EI110

Classification

Country Section Category
CIS, Russia, Ukraine Corrosion-resistant alloys and steels Corrosion-resistant alloys

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % P, % C, % S, %
95.59–96.41 1.3–1.6 0.9–1.1 1.2–1.4 < 0.03 0.19–0.25 < 0.03

Information on suppliers

Properties

Property
Calculated Properties Density: 7.76 g / cm3

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cr % Chrome
P % Phosphorus
C % Carbon
S % Sulfur