Alloy aluminum AK5M

Chemical composition according to GOST 1583−93

Fe Si Mn Al Cu Be Mg Zn Sn Impurities -
up to 1.5 4.5 — 5.5 up to 0.5 90.7 — 94.15 1 — 1.5 up to 0.1 0.35 — 0.6 up to 0.3 up to 0.01 total 1.7 Ti + Zr <0.15
Note: Al is the base; the percentage of Al is given approximately
Note: In pigs, the magnesium content is 0.4 — 0.65%

For the manufacture of shaped castings. It is delivered in ingots of pyramids, granules, grains. technical requirements — in accordance with GOST 1583−93 Cast aluminum alloys. Technical conditions GOST R 55375−12 Primary aluminum and alloys based on it. Stamps

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Foundry aluminum alloys

Information on suppliers

Analogues

USA
360

Standards

Standard Description
GOST 1583-93