$J$$
$$KV_{T}$$
,
$$J$$
Treatment
< 60
normalization
390–510
24
40–42
27
60–100
normalization
370–490
235
100–150
normalization
360–480
225
150–250
normalization
350–470
215
< 16
normalization
275
16–40
normalization
265
40–60
normalization
255
60–250
normalization
23
Description of chemical elements
Element
Units of measurement
Description
Fe
%
Iron
Si
%
Silicon
Mn
%
Manganese
Cr
%
Chrome
Ti
%
Titan
Cu
%
Copper
Ni
%
Nickel
V
%
Vanadium
Al
%
Aluminium
P
%
Phosphorus
C
%
Carbon
S
%
Sulfur
Nb
%
Niobium
Nd
%
Neodymium
Mo
%
Molybdenum
N
%
Nitrogen
Description of mechanical properties
Parameter
Units of measurement
Description
$$\sigma_{Y}$$
$$MPa$$
Yield strength
$$\sigma _{U}$$
$$MPa$$
Ultimate tensile strength
$$\epsilon_L$$
%
Elongation at break (longitudinal)
$$KV_{L}$$
$$J$$
Impact energy (longitudinal)
$$KV_{T}$$
$$J$$
Impact energy (transverse)
Aloro
EN
Ago
Forward
Search
Brand
Brands by region
CIS, Russia, Ukraine
CIS, Russia, Ukraine
Aluminum, aluminum alloys
Brass (copper-zinc alloy)
Bronze
Cast iron
Copper, copper alloys
Corrosion-resistant alloys and steels
Electrical steel
Ferroalloys
Heat resistant steels and alloys
Magnesium
Materials for welding and soldering
Metals and alloys
Nickel, nickel alloys
Powder metallurgy
Precious metals
Precision alloys
Rare earth metals and their alloys
Refractory metals, carbide
Steels and alloys for castings
Steels for special purposes
Structural steel
Tin, lead, babity
Titanium, titanium alloys
Tool steel
Germany
Germany
0.0000 - 0.9999
1.0000 - 1.0799
1.0800 - 1.0999
1.1000 - 1.1999
1.2000 - 1.2999
1.3000 - 1.3999
1.4000 - 1.4999
1.5000 - 1.5999
1.6000 - 1.6999
1.7000 - 1.7999
1.8000 - 1.8999
1.9000 - 1.9999
2.0000 - 2.9999
3.0000 - 3.9999
4.0000 - 4.9999
5.0000 - 5.9999
9.0000 - 9.9999
USA
USA
A00001 - A99999
C00001 - C99999
D00001 - D99999
E00001 - E99999
F00001 - F99999
G00001 - G99999
J00001 - J99999
K00001 - K99999
L00001 - L99999
M00001 - M99999
N00001 - N99999
P00001 - P99999
R00001 - R99999
S00001 - S99999
T00001 - T99999
W00001 - W99999
Z00001 - Z99999
Grades Comparison
Calculator steel
Purchase
Language —
English
Select the language
Deutsch
English
Русский
А−
А
А+