Alloy aluminum AK12MMgN

Chemical composition

Fe Si Mn Ni Cr Ti Al Cu Pb Mg Zn Sn Impurities
up to 0.7 11 — 13 up to 0.2 0.8 — 1.3 up to 0.2 up to 0.2 82.64 — 86.6 0.8 — 1.5 until 0.05 0.8 — 1.3 up to 0.2 up to 0.01 total 1.1
Note: Al is the base; the percentage of Al is given approximately
Note: In pigs, the magnesium content is 0.85 — 1.35%

Cast aluminum alloy of the Al-Si-Cu system (silumin). Designed for the manufacture of ingots and shaped castings in the chill mold; castings of diesel pistons. Technical requirements — according to GOST 1583−93.

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Foundry aluminum alloys

Information on suppliers

Standards

Standard Description
GOST 1583-93