Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | B, % | Mn, % | Co, % | Cr, % | Ti, % | Cu, % | Ni, % | V, % | Al, % | Ce, % | P, % | C, % | S, % | Nb, % | Mo, % | W, % |
GOST 23705 - 79 | < 4 | < 0.6 | < 0.01 | < 0.5 | < 0.5 | 17–20 | 2.2–2.8 | < 0.07 | 59.505–71.8 | < 0.2 | 1–1.5 | < 0.01 | < 0.015 | < 0.08 | < 0.01 | < 0.2 | 4–5 | 4–5 |
Standard | Description |
---|---|
Standard | Description |
GOST 23705 - 79 | |
TU 14-1-1214-75 | |
TU 14-1-588-73 | |
TU 14-1-592-73 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Si | % | Silicon |
B | % | Bor |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Ti | % | Titan |
Cu | % | Copper |
Ni | % | Nickel |
V | % | Vanadium |
Al | % | Aluminium |
Ce | % | Cerium |
P | % | Phosphorus |
C | % | Carbon |
S | % | Sulfur |
Nb | % | Niobium |
Mo | % | Molybdenum |
W | % | Tungsten |