CIS, Russia, Ukraine
-
Aluminum, aluminum alloys
-
Aluminium master alloys
- AlB3
- AlB4
- AlB5
- AlBe5
- AlBi3
- AlCa10
- AlCa6
- AlCo10
- AlCr10
- AlCr20 (A)
- AlCr20 (B)
- AlCr5 (A)
- AlCr5 (B)
- AlCu33 (A)
- AlCu33 (B)
- AlCu50 (A)
- AlCu50 (B)
- AlFe10 (A)
- AlFe10 (B)
- AlFe20
- AlMg10
- AlMg20
- AlMg50
- AlMn10 (A)
- AlMn10 (B)
- AlMn20 (A)
- AlMn20 (B)
- AlMn60 (A)
- AlMn60 (B)
- AlNi10
- AlNi20
- AlSb10
- AlSc2 (A)
- AlSc2 (B)
- AlSc5 (A)
- AlSc5 (B)
- AlSi20 (A)
- AlSi20 (B)
- AlSi50 (A)
- AlSi50 (B)
- AlSr10
- AlSr10Ti1B0.2
- AlSr3.5
- AlSr5
- AlTi10 (A)
- AlTi10 (B)
- AlTi2.5
- AlTi3B1
- AlTi5
- AlTi5B0.2
- AlTi5B0.6
- AlTi5B1
- AlV10
- AlV5
- AlZr10 (A)
- AlZr10 (B)
- AlZr15
- AlZr2.5
- AlZr5 (A)
- AlZr5 (B)
-
Antifriction aluminum alloy
-
Deoxidation aluminum
-
Foundry aluminum alloys
- 5KD
- ВКЖЛС-2 (AK21M2.5N2.5)
- AK5M2P
- АЛ9В (AK7 alloy)
- АК7Ц9 (AL11)
- АМг6л (AL23)
- АК8М (AL32)
- ВАЛ1 (AL33)
- ВАЛ5 (AL34)
- АК9ч (AL4)
- АК9пч (AL4-1)
- AL4M
- АК5М (AL5)
- АК5Мч (AL5-1)
- AL6
- АК10Су (AL7)
- AL7-4
- AL8
- АК7ч (AL9)
- АК7пч (AL9-1)
- Alloy AK10M2N
- АК11М2 (Alloy AK12M2)
- СИЛ-2 (Alloy AK12zh)
- АЛ10В (Alloy Alloy Aluminum)
- АК12М2МгН; АК12М2МгН; АЛ25 (Alloy AK12M2MgN)
- Alloy AK12MMgN
- АЛ15В (Alloy AK4M4)
- AK5M alloy
- АЛ3В (Alloy AK5M2)
- Alloy AK6M2
- Alloy AK7P
- АЛ4В (AK9 alloy)
- АЛ4 (Alloy AK9ch)
- АЛ4-1 (Alloy AK9pch)
- СИЛ-1 (Alloy AK12ch)
- Alloy AK12P
- Alloy AK18
- АЛ5 (Alloy AK5M4)
- Alloy AK5Mch
- АЛ32 (AK8M alloy)
- Alloy AK8M3
- Alloy AK9P
- Alloy Al3
- Alloy AK13
- СИЛ-00 (Alloy AK12och)
- СИЛ-0 (Alloy AK12pch)
- ВАЛ5, АЛ34 (Alloy AK8l)
- ВАЛ8 (Alloy AK8M3ch)
- Alloy Al1
- Alloy Al21
- АМг11 (Alloy Al22)
- АМг6лч (Alloy AL23-1)
- АМг5Мц (Alloy Al28)
- АМг7 (Alloy Al29)
- АК12ММгН (Alloy Al30)
- АЛ9 (Alloy AK7ch)
- АЛ9-1 (Alloy AK7pch)
- АЛ11 (Alloy AK7TS9)
- Alloy AK9M2
- Alloy AK9s
- АК9Ц6р (Srplav AK9TS6)
- АМг5К (Alloy Al13)
- АМ5 (Alloy Al19)
- АК12 (Alloy Al2)
- АЦ4Мг (Alloy Al24)
- АК12М2МгН (Alloy Al25)
- Alloy Al26
- АМг10 (Alloy Al27)
- АМг10ч (Alloy AL27-1)
- ВАЛ10 (AM4.5Kd)
- АЛ19 (AM5)
- АЛ27 (AMg10)
- АЛ27-1 (AMg10ch)
- АЛ22 (AMg11)
- АМг4К1.5М1 (AMg4K1.5M)
- АЛ13 (AMg5K)
- АЛ28 (AMg5Mts)
- АЛ23 (AMg6L)
- АЛ23-1 (AMg6lch)
- АЛ29 (AMg7)
- АЛ24 (ATs4Mg)
- B124
- AK10Su alloy
- АЛ14В (Alloy AK7M2)
- D10
- D11
- С740 (KS-740)
- КС-740 (KS740)
- KS741
- ЭП704 (Sv-10X22H7SAT)
- V2616
- VAL1
- АМ4.5Кд (VAL10)
- VAL10M
- VAL11
- VAL12
- VAL14P
- VAL5
- АК8М3ч (VAL8)
- VKZHLS-2
- VKZHLS-2K
- VSDP-11
- ZHLS
-
Primary aluminum
- 999
- A0
- A0H
- A0H2
- A0M
- A0P
- A0R
- A380
- A5
- A5E
- A5ER
- A5M
- A5N
- A5N2
- A5P
- A5R
- A6
- A6M
- A6N
- A6N2
- A6P
- A6R
- A7
- A7E
- A7E
- A7ER
- A7M
- A7N
- A7N2
- A7P
- A7R
- A8
- A85
- A85P
- A85R
- A8P
- A8R
- A9-2
- A95
- A95R
- A97
- A97R
- A98
- A99
- A995
- A995R
- A99KN
- A99KV
- A99R
- AB-0
- AB-1
- ABA-1
- ABa40
- ABa45
- ABT-101
- ABT-102
- AZH-1
- PA-BB-1
- PA-VV-1S
- PA-VV-2
- PAG-1
- PAG-2
- PAG-3
-
Technical aluminum
-
Wrought Aluminum Alloys
- 01545А
- 1050
- 1105
- 1145
- 1163
- 1201
- 1420
- 1901
- АБТ102 (1903)
- 1915
- 1920
- 1925
- 1980
- 8011
- 8011A
- 8111
- A1Mg1M1
- 1340 (AB)
- ABE
- Acpl
- AD000Sh
- AD00M
- AD00N
- AD00N2
- AD00Sh
- AD0M
- AD0N
- AD0N2
- AD0Sh
- AD1M
- AD1N
- AD1N2
- AD1Sh
- 1310 (AD31)
- 1310Е (AD31E)
- AD31Sh
- AD31T
- AD31T1
- 1330 (AD33)
- AD33Sh
- 1350 (AD35)
- AD35Sh
- AD9-1
- ADM
- ADN
- ADN2
- ADS-12
- ADSH
- 1140 (AK4 alloy)
- 1141 (AK4-1)
- Alloy ACCM
- AKM alloy
- Alloy AK4-1h
- 1380 (AK8 alloy)
- 6063 (AlMg0.7Si)
- AlMgSi
- 6060 (AlMgSi0.5)
- 1985ch alloy
- 1360 (AK6 alloy)
- Alloy AMtsS
- AM4
- 1400 (AMC)
- 1505 (AMg0.5)
- 1510 (Amg1)
- AMg1.5
- AMg1M1
- 1520 (AMg2)
- AMg2.5
- 1530 (AMg3)
- AMg3.5
- AMg3S
- 1540 (AMg4)
- AMg4.5
- 1550 (AMg5)
- 1557 (AMg5P)
- 1560 (AMg6)
- AVCH
- AVD1
- AVD1-1
- AVM
- AVP
- AVSH
- AVT
- AVT1
- AZH0.6
- AZH0.8
- AZH1
- 1165 (B65)
- 1950 (B95)
- B96
- D 2
- 1110 (D1)
- 1521 (D12)
- D12M
- D12N2
- D12Sh
- 1160 (D16)
- D16AM
- D16AT
- D16ATN
- D16B
- D16BM
- D16BT
- D16BTN
- D16ch
- D16chM
- D16chT
- D16M
- D16N
- 1167 (D16P)
- D16Sh
- D16T
- D16TN
- D16U
- D16UM
- D16UT
- 1180 (D18)
- D18Sh
- 1190 (D19)
- D19ch
- D19chT
- 1197 (D19P)
- D19Sh
- D19T
- D1A
- D1AM
- D1AT
- D1B
- D1ch
- 1117 (D1P)
- D1Sh
- D1T
- 1200 (D20)
- D20B
- D20T
- 1210 (D21)
- D23
- D24
- D25
- D26
- D3
- D31
- D33
- D35
- D4
- D41
- D42
- D43
- D44
- D45
- D46
- D6
- D65
- D8
- D9
- D95
- Сплав В96Цпч (1960pch Alloy)
- K48-2
- K48-2pch
- K48P
- 1403 (MM)
- Sil1S
- Sil2S
- St-30H15N35V3B3T
- ЭП792–ВИ) (Sv-01X12H2-VI)
- ЭП-959-ВИ (Sv-01X12H2MT-VI)
- ЭП 792 ВИ (Sv-01X12H2U-VI)
- 01Х19Н18Г10АМ4 (Sv-01X19H18G10AM4)
- ЭП909 (SV-01Х12Н4Б)
- ЭП908 (SV-01Х12Н4М)
- SV-01Х15Н4МГ
- 01Х17Н14М2 (SV-01Х17Н14М2)
- SV-01Х18Н10
- SV-01Х21Н10С6Ц
- ЭП553 (Sv-02X17H14S4)
- ЭП794 (Sv-02X8H22S6)
- ЭП936 (SV-03ГНДКА)
