V-1341

High-tech corrosion resistant weldable alloy of medium strength. The developed industrial technology of production of sheets with thickness of 0.6−3.0 mm with a grain size of less than 50 microns, which ensures their high workability in cold forming.

Used for production of sheets with a regulated structure, with a thickness of 0.6 to 3.0 mm, is designed for the aviation industry; aircraft products (skins, parts of a set, partitions, mounting assemblies, pipelines, welded tanks for different purposes) working in the temperature range from -70 °C to +150 °C. the Use of thin sheets (1.5 mm) in the weld cylinder operating under internal pressure, instead of the alloy sheets of Amg4 (up to 3 mm) ensures tightness to the base metal and reduce weight by 35−40%. Applied in a new regional aircraft SSJ. Can be applied in the construction of land transport (fuel tanks, etc.). Mastered the industrial production of all kinds of semi-finished products.

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Wrought Aluminum Alloys

Chemical composition

Standard Fe, % Si, % Mg, % Ca, % Mn, % Cr, % Ti, % Cu, % Zn, % Al, % Na, % OE, % ET, %
OST 1 90048-90 < 0.5 0.5–1.2 0.45–0.9 0.5–0.15 0.15–0.35 < 0.25 < 0.15 0.1–0.5 < 0.2 95.64–98.3 < 0.01 < 0.05 < 0.1

Information on suppliers

Standards

Standard Description
OST 1 90048-90

Description of chemical elements

Element Units of measurement Description
ET % Total other items
Fe % Iron
OE % Other items
Si % Silicon
Mg % Magnesium
Ca % Calcium
Mn % Manganese
Cr % Chrome
Ti % Titan
Cu % Copper
Zn % Zinc
Al % Aluminium