Sv-08G1N2FAA

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Wrought Aluminum Alloys

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Ti, % Cu, % Ni, % V, % Al, % As, % P, % C, % S, % Mo, % N, %
TU 14-4-1877-2004 94.023–96.15 0.2–0.4 1.3–1.8 < 0.3 < 0.04 < 0.3 2–2.4 0.04–0.08 < 0.05 < 0.04 < 0.012 0.06–0.09 < 0.005 0.25–0.45 < 0.01

Information on suppliers

Properties

Property
Wire according to TU 14-4-1877-2004 Temporary resistance: <931 MPa
Density: 7.87 g / cm3

Standards

Standard Description
TU 14-4-1877-2004

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cr % Chrome
Ti % Titan
Cu % Copper
Ni % Nickel
V % Vanadium
Al % Aluminium
As % Arsenic
P % Phosphorus
C % Carbon
S % Sulfur
Mo % Molybdenum
N % Nitrogen