Alloy aluminum AK12zh (SIL-2)

Chemical composition

Fe Si Mn Ti Al Cu Ca Zn
up to 0.7 10 — 13 up to 0.5 up to 0.2 85.29 — 90 until 0.03 up to 0.2 until 0.08
Note: Al is the base; the percentage of Al is given approximately
Note: By agreement with the consumer, iron content is allowed up to 0.9%, manganese — up to 0.8%, titanium — up to 0.25%

Alloy of the aluminum-manganese-silicon system (silumin). It is produced in ingots, used in mechanical engineering and for the manufacture of food products. Technical requirements — according to GOST 1583−93

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Foundry aluminum alloys

Chemical composition

Standard Fe, % Si, % Ca, % Mn, % Ti, % Cu, % Zn, % Al, %
GOST 1583-93 < 0.7 10–13 < 0.2 < 0.5 < 0.2 < 0.03 < 0.08 85.29–90

Information on suppliers

Analogues

Germany USA
3.2585 4047

Standards

Standard Description
GOST 1583-93

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Ca % Calcium
Mn % Manganese
Ti % Titan
Cu % Copper
Zn % Zinc
Al % Aluminium