Standards
Standard | Description |
---|---|
GOST 2171-90 | GOST 2171-90 |
Description of chemical elements
Element | Units of measurement | Description |
---|---|---|
Fe | % | Iron |
Примеси | % | Impurities |
Co | % | Cobalt |
Cu | % | Copper |
Zn | % | Zinc |
Ni | % | Nickel |
Pb | % | Lead |
Country | Section | Category |
---|---|---|
CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Standard | Fe, % | Co, % | Cu, % | Zn, % | Ni, % | Pb, % | Примеси, % |
---|---|---|---|---|---|---|---|
GOST 2171-90 | < 0.3 | < 0.5 | 62–66 | 19.55–27 | 11–13 | < 0.05 | < 0.6 |
Note: By agreement, the following are allowed: Si, Mg, As, Bi, P, Sn, Sb
Note: Ni: Ni + Co
Standard | Description |
---|---|
GOST 2171-90 | GOST 2171-90 |
Element | Units of measurement | Description |
---|---|---|
Fe | % | Iron |
Примеси | % | Impurities |
Co | % | Cobalt |
Cu | % | Copper |
Zn | % | Zinc |
Ni | % | Nickel |
Pb | % | Lead |