BrO10S12N3

for the manufacture of parts operating friction

Classification

Country Section Category
CIS, Russia, Ukraine Bronze Tin cast bronze

Information on suppliers

Mechanical properties at 20 °C

Rolling Standard Size, mm Tension Classifiers $$\sigma _{U}$$, $$MPa$$ $$\sigma_{0.5}$$, $$MPa$$ Treatment
Casting in chill mold 245 5

Brinell hardness number

Rolling Standard Classifiers Value, HBW
Alloy 73.5

Coefficients of Friction

coefficient of friction with lubrication coefficient of friction without lubrication
0.02 0.38

Standards

Standard Description
GOST 613-79

Description of mechanical properties

Parameter Units of measurement Description
$$\sigma_{0.5}$$ $$MPa$$ Tensile stress required to produce a total elongation of 0.5%
$$\sigma _{U}$$ $$MPa$$ Ultimate tensile strength