10880 (E10)
Weldability: without restrictions. Hardness 10880 hot-rolled Grade (GOST 11036−75) HB 10 -1 = 131 MPa
for use in magnetic circuits of electric devices and instruments
Weldability: without restrictions. Hardness 10880 hot-rolled Grade (GOST 11036−75) HB 10 -1 = 131 MPa
for use in magnetic circuits of electric devices and instruments
Standard | Fe, % | Si, % | Mn, % | Cu, % | P, % | C, % | S, % |
---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Mn, % | Cu, % | P, % | C, % | S, % |
GOST 11036-75 | > 99.015 | < 0.3 | < 0.3 | < 0.3 | < 0.02 | < 0.035 | < 0.03 |
Rolling | Standard | Size, mm | Tension | Classifiers | \sigma _{U}, MPa | \epsilon_L, % | \psi, % | Treatment |
---|---|---|---|---|---|---|---|---|
Rolling | Standard | Size, mm | Tension | Classifiers | \sigma _{U}, MPa | \epsilon_L, % | \psi, % | Treatment |
Metal rolling | GOST 11036-75 | hot rolling | 270 | 24 | 60 | |||
Metal rolling | GOST 11036-75 | calibrated | 350 | 4 |
Rolling | Dimensions, mm | H_c, A/m | \mu_{max}, MH/m | B_{500}, T | B_{1000}, T | B_{2500}, T | B_{5000}, T | B_{10000}, T | B_{30000}, T |
---|---|---|---|---|---|---|---|---|---|
Rolling | Dimensions, mm | H_c, A/m | \mu_{max}, MH/m | B_{500}, T | B_{1000}, T | B_{2500}, T | B_{5000}, T | B_{10000}, T | B_{30000}, T |
Sheet | 0.1–3.9 | 80 | 5 | 1.38 | 1.5 | 1.62 | 1.71 | 1.81 | 2.05 |
Grade | 80 | 1.36 | 1.47 | 1.57 |
Rolling | Standard | Classifiers | Value, HBW |
---|---|---|---|
Rolling | Standard | Classifiers | Value, HBW |
Metal rolling | GOST 11036-75 | hot rolling | 1310 |
Standard | Description |
---|---|
Standard | Description |
GOST 11036-75 | |
TU 14-1-3606-83 |
Parameter | Units of measurement | Description |
---|---|---|
Parameter | Units of measurement | Description |
Dimensions | mm | |
H_c | A/m | Magnetic coercivity (not more) |
\mu_{max} | MH/m | Magnetic permeability (not more) |
B_{500} | T | Magnetic induction (not less) in a magnetic field while magnetic field strength is 500 A/m |
B_{1000} | T | Magnetic induction (not less) in a magnetic field while magnetic field strength is 1000 A/m |
B_{2500} | T | Magnetic induction (not less) in a magnetic field while magnetic field strength is 2500 A/m |
B_{5000} | T | Magnetic induction (not less) in a magnetic field while magnetic field strength is 5000 A/m |
B_{10000} | T | Magnetic induction (not less) in a magnetic field while magnetic field strength is 10000 A/m |
B_{30000} | T | Magnetic induction (not less) in a magnetic field while magnetic field strength is 30000 A/m |
Parameter | Units of measurement | Description |
---|---|---|
Parameter | Units of measurement | Description |
no limits | Welding is performed without heating and without subsequent heat treatment | |
Boundedly welded | Welding is possible with heating up to 100–120 °C and subsequent heat treatment | |
Difficult to weld | For obtaining quality welded joints, additional operations are required: heating up to 200–300 °C for welding, heat treatment after welding — annealing | |
Not applicable for welded structures |