- Sv-03G2N2MTA
- Sv-03G2N2TA
- ЧС48 (Sv-03X12N8G3M2)
- Sv-03XH3MD
- ЭП935 (SV-03ГНКА)
- ВНС-17 (SV-03Х11Н10М2Т-VD)
- 03Х12Н9М2СТ (SV-03Х12Н9М2СТ)
- ЭП954 (SV-03Х16Н9М2)
- SV-03Х18Н15Г6М2АВ2
- ЧС39 (SV-03Х19Н15Г6М2АВ2)
- ЭК91 (SV-03Х21Н10АГ5)
- Sv-04N2GSTA
- Sv-04N2GTA
- Sv-04N3GMTA
- Sv-04N3GSMTA
- Sv-04X17H10M2
- ЭП568 (Sv-04X19H5AG12M)
- ЭП762 (Sv-04X20H10G2B)
- Sv-04X20H10G2BU
- Sv-05GNTAA
- ЧС31 (Sv-05X15H9G6AM)
- ЭП458 (Sv-06A)
- Sv-06H3G2SMFTYuch
- Sv-06H8G2SMFTYUch
- ЭП321 (Sv-06X18H5G11BAF)
- ЭП320 (Sv-06X18H5G12AB)
- ЭП319 (Sv-06X20H4AG10)
- 06Х21Н7БТ (Sv-06X21N7BT)
- ЭК51 (Sv-06X22H8M2FTAY)
- ЧС49 (Sv-07H22N13G5ST)
- Sv-07PNM
- Sv-07PNMA
- Sv-07PNMAA
- Sv-07X16H6
- Sv-07XH3MD
- Sv-08G1N2FAA
- Sv-08G1NFAA
- Sv-08G1NMA
- Sv-08G1NMA-O
- Sv-08G1NMFAA
- Sv-08g1s
- Sv-08g1sa
- Sv-08G1SP
- Sv-08g1sr
- Sv-08g2s-o
- Sv-08g2sa
- Sv-08G2SM
- Sv-08G2SNMT
- Sv-08G2SNTUR
- Sv-08g2sr
- Sv-08g2sts
- Sv-08GM
- ЭП934 (Sv-08GN2MDTA)
- Sv-08GNM
- Sv-08gs-o
- Sv-08gsa
- Sv-08GSNTA
- Sv-08GSP
- Sv-08GSR
- Sv-08GST
- Sv-08HG2SMF
- Sv-08HG2SU
- ЭП305 (Sv-08X14H8S3B)
- Sv-08X15H5D2TU-Sh
- Sv-08X17H5M3
- Sv-08X19H10G2BU
- Sv-08X19H11F2S2
- Sv-08X20H9S2BTYU
- ЭП854 (Sv-08X21H11FT)
- ЭП703 (Sv-08X21H6S2AT)
- Sv-09g2sts
- Sv-09HGNMTA
- Sv-09HGNMTAA-VI
- Sv-09X15H8Yu
- Sv-09Х15Н8Ю1
- Sv-10GAA
- Sv-10GN1MA
- Sv-10GNA
- Sv-10GNA-O
- Sv-10GNMDTA
- Sv-10GSM
- Sv-10H3GM
- Sv-10H3GMFTA
- Sv-10HG2SMF
- Sv-10HGSN2MT
- Sv-10HMFTU
- Sv-10HMFTU-A
- 10Н3ГМТ (Sv-10N3GMT)
- Sv-10Nude
- Sv-10X11N20T2R
- ЭП778 (Sv-10X15H23M4V4AF2)
- ЭП647 (Sv-10X19H11M4F)
- ЭП868 (Sv-10X19N23G2M5FAT)
- Sv-10X21H11FT
- Sv-10X2M
- Sv-10X3M1A
- Sv-11H11N2V2MF
- ЭИ962-Ш (Sv-11H11N2V2MF-Sh)
- Sv-12M
- Sv-12X17G9AN4
- Sv-12X17G9AN4-Sh
- ЭИ878-Ш (Sv-12X21H5T)
- ЭП830 (Sv-12XH7K2MF)
- ЭК119 (Sv-13X14N9S4F3G)
- Sv-14g2ch
- Sv-15X18H12S4TU
- Sv-15X18H12SCHTYU
- Sv-20H27N6M3AGV
- ЭП331 (Sv-20H2GSNVM)
- ЭП83 (Sv-20H4GMA)
- ЭП324 (Sv-20HSNVFA)
- ЭП324У-ВД (Sv-20HSNVFA-VD)
- ЭП835-ВД (Sv-28H3SNMVFA-VD)
- Sv-36NGMT
- Sv-Kh12N20T2R
- ЭП509 (Sv-Kh14N8M2)
- Sv-Kh15N5D2T
- Sv-Kh15N5D2TU-Sh
- Х12НМБФ (Sv-X12NMBF)
- Sv1201
- Sv1557
- Sv1577pch
- SvA5
- SvA85T
- SvA97
- SvA99
- АК10 (SvAK10)
- ER 4043 (SvAK5)
- SvAK5u
- Svamc
- SvAMg3
- SvAMg5
- SvAMg6
- SvAMg61
- SvAMg63
- V 93
- V-1341
- V-1461
- V-1469
- V-92
- V48-4
- V48P
- V65Sh
- V91
- V92
- 1930 (V93)
- V93pch
- 1940 (V94)
- V95-1
- V95-1A
- V95-1AM
- V95-1AT
- V95-1Sh
- V95-2
- V95-2A
- V95-2AM
- V95-2AT
- V95-2B
- V95-2BM
- V95-2Sh
- V95A
- V95AM
- V95AT1
- V95B
- V95och
- V95ochT1
- V95ochT2
- 1957 (V95P)
- V95pch
- V95pchT1
- V95pchT2
- V95Sh
- V96C-1
- V96C-3
- V96C-3PCH
- V96C1OCH
- V96CPCH
- 1960 (V96ts)
- V96TS1
- VAD1
- VAD1B
- VAD23
- VAD23PCH
- АК4ч (VAK4)
- АК6ч (VAK6)
- ВДч (VD)
- VD1
- 1170 (VD17)
- VD1A
- VD1AM
- VD1AN
- VD1AT
- VD1B
- VD1BM
- VD1BN
- VD1M
- VD1N
- VD1T
- VDCH
- Alloy 1925C
- Alloy 1925Sh
- 1985pch alloy
-
-
Brass (copper-zinc alloy)
-
Brass, pressure treated
- CuZn36Pb2As
- CuZn39Pb3
- L59
- L60
- L63
- L66
- L68
- L70
- L75
- L75mk
- L80
- L85
- L90
- L96
- LA77-2
- LA77-2u
- LA85-0.5
- LAMsh77-2-0.04
- LAMsh77-2-0.05
- LAN59-3-2
- LANKMts75-2-2.5-0.5-0.5
- LAZH60-1-1
- LK62-0.5
- LK75V
- LK80-3
- LKS65-1.5-3
- LMsh68-0.05
- LMts58-2
- LMtsA57-3-1
- LN65-5
- LO60-1
- LO62-1
- LO70-1
- LO90-1
- LOK59-1-0.3
- LOMsh70-1-0.05
- LS58-2
- LS58-3
- LS59-1
- LS59-1V
- LS59-2
- LS60-1
- LS63-3
- LS64-2
- LS74-3
- LZhMts59-1-1
- LZHS58-1-1
-
Foundry brass
-
Foundry brass ingots
-
-
Bronze
-
Bronze, heatproof
-
Pewter cast bronze in pigs
-
Pressure Tin Bronze
-
Pressureless bronze plated
-
Tin cast bronze
- BrO10
- БрОФ10-1 (BrO10F1)
- БрОС10-10 (BrO10S10)
- BrO10S12N3
- БрОЦ10-2 (BrO10Ts2)
- BrO19
- BrO3.5Ts7S5
- БрОЦС3-12-5 (BrO3Ts12S5)
- BrO3Ts6S5
- BrO3Ts7S5N
- БрОЦСН3-7-5-1 (BrO3Ts7S5N1)
- БрОЦС4-4-17 (BrO4Ts4S17)
- БрОЦС3.5-7-5 (BrO4Ts7S5)
- BrO4Ts8S5
- БрОС5-25 (BrO5S25)
- BrO6S6Ts3
- BrO6Ts6S2H
- БрОЦС6-6-3 (BrO6Ts6S3)
- BrO7S15N2
- БрОНЦ8,5-4-2 (BrO8N4Ts2)
- БрОС8-12 (BrO8S12)
- БрОЦ8-4 (BrO8Ts4)
- БрО10С10 (BrOS10-10)
- БрО10Ц2 (BrOTs10-2)
- БрОЦС5-5-5 (CuSn5Zn5Pb5)
- CuSn5Zn5Pb5-C
- OCS 3-12-5
- OCS 3-13-4
- OCS 5-5-5
- OCS 5-6-5
-
Tinless cast bronze
-
-
Cast iron
-
Copper, copper alloys
-
Copper
-
Copper Alloys
-
Copper-Nickel Alloys
- МНАХМц20-4-2,3-4 (Camelon)
- МНАХМц4,5-4,5-0,7-2,5 (Camelyn)
- Class A
- Class B
- Constantan
- Copel
- Kunial A
- МНА6−1,5 (Kunial B)
- СплавТП (MN0.6)
- МН-10 (MN10)
- СплавТБ (MN16)
- MN19
- MN25
- MN95-5
- КуниальА (MNA13-3)
- КуниальБ (MNA6-1.5)
- Манганин (MNMts3-12)
- Константан (MNMts40-1.5)
- Копель (MNMts43-0.5)
- MNMtsAZh3-12-0.3-0.3
- MNTS12-24
- Нейзильбер (MNTS15-20)
- MNTS18-20
- MNTS18-27
- MNTSS16-29-1.8
- MNZH5-1
- ERCuNi5Fe1 (MNZHKT5-1-0.2-0.2)
- Мельхиор (MNZhMts10-1-1)
- MNZhMts30-1-1
- Монель (NMZhMts28-2.5-1.5)
-
Copper-phosphorous alloys
-
-
