Alloy aluminum AK10Su

Chemical composition


Fe Si Mn Ni Al Cu Mg Zn Sb Impurities
up to 1.2 9 — 11 0.3 — 0.6 up to 0.5 83.1 — 90.6 up to 1.8 0.1 — 0.5 up to 1.8 0.1 — 0.25 total 4.8
Note: Al is the base; the percentage of Al is given approximately
Note: In pigs, the magnesium content is 0.15 — 0.55%

For the manufacture of ingots and various shaped castings by injection molding. Technical requirements GOST 1583−93 Cast aluminum alloys. Technical conditions GOST 1583−93 Cast aluminum alloys. Technical conditions GOST R 55375−12 Primary aluminum and alloys based on it. Stamps

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Foundry aluminum alloys

Chemical composition

Standard Fe, % Si, % Mg, % Mn, % Cu, % Zn, % Ni, % Sb, % Al, %
GOST 1583-93 < 1.2 9–11 0.1–0.5 0.3–0.6 < 1.8 < 1.8 < 0.5 0.1–0.25 82.35–90.5

Information on suppliers

Brinell hardness number

Rolling Standard Classifiers Value, HBW
Alloy 70

Standards

Standard Description
GOST 1583-93

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mg % Magnesium
Mn % Manganese
Cu % Copper
Zn % Zinc
Ni % Nickel
Sb % Antimony
Al % Aluminium