Alloy aluminum AK12och (SIL-00)

Chemical composition

Fe Si Mn Ni Cr Ti Al Cu Pb Mg Zn Sn Impurities
up to 0.7 11 — 13 up to 0.2 0.8 — 1.3 up to 0.2 up to 0.2 82.64 — 86.6 0.8 — 1.5 until 0.05 0.8 — 1.3 up to 0.2 up to 0.01 total 1.1
Note: Al is the base; the percentage of Al is given approximately
Note: In pigs, the magnesium content is 0.85 — 1.35%

Silumin in pigs is used in mechanical engineering and for the manufacture of food products. Technical requirements GOST 1583−93 Cast aluminum alloys. Technical conditions GOST R 55375−12 Primary aluminum and alloys based on it. Stamps

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Foundry aluminum alloys

Chemical composition

Standard Fe, % Si, % Ca, % Mn, % Ti, % Cu, % Zn, % Al, %
GOST 1583-93 < 0.2 10–13 < 0.04 < 0.03 < 0.03 < 0.02 < 0.04 86.64–90

Information on suppliers

Standards

Standard Description
GOST 1583-93

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Ca % Calcium
Mn % Manganese
Ti % Titan
Cu % Copper
Zn % Zinc
Al % Aluminium