Corrosion-resistant alloys and steels
-
Corrosion-resistant alloys
- 03ХН28МДТ. ЭП516. (000H23N28M3D3T)
- 00H16N15M3BSH
- ЭП337У (00H19N40B)
- ЭП743 (00H20N42M4V3B)
- ЭП579 (00H23N28M30T)
- ЭП754-ИД (015H20N25G2B-ID)
- 01H15N60M16
- ЭП753-ИД (01H18N40M5GB-ID)
- ЭП753Р-ИД (01H18N40M5GBR-ID)
- 01H20N54M9
- ЭК75 (01H24N25G7AM3D)
- ЧС-84 (01H25N19G5AM4)
- ЧС75-ВИ (01H25T-VI)
- ЧС85 (01H26N14GT)
- ЭК66 (01H29N35G8AM4D)
- ЭП 642 (02H15N65M13V3TYu)
- 02H18N25M4S3
- ЭП855 (03H15N35G7M6B)
- ЭП516 (03HN28MDT)
- ЭИ943 (06HN28MDT)
- ЭИ628 (06HN28MT)
- 45H25N35BS
- 45H25N35BSL
- 45H26N23S2B2
- 45H26N26S2B
- 45H26N33S2B2
- 45H26N33V5S2B-SH
- 45H28N49V5S
- 45H28N49V5SL
- Aeralloy 105 (46NHT)
- Aeralloy 101 (46NHVITYU)
- Aeralloy 500 (47ND-VI)
- Aeralloy 718 FineGrain (47NHM-VI)
- 48KHVN
- Aeralloy 751 (48KNF)
- Aeralloy 91 (49K2FN-VI)
- 4E
- 36Х18Н25С2 (4H18N25S2)
- 50BTC-VD
- 50H-VI
- 50H20N35S2B
- 50H25N35K15V5S
- 50H25N35S2B
- 50H25N35S2BL
- 50H25N35V5K15S
- 50H25N35V5K15SL
- 50KF
- ЭП967 (50N3HYU)
- 50TMB-VD
- 52NKHBMYU
- 52NTYU
- 53N
- 65BT
- 65N
- 65NP
- 67KN5B
- 67N26M
- 67N28M
- 70GNH
- 70KNB
- 70NHBMYU
- 70NHMBYU
- 70TMN-VD
- 71GYU
- 71N18HSR
- 72NMDH
- 75G22D3H
- 75G25D
- 75GNAD
- 75H24TL
- 75N13HSR
- ЭП636 (75N34H8G3)
- 75NM-VI
- 78ND2M
- 79NM-VI
- 80TF-VD
- 82N7HSR
- ДИ-38 (90G29YU9VBM)
- 90G29YUVBM
- 92K
- 92NSR
- A 146 briquettes
- 06ХН28МДТ (AISI 904L)
- 0Х16МТ (DI-11)
- 10Х14АГ15 (DI-13)
- 9Х4В2МФСГ (DI-17)
- 7Х3ВМФС (DI-18)
- 18ХГСН2ВМА (DI-2)
- 08Х17Н6Т (DI-21)
- 4Х4М2ВФС (DI-22)
- 45Х3В3МФС (DI-23)
- DI-37
- 90Г29Ю9ВБМ (DI-38)
- 18ХГСН2МА (DI-4)
- 5Х2ГСВМ (DI-42)
- 8Х4М4В2Ф1 (DI-43Sh)
- 0Х13Г12АС2Н2 (DI-50)
- Х12Ф4М (DI-51)
- 6Х4М2ФС (DI-55)
- 7ХГНМ (DI-56)
- Х5С4В2Ф2НМ (DI-57)
- 10Х14Г14Н3 (DI-6)
- 10Х13Г18ДУ (DI-61U)
- 08Х18Тч (DI-77)
- 0Х20Н5АГ12МФ (DI-8)
- 18Х15Н3М-Ш (DI1-SH)
- 18Х15Н3М-Ш "селект" (DI1-Sh "select")
- Р7М2Ф6-МП (DI100-MP)
- Р6М5К5-МП (DI101-MP)
- Р9М4К8-МП (DI102-MP)
- Р12М3К5Ф2-МП (DI103-MP)
- 85Х5С3В2Ф2МН (DI113)
- Х14Г14Н4Т (DI12)
- DI20
- DI22
- 5Х3В3МФС (DI23)
- 5Х2МНФ (DI32)
- ДИ-37 (DI37)
- 16Х3НВФМБ-Ш (DI39-Sh)
- DI3A
- 4Х3М2ВФГС (DI41)
- 8Х4М4В2Ф1-Ш (DI43-Sh)
- 12Х13Г12АС2Н2 (DI50)
- 03Х11Н8М2Ф-ИД (DI52-ID)
- 03Х11Н8М2Ф-ВД (DI52-VD)
- DI55
- 10Х13Г12БС2Н2Д2 (DI59)
- 10Х13Г18Д (DI61)
- 05ХН46МВБЧ (DI65)
- DI70-MP
- 05Х12Н6Д2МФСГТ (DI80)
- DI82
- 17Х5В3МФ5С2-МП (DI90-MP)
- Р6М5Ф3-МП (DI99-MP)
- 4Х3ВМФ (EI-2)
- EI1
- 20Х13Н4Г9 (EI10)
- EI100
- EI102
- EI103
- EI104
- EI105
- EI106
- 40Х10С2М (EI107)
- EI108
- EI109
- EI11
- EI110
- EI111
- EI112
- EI113
- EI115
- EI116
- EI117
- EI118
- EI119
- EI12
- EI120
- EI121
- EI122
- EI123
- EI127
- EI128
- EI129
- EI13
- EI130
- EI131
- EI132
- EI133
- EI134
- EI135
- EI136
- EI137
- EI138
- EI14
- EI140
- EI141
- 70С2ХА (EI142)
- EI143
- EI144
- EI145
- EI146
- EI147
- EI148
- EI149
- EI150
- EI151
- EI152
- EI153
- EI154
- EI155
- EI156
- EI157
- EI158
- EI159
- EI16
- EI160
- 6Х7В7ФМ (EI161)
- EI162
- EI163
- EI164
- EI165
- EI166
- EI167
- EI168
- EI169
- EI17
- EI170
- EI171
- EI172
- EI173
- EI174
- EI175
- EI176
- EI177
- EI178
- EI179
- EI18
- EI180
- EI182
- EI183
- EI184
- EI185
- EI186
- EI187
- EI188
- EI189
- EI19
- 8ХВ2Ф (EI190)
- EI191
- EI192
- EI195
- EI196
- EI197
- EI198
- EI20
- EI200
- EI201
- EI202
- EI203
- EI204
- EI205
- EI206
- EI207
- EI208
- EI209
- EI21
- EI210
- 20Х20Н14С2 (EI211)
- EI212
- EI213
- EI214
- EI215
- EI216
- EI217
- EI218
- EI219
- EI22
- EI221
- EI222
- EI223
- EI224
- EI225
- EI226
- EI229
- EI23
- EI230
- EI231
- EI232
- EI233
- EI234
- EI235
- 120Г13 (EI236)
- 1Х14Н14В2М (EI237)
- EI238
- EI239
- EI24
- 45Х14Н14СВ2М (EI240)
- Х14 (EI241)
- EI242
- EI243
- EI244
- EI245
- EI246
- EI247
- EI248
- EI249
- EI250
- EI251
- EI252
- EI253
- EI254
- EI255
- EI256
- EI258
- EI259
- EI26
- EI260
- EI262
- EI263
- EI266
- EI267
- EI268
- 268Л (EI268L)
- EI269
- EI272
- EI273
- 16ХГТА (EI274)
- EI275
- EI277
- EI279
- EI28
- EI280
- EI281
- EI282
- EI284
- EI285
- EI286
- EI288
- EI289
- EI29
- EI290
- EI291
- EI293
- EI294
- EI295
- EI296
- 20Х3 (EI297)
- EI298
- EI299
- EI3
- EI30
- EI300
- EI301
- EI302
- 55Х20Г9АН4 (EI303)
- 55Х20Г9АН4Б (EI303B)
- EI304
- EI305
- EI306
- EI308
- EI309
- EI31
- EI310
- EI311
- EI312
- EI313
- EI314
- EI315
- EI317
- EI318
- EI32
- EI320
- EI321
- EI322
- EI323
- EI324
- EI325
- EI326
- EI327
- EI328
- EI329
- EI33
- EI330
- EI333
- EI335
- У16 (EI336)
- EI337
- EI338
- EI339
- EI34
- EI341
- EI342
- EI343
- EI344
- EI345
- EI347
- Р9Ф (EI347-Sh)
- EI347M
- EI348
- EI350
- EI351
- EI352
- EI353
- EI354
- EI355
- EI356
- EI357
- EI358
- EI359
- EI36
- EI361
- EI365
- 130СЛ (EI366)
- EI367
- EI368
- EI37
- EI371
- EI372
- EI373
- EI374
- EI375
- EI376
- EI377
- EI378
- EI379
- EI38
- EI380
- EI381
- EI382
- EI383
- EI385
- EI386
- EI387
- 40Х15Н7Г7Ф2МС (EI388)
- EI39
- EI390
- EI391
- EI392
- EI393
- EI394
- EI396
- EI397
- EI398
- EI4
- EI40
- Х17Н13М (EI400)
- EI401
- 8Х18Н12Б (EI402)
- EI403
- 10Х13СЮ (EI404)
- EI405
- EI406
- EI407
- EI408
- EI409
- EI41
- EI410
- EI411
- EI413
- EI414
- 20Х3МВФ (EI415)
- 20Х3МВФ-Ш (EI415-Sh)
- 20Х3МВФ-ВД (EI415-VD)
- 20ХН3МВФА (EI415A)
- 20ХН3МВФА-Ш (EI415A-Sh)
- 20ХН3МВФА-ВД (EI415A-VD)
- 20Х3МВФЛ (EI415L)
- EI419
- EI42
- EI420
- EI423
- EI425
- EI426
- EI427
- EI428
- Н12ХГ (EI429)
- EI43
- EI430
- EI431
- 10Х17Н13М3Т (EI432)
- EI433
- EI434
- EI436
- EI438
- EI44
- EI440
- EI446
- EI448
- EI449
- EI45
- EI450
- EI451
- EI452
- EI453
- EI454
- EI455
- EI456
- EI458
- EI459
- EI46
- EI463
- EI464
- EI468
- EI469
- EI47
- EI471
- EI472
- EI474
- EI475
- EI476
- EI477
- Х20Н10Г6А (EI478)
- EI479
- EI48
- EI480
- 37Х12Н8Г8МФБ (EI481)
- 4Х12Н8Г8МФБ-Ш (EI481-Sh)
- EI481B
- EI482
- EI483
- 15Х18СЮ (EI484)
- EI486
- EI487
- EI488
- EI489
- EI49
- EI490
- EI491
- EI492
- EI493
- EI494
- EI495
- 08Х13 (EI496)
- 08Х13Л (EI496L)
- EI498
- EI5
- EI50
- EI501
- EI502
- EI504
- EI505
- EI506
- EI508
- EI509
- EI51
- EI510
- EI511
- EI512
- 10Х13М (EI515)
- EI517
- EI519
- EI52
- EI520
- EI526
- EI527
- EI529
- EI53
- 12Х2МФБ (EI531)
- EI532
- EI539
- EI54
- EI541
- EI542
- EI543
- EI545
- EI546
- EI547
- EI548
- EI549
- EI55
- EI550
- EI551
- EI552
- EI553
- EI554
- EI555
- EI56
- EI561
- EI562
- EI564
- EI565
- EI566
- EI567
- 10НМ (EI569)
- EI571
- 31Х19Н9 (EI572)
- 31Х19Н9МВБТ-ВД (EI572-VD)
- 31Х19Н9МВБТЛ (EI572L)
- EI573
- EI575
- EI576
- EI577
- 18Х3МВ (EI578)
- 20Х3ВМФ (EI579)
- EI58
- 08Х17Н15М3Т (EI580)
- EI581
- 06ХН2М (EI582)
- EI585
- EI586
- EI587
- EI588
- EI589
- EI590
- EI591
- Х16Н13М3 (EI592)
- EI593
- 0Х23Ю5 (EI595)
- EI597
- EI6
- Х13Ю4 (EI60)
- EI603
- EI605
- 08Х19Н9Ф2С2 (EI606)
- EI606A
- ХН80ТБЮА (EI607A)
- 18ХСНР (EI609)
- EI61
- EI610
- EI611
- EI613
- EI614
- EI62
- EI63
- EI631
- EI636
- EI64
- EI640
- EI641
- EI642
- 40ХН2СВА (EI643)
- 40ХН2СМА-ВД (EI643-VD)
- 40ХН2СМА (EI643M)
- EI644
- EI645
- Х05Ф (EI646)
- EI647
- EI648
- EI649
- EI65
- 15Х18Н12С4ТЮ (EI654)
- 15Х18Н12С4ТЮ-Ш (EI654-Sh)
- 15Х18Н12С4ТЮЛ (EI654L)
- EI655
- EI656
- EI658
- 23Х2НВФА (EI659)
- 23Х2НВФА-Ш (EI659-Sh)
- EI66
- EI660
- EI662
- EI663
- EI664
- EI665
- EI666
- EI667
- EI669
- EI67
- EI670
- EI671
- EI672
- EI679
- EI68
- 08Х16Н13М2Б (EI680)
- 12Г2Х (EI681)
- EI683
- 06Х18Н11 (EI684)
- EI685
- EI686
- EI687
- 10Х17Н18ГМ2 (EI689)
- 45Х14Н14В2М (EI69)
- EI690
- EI691
- 1Х14Н16Б (EI694)
- 1Х14Н16БР (EI694P)
- 1Х14Н18В2Б (EI695)
- 09Х14Н19В2БР (EI695R)
- 10Х11Н20Т3Р (EI696)
- Х12Н20Т2Р (EI696 (A))
- 10Х11Н20Т2Р (EI696A)
- EI697
- EI699
- EI7
- EI70
- 85Г13 (EI700)
- Нп-60Х3В10Ф (EI701)
- EI705
- EI706
- EI707
- 14НХ (EI708)
- ЭИ708 (EI708A)
- EI709
- EI71
- EI711
- 12Х2НВФА (EI712)
- EI712A
- EI712A-Sh
- ЭП506 (EI712M)
- 12Х2НВФМА-Ш (EI712M-Sh)
- EI713
- EI714
- EI715
- EI716
- EI717
- EI718
- EI719
- 30Х13Н7С2 (EI72)
- EI720
- EI721
- 70С3ХМВА (EI722)
- EI723
- EI724
- 09Х14Н19В2БР1 (EI726)
- EI727
- EI729
- EI73
- EI730
- EI731
- 08Х20Н14С2 (EI732)
- EI733
- EI734
- 13Х14Н3В2ФР (EI736)
- 13Х14Н3В2ФР-Ш (EI736-Sh)
- 13Х14Н3В2ФРЛ (EI736L)
- EI738
- EI739
- EI74
- EI740
- EI741
- EI742
- EI743
- EI744
- EI745
- EI746
- EI747
- EI748
- EI749
- EI75
- EI750
- EI751
- EI752
- 40ХНР (EI753)
- EI754
- EI755
- 12Х11В2МФ (EI756)
- EI757
- EI76
- ЭИ760-Ш (EI760)
- ЭИ760 (EI760-Sh)
- EI761
- EI762
- 21Х2НВФА (EI763)
- EI764
- EI768
- EI769
- EI77
- EI770
- EI771
- EI772
- EI773
- EI78
- EI783
- EI784
- EI785
- EI79
- EI790
- EI791
- EI793
- EI794
- EI796
- EI797
- EI798
- EI8
- EI80
- EI800
- EI801
- 15Х12ВНМФ (EI802)
- EI803
- EI804
- EI806
- EI807
- EJ1
- EJ2
- 40Х13 (EJ4)
- EP607
- EZh17
- EZH3
- HK62M6L
- ЭП795 (HN58V)
- ЭП567 (HN65MV)
- ЭП760 (HN65MVU)
- JUNKERALLOY C22C
- ВНС-13 (K65H20N9M3L2)
- Alloy 45KHNMVT
- N70MF
- ЭП814А (N70MFV)
- Alloy 35N32KXM
- VNS-13
- VNS-39
- VNS45
- VNS46
- VNS48
- VUS-15
- VUS-17
- VUS-22
- VZH100
- VZH101
- VZH105
- VZH105-ID
- VZH105-PD
- VZH136
- VZH136-ID
- VZH136U
- VZH145
- VZH159
- VZH172
- VZH175
- VZH36-VD
- VZH98
- Х15Н5МВФБ (ZI-53)
- 50Х14МФ (ZI128)
- ZI130
- 03Х18Н16М3 (ZI133)
- 03Н18К8М3ТЮ-ВД (ZI25-VD)
- ZI35
- 00Н19К9М5ТЮ (ZI56)
- ZI66
- 03Х22Н6М2 (ZI67)
- 03Х23Н6 (ZI68)
- 03Н18К1М3ТЮ-ВД (ZI80-VD)
- Н16К4М5Т2Ю (ZI89)
- Х12Н8К5М2ТЮ (ZI90-VI)
- ZIO-8
-
Corrosion-resistant heat-resistant steel
- ЧС78-ВИ (01H25M2T-VI)
- ЧС76-ВИ (01H25tBYU-VI)
- ЭП 367 (02H15N60M16)
- ЧС-116 ИД (02H18N40M5G2TFRYU-ID)
- ЭП753-ИДД (02H18N40M5G2TFRYU-IDD)
- 02H21N42M3
- ЧС108-ПТ (02H25N22AM2-PT)
- 02H25N22AM2-VI
- 02H25N22AM2L
- ЭК77 (02H28N30MDB)
- 02HN30MDB
- ЭК5У (02Х21Н25М4ДБ)
- 02Х21Н25М5Б
- ЭК5 (02Х21Н25М5ДБ)
- 02Х22Н50М7
- 02Х22Н52М11
- ЧС108 (02Х25Н22АМ2)
- 02Х25Н32М3
- 02Х25Н50М6
- 02Х25Н7М3
- 02Х25Н7М4
- ЭП843-ИД (02Х26Н6-ИД)
- ХН30МДБ-Ш (02Х27Н31М4)
