Sv-08g1s

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Wrought Aluminum Alloys

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Cu, % Ni, % P, % C, % S, %
TU 14-4-133-73 96.63–97.8 0.8–1.1 1.4–1.7 < 0.1 < 0.2 < 0.1 < 0.03 < 0.11 < 0.03

Information on suppliers

Properties

Property
Wire according to TU 14-4-133-73 Temporary resistance: 780 - 1180 MPa
Density: 7.81 g / cm3

Analogues

Germany USA
1.5125 (11MnSi6) K11140

Standards

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cr % Chrome
Cu % Copper
Ni % Nickel
P % Phosphorus
C % Carbon
S % Sulfur