PDA-0 (PDA-0, PDA-0)
For the production of ingots for the manufacture of alloys, semi-chemical palladium compounds, chemicals and other purposes
Classification
Chemical composition
Note: Pt + Rh + Ru + Ir < 0.015
For the production of ingots for the manufacture of alloys, semi-chemical palladium compounds, chemicals and other purposes
Standard | Fe, % | Si, % | Sn, % | Mg, % | Ca, % | Mn, % | Co, % | Cr, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | Ag, % | Au, % | Pd, % | Примеси, % |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Standard | Fe, % | Si, % | Sn, % | Mg, % | Ca, % | Mn, % | Co, % | Cr, % | Cu, % | Zn, % | Ni, % | Sb, % | Al, % | Pb, % | Ag, % | Au, % | Pd, % | Примеси, % |
GOST 31291 - 2005 | < 0.003 | < 0.002 | < 0.001 | < 0.002 | < 0.005 | < 0.001 | < 0.001 | < 0.001 | < 0.005 | < 0.002 | < 0.001 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | < 0.002 | > 99.951 | < 0.02 |
Note: Pt + Rh + Ru + Ir < 0.015
Standard | Description |
---|---|
Standard | Description |
GOST 31291 - 2005 |
Element | Units of measurement | Description |
---|---|---|
Element | Units of measurement | Description |
Fe | % | Iron |
Примеси | % | Impurities |
Si | % | Silicon |
Sn | % | Tin |
Mg | % | Magnesium |
Ca | % | Calcium |
Mn | % | Manganese |
Co | % | Cobalt |
Cr | % | Chrome |
Cu | % | Copper |
Zn | % | Zinc |
Ni | % | Nickel |
Sb | % | Antimony |
Al | % | Aluminium |
Pb | % | Lead |
Ag | % | Silver |
Au | % | Gold |
Pd | % | Palladium |