- ЭК145 (03H15N35G7M6BU)
- 03H20N45G6M6B
- ЭК146 (03H20N45G7M6BU)
- ЧС42 (03H20N45M4Bch)
- ЧС43-ВИ (03H20N45M4BRTS (VI))
- 03H20N65G5M4B3V
- 03H20N65G5M4VB
- ЭК148 (03H20N70G3B3T)
- 03H20N70G3B3TU
- ЭК150 (03H20N70M7B2TU)
- 03Х21Н32М3Б-ВИ (03H21N32M3B)
- 03H21N32M3B-VI
- ЧС33У (03H21N32M3BU)
- ЭК 86 (03H23N28YU4T)
- ЭП955 (03H24N13G2B)
- 03H24N13G2BU
- ЭК23 (03H25N14G2FBT)
- 03H25N25YU5TL
- ЭП979 (03HN25MDG)
- 03HN45MB
- 03N14H4M2T2-VI
- ЭК147 (03N60G8M7TU)
- 03Х13
- 03Х20Н32М3Б
- ЧС32 (03Х20Н45М5Б)
- 03Х22Н35М4
- ЭИ629 (03Х23Н28М3Д3Т)
- 03Х23Н6М4Д3АБ-Ш
- 03Х24Н6АМ3
- ЭИ130 (03Х24Н6АМ3Л)
- 03Х25Н50М6
- ЭК65 (03Х26Н6Т)
- ЭП978 (03ХН25МДГБ)
- ЭП796 (03ХН35МЮ)
- 03ХН58В
- ЭП 535 ВД (04H32N8-VD)
- 04HN40MDTY
- 04Х26Н5М3
- 05H20N32TL
- ЭК179 (05H22N10G6AM2)
- ЭП829 (05H30N40M6TB)
- 05HN32T
- ДИ65 (05HN46MVBCH)
- 05Х20Н32Т
- 05Х26Н6М2Д2АБФЛ
- 08Х12Н3Д (06H12N3D)
- 06H15N35G7M6B
- ЧС68-ИД (06H16N15M2G2TFR-ID)
- 06Х18Н10 (06H18N10T)
- ЭК56 (06H20N25M8G8)
- ЭП87 (06H25N12TYu)
- ЭП781 (06H25N16AG6Ts)
- ЭП 350 (06HN46B)
- ЭП367 (06Х15Н60М15)
- 06Х23Н28М3Д3Т
- 06Х24Н6ТАФМ
- 06Х25Н35Ю2С-Н
- ЧС59-ВИ (07H15N35M3RTSCH-VI)
- 07H20N25M3D2TL
- 07H25N12G2T
- ЭП750-Ш (07H25N16AG6F-Sh)
- 07H25N16AG6Ts
- ЭП883 (07H25N50M9K9B2G3)
- 07HN25MDTL
- ЧС81 (07Х15Н30В5М2)
- ER309L (07Х25Н13У)
- ЭП244 (08G32H10)
- ЭП181 (08G35YU6M2)
- ЭП939 (08H11G35MR)
- 08H11N35MTYUR
- ЭИ496 (08H13)
- 08H14F
- 08Х14МФ-Ш (08H14MF)
- ЭП674 (08H15N25T2MFR)
- 08Х15Н5Д2ТУ-Ш (08H15N5D2TU)
- ЭИ645 (08H17T)
- ЭИ825 (08H18N10)
- ЭП512 (08H20N45G6M2B)
- 08H25N13BTYu
- ЭИ824 (08H50)
- 0Х18Т1 (08Kh18T1)
- 08N60G8M7T
- ЭП164-Ш (08X15H24V4TR-Sh)
- ЭИ914 (08X18H10T)
- 08XH28MDT
- 08XH35WTO
- 08Х15Н23В7Г7М2
- 08Х15Н5Д2Т (08Х15Н5Д2Т-Ш)
- 08Х17
- 08Х25Н20С3Р1
- 08Х25Н25М3
- 08Х25Н40М7
- 08Х25Н50М10
- ЧС130 (09H17N)
- 1Х18Н10Т (09H18N10T)
- ЭИ981A (09X16H25M6AF)
- ЭП496 (0N70M27F)
- ЭП872 (0X16H65M7B2T)
- 0X16H70B2T
- ЭП870 (0X16H80B2T)
- 0X20H65M7B2T
- ЭП871 (0X20N70B2T)
- 0X23H28M2T
- 0X27U5A
- ЭИ626 (0X27YU5)
- 0Х15Н65М16В
- 0Х23Н18
- 0Х23Н28М3Д3Т
- 1 / 2SSuMT
- 1 / 4SSuMT
- АД00Е (1010E)
- 1010Sh
- АД0Е (1011E)
- АД0Ш (1011Sh)
- АД1Ш (1013Sh)
- АД0 (1050A)
- 0Х12НД (10H12ND)
- ЭП700-ВД (10H15N27T3MR-VD)
- ЭП485 (10H15N28V2M4B)
- 10H18N10T
- ЭП529 (10H32N4D-VD)
- 10Х9МФБ (10H9MFB-W)
- 10X11N23T3MR-VD
- 10X16H25AM6
- ЭК143 (10X16H25AM6)
- ЭК144 (10X16H25G5AM6U)
- 10X16H27T3MR
- 10X20H32TUL
- 10X20H33BL
- 10X20H77TUL
- 10X20N33B
- 10XH28VMAB
- 10XH45YU
- 10Х11Н23Т3МР-Ш
- 10Х20Н32ТЮ
- 10Х20Н77ТЮ
- 10Х22Н77ТЮ
- ЭП988 (10Х28Н11С4AD)
- ЭП263 (10Х32Н8)
- 1105Sh
- АКД4Ш (1140Sh)
- АК4-1Ш (1141Sh)
- Д16Ш (1160Sh)
- В65Ш (1165Sh)
- Д18Ш (1180Sh)
- Д19Ш (1190Sh)
- 1201Sh
- ВАД23пч (1230ph)
- ЭИ756 (12H11V2MF)
- ЭП450-Ш (12H12M1BFR-W)
- 1Х13 (12H13)
- ЭЖ17 (12H17)
- Х18Н12Т (12H18N12T)
- Х18Н9 (12H18N9)
- 12H25N16G7AR-Sh
- ЭК37 (12H25N33S3G6BR)
- 12HN38VT
- 12X16H25M6AG
- Х18Н9Т (12X18H9T)
- 12XH35WT
- 12XH38VB
- АД31Е (1310E)
- АД31Ш (1310Sh)
- АД33Ш (1330Sh)
- АВШ (1340Sh)
- АД35Ш (1350Sh)
- АКД6Ш (1360Sh)
- АКД8Ш (1380Sh)
- 13H16N3B
- 13X25T
- АМцШ (1400Sh)
- АМцСШ (1401Sh)
- ММШ (1403Sh)
- 14B
- ЭИ268 (14H17N2)
- Д12Ш (1521Sh)
- 1541pc
- 1561 cladding material
- АМг61Н (1561H)
- АМг61НН (1561HN)
- АМг61М (1561M)
- 1561N cladding material
- 1561Н (1561NB)
- 1561NBN
- 1565h
- 18Х15Н3М (18H15N3M-SH)
- 2Х13 (20X13)
- 3Х13 (30Ch13)
- 4Х13 (40X13)
- 47HNM-VI
- 08Х18Н10 (AISI 304)
- 08Х18Н10Т (AISI 321)
- 03Х13 (AISI 409L)
- 12Х13 (AISI 410)
- AISI 420
- 30Х13 (AISI 420S)
- 12Х17 (AISI 430)
- 08Х17Т (AISI 439)
- AL32D
- AL32K
- AL32V
- AL32Z
- AL35
- AL4D
- AL4K
- AL4V
- AL5-1D
- AL5-1K
- AL5-1V
- AL5-1Z
- AL5D
- AL5K
- AL9-1D
- AL9-1K
- AL9-1Z
- AL9D
- AL9K
- AL9M
- АК7 (AL9V)
- AL9Z
- АК5М2 (ALB)
- ПОСВ-50 (Alloy Rose)
- ЮНС (Alnisi)
- НМцАК2-2-1 (Alumel)
- Alyunik 7/1
- AM4.5cd
- AMg 2.5
- AMg 4.0
- AMg0.5pch
- AMg0.7
- AMg1.5
- AMg11D
- AMg11K
- AMg11V
- AMg11Z
- AMg2M
- AMg2N
- AMg2N2
- AMg3.5
- AMg3M
- AMg3N
- AMg3N2
- AMg4.5
- AMg4K1.5M
- AMg4K1.5M1
- AMg5M
- 1561 (AMg61)
- 1561М (AMg61M)
- AMg61N
- AMg65
- AMg6B
- AMg6BM
- AMg6M
- AMg6U
- AMg6UM
- AMg7D
- AMgM1
- AMO1-10
- AMO1-20
- AMO1-30
- AMO1-40
- AMO2-15
- AMT-1
- AMT-1D
- AMT-2
- AMT-2D
- BCR
- Bhr
- BOD
- BOF4
- BOF8
- BOTS10
- BOTs4
- BOTS8
- BPI
- Br AZh9-4L
- Br AZhMts 10-3-1.5
- Br AZhN 10-4-4L
- Br OC 8-12
- Br OF 10-1
- Br OFN 10-0.7-0.5
- Br OTsN 10-2-1,5
- Br OTsS 5-5-5
- BrAMg6-1
- BrAMts9-2l
- Brand "A"
- Brand "B"
- Brass
- BrAZh10-1,5
- BrAZh9-4l
- BrAZhMts10-3-1.5
- BrAZhMts10-3-1.5l
- BrAZhN10-4-4l
- BrAZhN11-6-6l
- BrAZhNmts8.5-4-5-1.5
- CuBe2NiTi (BrBNT1.9)
- БрБ1,9НТМг (BrBNT1.9Mg)
- Brcr0.2
- BrHKd0.5-0.3
- 204А (BrHNb0.2-0.1)
- 204 (BrHNb0.4-0.25)
- БрХ0,3О0,3Цр0,1 (BrHOTsr0.3-0.3-0.1)
- БрХ0,6Т0,5 (BrHT0.6-0.5)
- BrKd1,0F
- BrKd1.0FO
- BrKdKh0.5-0.15
- BrKMts3-1A
- BrKoMts3-10
- BrMg 0.25FO
- BrMg0.25F
- BrMgTsr0.15-0.15F
- BrMgtsr0.15-0.15FO
- БОМц (BrMts0.7-3)
- БрМц12А8Ж3Н2 (BrMtsAZHN12-8-3-2)
- BrMtsS5-21
- BrNTsr
- Bro.VAZh 9-4
- Bro.VAZh9-4L
- Bro.VAZHMts 10-3-1.5
- BrO12
- БО3Н (BrO3Ts17S5N1)
- BrO4TSS17
- БО8С (BrO8S21)
- БрО3Ц12С5 (BrÖCS3-12-5)
- BrOF10-1
- BrOF2-0,25A
- BrOF4-0.25
- BrOF4-0.25A
- BrOF6.5-0.15
- BrOF6.5-0.15A
- BrOF6.5-0.4
- BrOF6.5-0.4A
- BrOF7-0.2
- BrOF7-0.2A
- BrOF8-0.3
- BrOF8-0.3A
- BrOF8.0-0.3
- BrOF8.0-0.3A
- BrOF8.5-0.3
- BrOS1-22
- BrOS16-5
- BrOS5-25
- БрО8С12 (BrOS8-12)
- БрО10С2Н3 (BrOSN10-2-3)
- BrOTs4-3A
- БрО4Ц4С17 (BrOTs4-4-17)
- BrOTs8-4
- БрО3Ц7С5Н1 (BrOTsN3-7-5-1)
- BrOTsS4-4-2,5
- BrOTsS4-4-2,5A
- BrOTsS4-4-4A
- Brs
- CuAg0.1 (BrSr0.1)
- БрС3С30 (BrSS3-30)
- BrSuF6-1
- ВБ24Н (BrSuN6-2)
- ВБ23Нц (BrSuNTSSF3-3-3-20-0,2)
- ВБр2 (BrSuNTSSF4-5-3-20-0.3)
- ВБ23НЦК (BrSuNTSSKF3-3-20-0.6-0.2)
- ВБ-23 (BrSuSF6-12-0.3)
- Brtsr0.5F
- Brtsr0.5FO
- БрТ5Х0,5 (BrTX5-0.5)
- BrX0.7
- BrX0.9
- BrX08T
- BS
- BSP
- Bsr
- БрСу3Н3Ц3С20Ф (BSuS)
- CA0
- CA03
- CA04
- CA10
- CAC1-400
- САС1−400 (CAC1-50)
- ЭК120 (CELLIT-P)
- CfN 0.1
- Ch-09sf
- CH22-VI
- ХН65КВЮТБ (CH24)
- ЧС70-ВИ (CH25-VI)
- ЭИ349 (steel 15Х28)
- Chromel K
- НХМ9 (Chromel KM)
- НХ9,5 (Chromel T)
- НХМ9,5 (Chromel TM)
- ХН58КТВЮМБЛ-ВИ (ChS104-VI)
- 02Х25Н22АМ2-ВИ (ChS108-VI)
- ChS120-VI
- ChS120U-VI
- 03X21Н32М3БУ (CHS33U)
- ХН60МВЮ (ChS40)
- 03Х20Н45М4БРЦ (ChS43)
- ХН55МВЦ (ChS57)
- ХН55МВЦУ (ChS57U)
- ХН36МРЦч-ВИ (CHS59-VI)
- ХН55КВЮМБЛ-ВИ (ChS69-VI)
- ХН58КВТЮМБЛ (ChS70)
- СН25-ВИ (ChS70-VI)
- ChS70U-VI
- ХН60КМВЮТБ-ВИ (ChS71-VI)
- 01Х25Т-ВИ (ChS75-VI)
- 01Х25М2Т-ВИ (CHS78-VI)
- ChS83
- 01Х25Н19Г5АМ4 (ChS84)
- ХН57КВЮТМБЛ-ВИ (ChS88-VI)
- ХН57КВЮТМБРЛ-ВИ (ChS88U-VI)
- 01Х24Н25Г7АМ3Д (ChS89)
- ХН57ВМТЮБЛ-ВИ (ChS91-VI)
- ХН54МВТЮЛ-ВИ (ChS94-VI)
- CHX28N2
- Cladding material 1
- Cladding material 2
- CO 10
- СрМ 50 (CPM 500)
- СрМ 75 (CPM 750)
- CPM 77
- СрМ 77 (CPM 770)
- СрМ 90 (CPM 900)
- СрМ 92,5 (CPM 925)
- СрМ 94 (CPM 940)
- СрМ 95 (CPM 950)
- CPM 960
- CPM 97
- CPU1
- CPU2
- CPU3
- 02Х25Н22АМ2 (CS108)
- 02Х25Н22АМ2-ПТ (CS108-PT)
- 03Х20Н45М5Б (CS32)
- CS33
- 03Х20Н45М4БЧ (CS42)
- 01Х25ТБЮ-ВИ (CS76-VI)
- 07Х15Н30В5М2 (CS81)
- 01Х26Н14ГТ (CS85)
- CT-10
- CT-36
- CT-45
- CT-48
- E-04X10H60M24
- E-04X16H35G6M7B
- E-06X25H40M7G2
- ЦТ-28 (E-08H14N65M15V4G2)
- E-08H24N12G3ST
- E-08N60G7M7T
- E-08X20H60M15V3
- E-08X25H60M10G2
- E-09X15H25M6G2F
- E-09X31H8AM2
- E-10H20N70G2M2B2V
- E-10H20N70G2M2V
- E-10H25N13G2B
- E-10X25H13G2
- E-10X28N12G2
- E-11H15N25M6AG2
- E-12X24H14C2
- E-15H28N10S3GT
- E-15H28N10S3M2GT
- E-190K62X29V5S2
- E-200X29N6G2
- E-27H15N35V3G2B2T
- E-28X24N16G6
- E-300X28H4S4
- E-320X25S2GR
- E-350H26G2R2ST
- E-65H25G13N3
- E635
- Св-30Х26Н32С2Б-Ш (EA-40 25/64)
- 29КНБВТЮ (EC20)
- Н70ВТЮ (EC27)
- ХН80МТЮ (EC50)
- 35НКГ (EC53)
- 08Х20Н25М6Г8 (EC56)
- Х33ТМДЮ (EC63)
- 03Х26Н6Т (EC65)
- 01Х29Н35Г8АМ4Д (EC66)
- ХН65КВМЮТБ (EC78)
- ХН59ВГ (EC82)
- 03Х23Н28Ю4Т (EC86)
- ECDE
- ECEF
- Eh
- Ehf
- Х15Н60 (EHN60)
- Х20Н80 (EHN80)
- EI101
- EI124
- EI125
- EI126
- EI139
- Х25 (EI181)
- EI194
- XH56MBTЮ (EI199)
- EI220
- EI25
- Х25С3Н (EI261)
- EI264
- EI265
- EI27
- EI270
- EI271
- EI278
- 20Х25Н20С2 (EI283)
- EI292
- EI307
- EI316
- 20Х23Н13 (EI319)
- EI331
- EI332
- ХН80 (EI334)
- EI340
- EI346
- 15Х28 (EI349)
- 03Х21Н21М4ГБ (EI35)
- EI360
- EI362
- EI363
- EI364
- EI384
- EI389
- Св-10Х16Н25АМ6 (EI395)
- 10Х17Н10Г4МБЛ (EI402ML)
- EI412
- ВК36А (EI416)
- 20Х23Н18 (EI417)
- EI418
- Х14Н75Т3Ю (EI421)
- EI422
- EI424
- ХН78Т (EI435)
- ХН77ТЮР (EI437)
- EI437-VD
- ХН77ТЮ (EI437A)
- EI437B
- ХН77ТЮР-ВД (EI437B-VD)
- ХН77ТЮРУ (EI437BU)
- EI437BU-VD
- 15Х25Т (EI439)
- EI441
- ХН70 (EI442)
- ХН72МТЮ (EI444)
- EI445
- EI445R
- EI447
- EI457
- EI460
- Хастелой В (EI461)
- EI465
- 50Н (EI467)
- EI470
- EI473
- EI485
- EI499
- EI507
- EI513
- EI518
- EI521
- EI528
- ХН65ВКМБЮТЛ (EI539LMU)
- EI544
- EI556
- ХН60Ю (EI559)
- EI559A
- EI560
- 47НХ (EI563)
- EI568
- EI57
- EI570
- EI574
- EI59
- EI594
- ХН70МВТЮБ (EI598)
- ХН70МВТЮБ-ВД (EI598-VD)
- ХН70МВТЮБ-ВИ (EI598-VI)
- ХН75МБТЮ (EI602)
- EI604
- ХН80ТБЮ (EI607)
- ХН80Т1БЮ (EI607A)
- EI608
- ХН35ВТ (EI612)
- ХН35КВТ (EI612K)
- EI615
- ХН70ВМТЮ (EI617)
- EI617-VI
- EI618
- EI619
- EI620
- EI621
- EI622
- EI623
- EI624
- EI625
- Х27Ю5Т (EI626)
- 06ХН28МТ (EI628)
- 12ХН28МДТЛ (EI629)
- EI630
- 32НКД (EI630A)
- EI632
- EI633
- EI638
- 67Н26М (EI639)
- ХН70Ю (EI652)
- EI653
- Х28АН (EI657)
- EI661
- EI668
- Н33Ю1 (EI674)
- EI675
- 52Н (EI676)
- 47НХР (EI677)
- EI688
- ХН35ВМТ (EI692)
- 48НХ (EI693)
- EI696M
- EI696M-SH
- 10Х11Н23Т3МР (EI696M-VD)
- ХН73МБТЮ (EI698)
- ХН73МБТЮ-ВД (EI698-VD)
- 36ХНТЮ (EI702)
- ХН38ВТ (EI703)
- EI703-Sh
- ХН38ВТ-ВД (EI703-VD)
- ХН38ВБ (EI703B)
- ХН35ВТР (EI725)
- Х20Н70ВЗЮ2Б (EI728)
- Х60МБ (EI758)
- ХН70ВМЮТ (EI765)
- EI766
- EI774
- EI775
- EI776
- EI777
- EI778
- EI779
- EI780
- EI781
