1.0034 (RSt34-2)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Base Steels |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
P, % |
C, % |
S, % |
| DIN 2393 Part 2 |
> 98.71 |
< 0.35 |
< 0.7 |
< 0.045 |
< 0.15 |
< 0.045 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
$$\epsilon_L$$, % |
Treatment |
|
|
|
|
raw |
330 |
250 |
8 |
|
|
|
|
|
annealing, soft |
290–300 |
|
28 |
|
|
|
|
|
normalization |
300–440 |
195 |
|
|
|
|
|
|
solid, cold drawn |
420 |
|
6 |
|
|
|
|
|
soft, cold drawn |
370 |
|
10 |
|
|
|
|
|
stress relief, cold drawn |
370 |
260 |
18 |
|
Properties
| Property |
| Density: 7.85 g / cm3 |
Analogues
| CIS, Russia, Ukraine |
Germany |
USA |
| VSt2ps |
RSt 34-2 |
S235JR |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |