Alloy aluminum AK4M4 (AL15V)

  • Chemical composition
    Al Aluminum Rest
    Fe Iron <1.3
    Si Silicon 3.0 — 5.0
    Mg Magnesium <0.5
    Mn Manganese 0.2 — 0.6
    Cu Copper 3.5 — 5.0
    Ni Nickel <0.5
    Zn Zinc <2.0
    Ot Total impurities <4.1
    Analogs in Germany
  • GK-AlSi6Cu4 DIN 1725 Part 2

    3.2151.02 DIN 1725 Part 2

    G-AlSi6Cu4 DIN 1725 Part 2

    3.2151.01 DIN 1725 Part 2

    GB-AlSi6Cu4 DIN 1725 Part 5

    3.2155 DIN 1725 Part 5

    225 DIN 1725 Part 5

    EN AB-45000 DIN EN 1676: 2010

    EN AB-AlSi6Cu4 DIN EN 1676: 2010

    EN AB-45000 DIN EN 1676: 2019

    EN AB-AlSi6Cu4 DIN EN 1676: 2019

    EN AC-45000 DIN EN 1706: 2013

    EN AC-45400 DIN EN 1706: 2013

    EN AC-AlSi6Cu4 DIN EN 1706: 2013

    EN AC-AlSi5Cu3 DIN EN 1706: 2013

    EN AC-45000 DIN EN 1706: 2019

    EN AC-AlSi6Cu4 DIN EN 1706: 2019

    EN AC-45400 DIN EN 1706: 2019

    EN AC-AlSi5Cu3 DIN EN 1706: 2019

    225 VDS

  • Analogs in the USA
  • 319.0 ANSI

    EN AC-45000 ASME SB / EN 1706

    EN AC-45400 ASME SB / EN 1706

    EN AC-AlSi6Cu4 ASME SB / EN 1706

    EN AC-AlSi5Cu3 ASME SB / EN 1706

    SB 108 (319.0) ASME SB108

    SB 108 (A03190) ASME SB108

    B 108 (319.0) ASTM B108

    B 108 (A03190) ASTM B108

    B 26 (319.0) ASTM B26

    B 26 (A03190) ASTM B26

    B 275 (A 03190) ASTM B275

    B 969 (319.0) ASTM B969

    319.0 ASTM B969

    J452 (326) SAE J452

    A03190 UNS

    319.0 Included in 2 standards

    319.0 Included in 4 standards

For the manufacture of shaped castings. Technical requirements — according to GOST 2685−75 Cast aluminum alloys. Stamps

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Foundry aluminum alloys

Chemical composition

Standard Fe, % Si, % Mg, % Mn, % Cu, % Zn, % Ni, % Al, %
GOST 1583-93 < 1.3 3–5 < 0.5 0.2–0.6 3.5–5 < 2 < 0.5 85.3–93.3

Information on suppliers

Analogues

Germany USA
GK-AlSi6Cu4 319

Standards

Standard Description
GOST 1583-93

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mg % Magnesium
Mn % Manganese
Cu % Copper
Zn % Zinc
Ni % Nickel
Al % Aluminium