- EI782
- EI786
- ХН35ВТЮ (EI787)
- ХН35ВТЮ-ВД (EI787-VD)
- EI788
- EI789
- 58Н (EI792)
- 58Н-ВИ (EI792-VI)
- EI795
- EI799
- EI812
- EI813
- EI824
- ХН70ВМТЮФ (EI826)
- ХН70ВМТЮФ-ВД (EI826-VD)
- EI826-VI
- ХН75ВМЮ (EI827)
- ХН70МВЮ (EI828)
- 12Х25Н16Г7АР (EI835)
- 12Х25Н16Г7АР-Ш (EI835-Sh)
- EI844BSh
- EI855
- EI857
- EI858
- EI859
- EI860
- EI862
- EI863
- EI864
- EI865
- EI866
- ХН62МВКЮ (EI867)
- ХН62МВКЮ-ВД (EI867-VD)
- ХН60ВТ (EI868)
- ХН60ВТ-П (EI868-P)
- ХН60ВТ-ВД (EI868-VD)
- ХН75ТБЮ (EI869)
- EI87
- EI871
- EI872
- EI873
- EI887
- ХН65ВМТЮ (EI893)
- ХН65ВМЮТЛ (EI893L)
- ХН56ВЮТМР (EI894)
- EI905
- ХН55ВМТКЮ (EI929)
- ХН55ВМТКЮ-ВД (EI929-VD)
- EI929A
- EI941
- EI942
- EI943
- EI954
- EI957-VD
- EI963
- EI964
- EI965
- EI966
- ХН50ВМТЮБК (EI969)
- EI974
- Св-09Х16Н25М6АФ-Э (EI981)
- Св-09Х16Н25М6АФ (EI981A)
- EI991
- 40КХНМ (EI995)
- 97НЛ (EI996)
- 95НЛМ (EI996M)
- 95НЛВФ (EI996V)
- ХН50МГЮ (EK1)
- EK100
- ХН69МБЮТВФ-ИД (EK100-ID)
- EK100-VD
- ХН45ТЮ (EK101)
- ХН33КВЮ (EK102)
- ХН33КВЮ-ИД (EK102-ID)
- ХН33КВЮ-ВИ (EK102-VI)
- ХН68КМБТЮ-ИД (EK104-ID)
- EK106
- ХН63ВФБЮТ-ВИ (EK107-VI)
- EK109-VI
- EK112-VD
- ХН65МБ (EK114)
- EK115
- EK116
- EK120
- EK121
- EK122
- EK141
- EK142
- EK143
- 10Х16Н25Г5АМ6 (EK144)
- EK145
- EK146
- EK147
- 03Х20Н70Г3Б3Т (EK148)
- EK150
- ХН63ВФБЮТ (EK151)
- ЭК79У-ИД (EK151-ID)
- EK152-ID
- EK155
- EK156
- ХН56МДБ (EK157)
- EK158
- EK16
- 36НКВХБТЮ (EK162)
- ХН50КВТ (EK167)
- ХН58МБЮ (EK171)
- ХН40М5Т2ГЮБР-ИД (EK173-ID)
- ХН60МВЮБ (EK174)
- 05Х22Н10Г6АМ2 (EK179)
- EK2
- 29КНБВТЮ-ВИ (EK20-VI)
- Св-ХН64КБМЮВФ (EK22)
- 03Х25Н14Г2ФБТ (EK23)
- НВ10 (EK31)
- 25Х15КЮБФ (EK33)
- 42Х25Н35Г6Б2Р (EK35)
- 42Х25Н35С2Г6Б3В3Р (EK36)
- 12Х25Н33С3Г6БР (EK37)
- 20Х27Н6М3АГ2В (EK38)
- ХН35В6ТЮ (EK39)
- 30Н25КТЮ (EK4)
- 02Х21Н25М5ДБ (EK5)
- ХН45ЮБЦ-ИД (EK54-ID)
- 36НХКБТЮ (EK55)
- ХН61МТВБЮ (EK57-VD)
- ЭП693М (EK58)
- ХН70БДТ (EK59)
- Св-02Х21Н25М5ДБ (EK5U)
- 36ХНЮФ (EK6)
- ХН58МБЮД-ИД (EK61-ID)
- ХН58МБЮ-ВД (EK61-VD)
- ХН56МБЮД-ИД (EK62-ID)
- ХН56МБЮ-ВД (EK62-VD)
- ХН65ВБ (EK64)
- EK69
- 42НХЮ (EK71)
- EK74-ID
- ХН68БЮФ-ВД (EK74-VD)
- EK75
- ХН30МДБ (EK77)
- ХН65КВМЮТБ–ВД (EK78-VD)
- ЭП742У (EK79)
- ХН52БМКТЮ-ИД (EK79-ID)
- EK79U
- ХН59ВГ-ИД (EK82-ID)
- EK84-VD
- EK9-VD
- EKDB
- EKES
- EL3-NV-1
- ELP
- EN AC-21100
- EP105-VD
- EP108
- EP109
- EP109-VD
- EP110
- EP114
- EP116
- EP118
- EP119
- EP122
- EP125
- EP126
- EP126-VD
- EP128
- EP129
- EP130
- Х18К60В14Н11 (EP131)
- EP135
- EP138
- 33НК (EP139)
- EP14
- EP140
- EP147
- EP148
- EP15
- ХН36МГБТЮР (EP150)
- EP151
- EP163
- 08Х15Н24В4ТР (EP164)
- 08Х15Н24В4ТР-ш (EP164-Sh)
- EP179
- Н95Г (EP18)
- EP180
- 08Г35Ю6М2 (EP181)
- EP185
- EP192
- EP193
- EP194
- EP195
- EP196
- СВ-30Х15Н35В3Б3Т (EP198)
- ХН56ВМТЮ (EP199)
- ХН56ВМТЮ-ВД (EP199-VD)
- ХН67МВТЮ (EP202)
- EP202-VD
- EP203
- EP204
- EP205
- EP206
- 49К2Ф (EP207)
- Н36ХТЮР (EP215)
- EP216
- EP217
- EP219
- EP22
- EP220
- EP220-VD
- EP220A
- EP221
- EP226
- EP23
- 74НМД (EP233)
- EP235
- EP237
- EP238
- ХН58ВМКЮР-ВД (EP238-VD)
- EP239
- EP240
- EP244
- EP251
- EP252
- EP254
- EP255
- ХН23МТЮР (EP260)
- EP262
- 10Х32Н8 (EP263)
- 77НМД (EP264)
- EP265
- EP267
- 68НМ (EP271)
- EP282
- EP283
- EP284
- EP285
- EP286
- EP29
- EP296
- 36Н11Х (EP297)
- 47НД (EP314)
- 42Н (EP318)
- EP323
- EP33
- EP33-Sh
- EP33-VD
- EP333
- EP334
- ХН40Б (EP337)
- EP337- (RI + VD)
- ХН40Б-Ш (EP337-Sh)
- ХН40Б-ВД (EP337-VD)
- ХН40Б-ВИ (EP337-VI)
- 00Х19Н40Б (EP337U)
- EP338
- EP339
- EP346
- ХН46Б (EP350)
- EP356
- EP36
- EP360
- EP361
- EP362
- EP367
- EP37
- iX15H55M16B (EP375)
- 40Х15Н7ГФ2МС (EP388)
- Св-08Х25Н13БТЮ (EP389)
- EP393
- EP4
- 06Х24Н6ТАФМ (EP401)
- EP409
- EP415
- EP419
- EP420
- EP421
- EP422
- EP423
- 20Х12ВНМФ (EP427)
- ВУС-1 (EP431)
- ВУС-1-ВИ (EP431-VI)
- EP432
- EP435
- ХН30МВТ (EP437)
- ХН30ВМТ-ВД (EP437-VD)
- ХН22МТ (EP453)
- ХН55МВЮ (EP454)
- ХН59ВМТКЮ (EP455A)
- 30НГ (EP456)
- ХН82ТЮМБ (EP460)
- Х15Н24В4Т2Р1 (EP467)
- ХН35В (EP468)
- EP469
- EP474
- 32НК (EP475)
- 32НК-ЭЛ (EP475-EL)
- 32НК-ВИ (EP475-VI)
- EP481
- 35КХ8Ф (EP482)
- 10Х15Н28В2М4Б (EP485)
- ХН60МВТЮ (EP487)
- ХН60МВТЮ-ВД (EP487-VD)
- EP487RL-ID
- 35Г26Х14М (EP488)
- EP489
- EP493
- EP494
- Nistelle B-2C (EP495-VI alloy)
- Х15Н23М7Г7 (EP497)
- EP498
- 36НХТЮ5М (EP51)
- EP512
- EP512a
- EP513
- EP514
- 03ХН28МДТ (EP516)
- EP518
- 36НХТЮ8М (EP52)
- EP520
- EP520A
- 10Х16Н25М6Г6 (EP521)
- EP527
- Х32Н8М2Д2 (EP528)
- 10Х32Н4Д-ВД (EP529-VD)
- 08Х25Н20С3Р1 (EP532)
- Св-08Х20Н57М8В8Т3Р-ИД (EP533-ID)
- 04Х32Н8-ВД (EP535-VD)
- 52Н-ВИ (EP536)
- ХHбOMOBT (EP537)
- EP538
- EP539
- ХН60МЮВТ-ВД (EP539-VD)
- EP540
- ХН40МДТЮ (EP543U)
- ХН40МДТЮ-ИД (EP543U-ID)
- 31НХЗГ2 (EP544)
- 31НХ3Г (EP545)
- 32НХ3 (EP546)
- 33НХ3 (EP547)
- Х15Н60Ю3А (EP548)
- EP554
- EP555
- EP556
- ВУКС1 (EP557-VI)
- 49КФ-ВИ (EP558)
- ХН65МВ (EP567)
- ХН50ВМТКФЮ (EP57)
- ХН50ВМТКФЮ-ВД (EP57-VD)
