TV brand beryllium is a production grade of metal used for the manufacture of parts, the production of alloys, chemical compounds, etc. Unlike many other materials, the marking here reflects the production technology. In this case, TV means — technical extruded metal.

Classification

Country Section Category
CIS, Russia, Ukraine Refractory metals, carbide Beryllium

Chemical composition

Standard Fe, % Si, % Be, % Cr, % Ti, % Al, % C, % O, %
< 0.25 < 0.04 > 98.17 < 0.05 < 0.04 < 0.03 < 0.12 < 1.3

Information on suppliers

Physical characteristics

Temperature, °C \rho, \frac{kg}{m^3}
20 1850

Casting and technological parameters

melting point, °C
1278

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Be % Beryllium
Cr % Chrome
Ti % Titan
Al % Aluminium
C % Carbon
O % Oxygen

Description of physical characteristics

Parameter Units of measurement Description
\rho \frac{kg}{m^3} The density of the material

Description of the casting and technological parameters

Parameter Units of measurement Description
melting point °C The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa