XH55VMTKYUA
Classification
Chemical composition
Standard | Fe, % | Si, % | B, % | Sn, % | Bi, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | Sb, % | V, % | Al, % | As, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Sn, % | Bi, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | Sb, % | V, % | Al, % | As, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
TU 14-1-402-72 | < 5 | < 0.5 | < 0.02 | < 0.001 | < 0.0001 | < 0.5 | 12–16 | 9–12 | 1.4–2 | < 0.07 | 45.7419–65.22 | < 0.001 | 0.2–0.8 | 3.6–4.5 | < 0.001 | < 0.02 | < 0.015 | 0.08–0.12 | < 0.01 | < 0.2 | 4–6 | 4.5–6.5 |
Information on suppliers
Analogues
Standards
Standard | Description |
---|---|
Standard | Description |
TU 14-1-402-72 |
Description of chemical elements
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Sn | % | Tin |
Bi | % | Bismuth |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
Sb | % | Antimony |
V | % | Vanadium |
Al | % | Aluminium |
As | % | Arsenic |
Ce | % | Cerium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Mo | % | Molybdenum |
W | % | Tungsten |