DI-57 (X5S4V2F2NM)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | P, % | C, % | S, % | Mo, % | W, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 82.63–86.37 | 3.35–3.95 | 0.3–0.5 | 4.2–5 | < 0.03 | < 0.3 | 0.3–0.6 | 1.9–2.4 | < 0.03 | 0.98–1.13 | < 0.03 | 0.8–1.1 | 1.8–2.3 |
Information on suppliers
Eigenschaften
| Eigenschaft |
|---|
| Berechnete Eigenschaften Dichte: 7,8 g / cm3 |
| Beachten Sie gestanzten Stahl |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| W | % | Tungsten |