- Main
- Brand
- CIS, Russia, Ukraine
- Corrosion-resistant alloys and steels
- Corrosion-resistant heat-resistant steel
XH60KMVTYUB-ID
Classification
Chemical composition
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Zr, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % | Hf, % | Ge, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Ni, % | Zr, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % | Hf, % | Ge, % |
| TU 14-131-369-77 | < 0.5 | < 0.5 | < 0.015 | < 0.5 | 15–16.5 | 8–10 | 1.3–1.8 | 52.81–61.05 | < 0.015 | 4.75–5.15 | < 0.01 | < 0.015 | < 0.06 | < 0.015 | 1.2–1.6 | 2.2–3 | 6.5–7.2 | < 0.3 | < 0.01 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| Standard | Description |
| TU 14-131-369-77 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Element | Units of measurement | Description |
| Fe | % | Iron |
| Si | % | Silicon |
| B | % | Bor |
| Mn | % | Manganese |
| Co | % | Cobalt |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| Zr | % | Zirconium |
| Al | % | Aluminium |
| Ce | % | Cerium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |
| W | % | Tungsten |
| Hf | % | Hafnium |
| Ge | % | Germanium |