EI295

Classification

Country Section Category
CIS, Russia, Ukraine Corrosion-resistant alloys and steels Corrosion-resistant alloys

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Ni, % P, % C, % S, %
72.77–76.3 1.8–2.6 0.3–0.6 16.5–18 5–5.8 < 0.03 0.1–0.17 < 0.03

Information on suppliers

Properties

Property
Calculated Properties Density: 7.68 g / cm3