1.1105 (S315NL1)

Particularly strong at low temperatures

Classification

Country Section Category
Germany Non-alloy Special Steels Structural Pressure Vessel and Engineering Steels with C < 0,5%

Chemical composition

Standard Fe, % Si, % Mn, % Cu, % Al, % P, % C, % S, %
97.63–99.3 < 0.45 0.7–1.5 < 0.2 < 0.02 < 0.025 < 0.16 < 0.015

Information on suppliers

Mechanical properties at 20 °C

Rolling Standard Size, mm Tension Classifiers \sigma _{U}, MPa \epsilon_L, % R_{eH}, MPa Treatment
< 70 440–560 > 23 > 295
70–85 430–550 > 23 > 285
85–100 420–540 > 23 > 275
100–125 410–530 > 23 > 265
125–150 400–520 > 23 > 255
150–250 390–520 > 23 > 245

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cu % Copper
Al % Aluminium
P % Phosphorus
C % Carbon
S % Sulfur

Description of mechanical properties

Parameter Units of measurement Description
\sigma _{U} MPa Ultimate tensile strength
\epsilon_L % Elongation at break (longitudinal)
R_{eH} MPa Upper yield point