Main
Brand
Germany
1.8000 - 1.8999 (Structural, Pressure Vessel and Engineering Steels)
1.8900 - 1.8999 (High Strength Weldable Steels not Intended for Heat Treatment by User)
1.8915 (P460NL1)
Durable at low temperatures
Classification
Country
Section
Category
Country
Section
Category
Germany
Structural, Pressure Vessel and Engineering Steels
High Strength Weldable Steels not Intended for Heat Treatment by User
Chemical composition
Standard
Fe, %
Si, %
Mn, %
Cr, %
Ti, %
Cu, %
Ni, %
V, %
Al, %
P, %
C, %
S, %
Nb, %
Mo, %
N, %
Standard
Fe, %
Si, %
Mn, %
Cr, %
Ti, %
Cu, %
Ni, %
V, %
Al, %
P, %
C, %
S, %
Nb, %
Mo, %
N, %
95.235–98.9
< 0.6
1.1–1.7
< 0.3
< 0.03
< 0.7
< 0.8
< 0.2
< 0.02
< 0.025
< 0.2
< 0.015
< 0.05
< 0.1
< 0.025
Information on suppliers
Wish to advertise here?
Mechanical properties at 20 °C
Rolling
Standard
Size, mm
Tension
Classifiers
\sigma _{U}
,
MPa
\sigma_{Y}
,
MPa
\epsilon_L
, %
KV_{L}
,
J
KV_{T}
,
J
Treatment
Rolling
Standard
Size, mm
Tension
Classifiers
\sigma _{U}
,
MPa
\sigma_{Y}
,
MPa
\epsilon_L
, %
KV_{L}
,
J
KV_{T}
,
J
Treatment
< 16
normalization
560–730
460
17–19
30
27
16–60
normalization
570–720
60–100
normalization
540–710
400
16–40
normalization
445
40–60
normalization
430
Description of chemical elements
Element
Units of measurement
Description
Element
Units of measurement
Description
Fe
%
Iron
Si
%
Silicon
Mn
%
Manganese
Cr
%
Chrome
Ti
%
Titan
Cu
%
Copper
Ni
%
Nickel
V
%
Vanadium
Al
%
Aluminium
P
%
Phosphorus
C
%
Carbon
S
%
Sulfur
Nb
%
Niobium
Mo
%
Molybdenum
N
%
Nitrogen
Description of mechanical properties
Parameter
Units of measurement
Description
Parameter
Units of measurement
Description
\sigma_{Y}
MPa
Yield strength
\sigma _{U}
MPa
Ultimate tensile strength
\epsilon_L
%
Elongation at break (longitudinal)
KV_{L}
J
Impact energy (longitudinal)
KV_{T}
J
Impact energy (transverse)
Aloro
EN
Ago
Forward
Search
Brand
Brands by region
CIS, Russia, Ukraine
CIS, Russia, Ukraine
Aluminum, aluminum alloys
Brass (copper-zinc alloy)
Bronze
Cast iron
Copper, copper alloys
Corrosion-resistant alloys and steels
Electrical steel
Ferroalloys
Heat resistant steels and alloys
Magnesium
Materials for welding and soldering
Metals and alloys
Nickel, nickel alloys
Powder metallurgy
Precious metals
Precision alloys
Rare earth metals and their alloys
Refractory metals, carbide
Steels and alloys for castings
Steels for special purposes
Structural steel
Tin, lead, babity
Titanium, titanium alloys
Tool steel
Germany
Germany
0.0000 - 0.9999
1.0000 - 1.0799
1.0800 - 1.0999
1.1000 - 1.1999
1.2000 - 1.2999
1.3000 - 1.3999
1.4000 - 1.4999
1.5000 - 1.5999
1.6000 - 1.6999
1.7000 - 1.7999
1.8000 - 1.8999
1.9000 - 1.9999
2.0000 - 2.9999
3.0000 - 3.9999
4.0000 - 4.9999
5.0000 - 5.9999
9.0000 - 9.9999
USA
USA
A00001 - A99999
C00001 - C99999
D00001 - D99999
E00001 - E99999
F00001 - F99999
G00001 - G99999
J00001 - J99999
K00001 - K99999
L00001 - L99999
M00001 - M99999
N00001 - N99999
P00001 - P99999
R00001 - R99999
S00001 - S99999
T00001 - T99999
W00001 - W99999
Z00001 - Z99999
Grades Comparison
Calculator steel
Purchase
Language —
English
Select the language
Deutsch
English
Русский
А−
А
А+