- 68НХВКТЮ (EP578)
- 68НХВКТЮ-ВИ (EP578-VI)
- EP579
- 08Х17Н15МЗТ (EP580)
- 49КФ (EP581)
- Св-06Х15Н35Г7М6Б (EP582)
- EP584
- EP585
- EP59
- ХН57МТВЮ (EP590)
- ХН57МТВЮ-ВД (EP590-VD)
- ХН57МТВЮ-ВИ (EP590-VI)
- EP591
- Х11Н60М23 (EP595)
- EP596
- EP616A
- EP616B
- EP629
- 75Н34Х8Г3 (EP636)
- Х15Н70М10В2ТЮ (EP643)
- ХН50ВМТЮБ (EP648)
- ХН50ВМТЮБ-ИД (EP648-ID)
- ХН50ВМТЮБ-ВИ (EP648-VI)
- Св-05Х20Н9ФБС (EP649)
- ХН32Т (EP650)
- EP651
- EP652
- EP653
- EP654
- EP656
- EP660
- EP662
- EP663
- Н50К10 (EP664)
- EP665
- ХН55МБЮ (EP666)
- ХН55МБЮ-ВД (EP666-VD)
- ХН50 (EP668)
- EP669
- EP670
- EP671
- EP672
- Св-08Х25Н40М7 (EP673)
- 08Х15Н25Т2МФР (EP674)
- Св-Х25-Н40М7 (EP675)
- EP677
- EP683
- ОХ18Н11 (EP684)
- 27КХ (EP685)
- EP686
- EP687
- EP691
- ХН68ВМТЮК (EP693)
- ХН68ВМТЮК-ВД (EP693-VD)
- ЭК58 (EP693M)
- 10Х14Н16Б (EP694)
- 10Х15Н27Т3МР-ВД (EP700-VD)
- 08Н60Г8М7Т (EP705)
- ХН62ВМЮТ (EP708)
- ХН62ВМЮТ-ВД (EP708-VD)
- ХН62БМВЮ-ВД (EP709-VD)
- EP710
- Н95С3Ю (EP711)
- 36НХ (EP713)
- ХН45МВТЮБР (EP718)
- ХН45МВТЮБР-ИД (EP718-ID)
- ХН45МВТЮБР-ПД (EP718-PD)
- ХН45МВТЮБР-ВД (EP718-VD)
- EP719
- ХК30НВМТ (EP720)
- EP721
- В14М7К25 (EP723)
- EP728
- EP729
- EP730
- ХН40МГ3Б (EP735)
- Х25Н20 (EP74)
- EP741-ID
- ХН62БМКТЮ (EP742)
- EP742-ID
- ХН62БМКТЮ-ИД (EP742-VD)
- ЭК79 (EP742U)
- 00Х20Н42М4В3Б (EP743)
- EP744
- ХН45Ю (EP747)
- EP749
- Св-07Х25Н12Г2Т (EP75)
- 07Х25Н16АГ6Ф-Ш (EP750-Sh)
- 02Х18Н40М5Г2ТФРЮ-ИДД (EP753-DID)
- 01Х18Н40М5ГБ-ИД (EP753-ID)
- 01Х18Н40М5ГБР-ИД (EP753R-ID)
- ХН40МГБТЮР (EP753RTYU)
- 015Х20Н25Г2Б-ИД (EP754-ID)
- EP755
- EP756
- Х50Н70Г5Б2Т (EP757)
- ХН60МБ (EP758)
- ХН63МБ (EP758U)
- ХН63МБ-ВИ (EP758U-VI)
- EP759
- ХН65МВУ (EP760)
- ХН65МВУ-ВИ (EP760-VI)
- ХН45МБ (EP774)
- 07Х25Н16АГЦ (EP781)
- ХН67МБЮ (EP782)
- EP783
- 80Н2М (EP784)
- EP786
- Св-08Х4Н70М12Г6Т (EP787)
- EP789
- EP790
- EP791
- 40ХНЮ-ВИ (EP793-VI)
- EP793A
- ХН58В (EP795)
- 03ХН35МЮ (EP796)
- ХН85МЮ (EP797)
- ХН65КМВЮБ (EP800)
- ХН65КМВЮБ-ВД (EP800-VD)
- 36НГТ (EP802)
- Св-36НГМТ (EP803)
- EP812
- EP813
- Н70МФВ (EP814)
- EP814A
- Н70МФВ-ИД (EP814A-ID)
- Н70МФВ-ВИ (EP814A-VI)
- EP828
- 05Х30Н40М6ТБ (EP829)
- EP834
- EP839
- EP840
- 02Х26Н6-ИД (EP843-ID)
- 4Х25Н20С2 (EP846)
- ХН70В (EP847)
- EP848
- Х40Н50 (EP851)
- 03Х15Н35Г7М6Б (EP855)
- 40Н35Х8Г (EP861)
- 03Х21Н32М3Б (EP864)
- EP867
- КХ30С2В4 (EP869)
- 06Х25Н12ТЮ (EP87)
- 0Х16Н80Б2Т (EP870)
- EP871
- EP872
- Х14Н27М9Г6Б (EP873)
- ХН61КМЮВБ (EP874)
- EP876
- 58НХВКТБЮ (EP877)
- 58НХВКТБЮ-ВИ (EP877-VI)
- ХН60МКБЮТ-ВД (EP879-VD)
- Св-08Х15Н23В7Г7М2 (EP88)
- EP880
- ХН55КМВЮТ-ИД (EP881-ID)
- 07Х25Н50М9К9Б2Г3 (EP883)
- ВЖ121 (EP884)
- ХН62ВМКТЮБ (EP885)
- ХН60ВМБ (EP886)
- EP897
- EP901
- ХН65ВБМЮ (EP902)
- ХН35ВБ-ИД (EP912-ID)
- ХН35ВБ-ВД (EP912-VD)
- ХН60К (EP913)
- ХН65ВМБЮ-ИД (EP914-ID)
- ХН43БМТЮ-ИД (EP915-ID)
- ХН43БМТЮ-ВД (EP915-VD)
- ХН35ЮС (EP919)
- 37НКВТЮ (EP920)
- 37НКВТЮ-ВИ (EP920-VI)
- Н90Ю (EP922)
- EP923
- EP924
- ХН40МДБ (EP937)
- 08Х11Г35МР (EP939)
- 38ХНВЮ-ви (EP940-VI)
- ХН43МГБ-ВИ (EP941-VI)
- ХН40МТЮБР (EP943)
- ХН30МБЮ (EP946)
- ХК42НМ (EP949)
- ХН71МВЮ (EP950)
- Св-03Х20Н45Г6М6Б-ВИ (EP953-VI)
- 03Х24Н13Г2Б (EP955)
- ХН60КВЮМБ (EP957)
- ХН60КВЮМБ-ИД (EP957-ID)
- ХН60КВЮМБ-ВД (EP957-VD)
- ХН57МКЮВТБР-ВД (EP958-VD)
- Х5Н40Г7М8Т (EP960)
- ХН60КМЮБВТФ (EP962)
- ХН60КМЮБВТФ-ИД (EP962-ID)
- EP962U
- ХН50МД (EP963)
- EP964
- 40КНБ (EP966)
- 50Н3ХЮ (EP967)
- ХН50ВМТЮБК-ИД (EP969-ID)
- EP97
- 32Н6ХЮ (EP974)
- EP975
- Н68М (EP983)
- ERH 99.9-MP
- ERH 99.95-MP
- ERH 99.97-MP
- ERH-0
- ERH-1
- ERH-2
- ERX 99.99-MP
- ERX99.9-MP
- ERX99.95-MP
- ERX99.97-MP
- ERX99.99-MP
- ET2
- ET3
- ET5
- EVI-1
- EVI-2
- EVI-3
- EVL
- EVT-15
- EYA3S
- 15Х28, ш (EZH27)
- F-75
- FA30
- FA35
- FA60
- FA65
- FACr15
- FACr18
- FANb17Ti10KU20
- FH010N1SA
- FH010N2SA
- FH50U12
- FH55U10
- FH60U9
- FH650
- FH700
- FH800CA
- FH800SB
- FHB-1
- FHB-2
- FHP850A
- FMN30Ti13
- FMN30Ti18
- FMN30Ti8
- FMN35Ti13
- FMn70
- FMn78
- FMn88
- FMN90
- Fn-1
- Fn-3
- FNb15S15
- FNb20S20
- FNb50S
- FNb55 (f)
- FNb55S
- FNb58
- FNb58 (f)
- FNb60
- FNBA20
- Fng
- Fnkh
- FS10Vd8Mn30
- FS20 (L)
- FS30R3M10 class A
- FS30R3M10 class B
- FS30R3M15 class A
- FS30R3M15 class B
- FS30R3M20 class A
- FS30R3M20 class B
- FS30R3M30 class A
- FS30R3M30 class B
- FS30R3M5 class A
- FS30R3M5 class B
- FS40L15
- FS40L20
- FS40L30
- FS40TS15
- FS40TS20
- FS40TS30
- FS45 (L)
- FS50Mg2
- FS50Mg5
- FS60Ba22
- FS60Tsr1.5Mn1
- FS65 (L)
- FS65A
- FS65Al2
- FS65Ba12
- FS65Ba4
- FS65Ba7
- FS70CR1.5
- FS75 (L)
- FS75Al2.5
- FS75Ba1-6
- FS75Ba1-6
- FS75Ba1-7
- FS75Ba1-7
- FS75F2
- FSA-23
- FSA-30
- FSA-40
- FSCr30
- FSCr40
- FSCr45
- Ф24 (FSH48)
- FSK13Vd4
- FSK15Vd6
- FSK20A3
- FSK25F3
- FSK8A3
- FSK8Vd6
- FSMg5
- FSMg5.5La
- FSMg7
- FSMg9
- FSNb15Ti20tsr5
- FSNb15Ti5
- FSNb20Ti10
- FSNb20Ti15
- FSNb25Ti10
- FSNb25Ti3
- FSNb3Ti15tsr5
- FTi20S40
- FTi50Al16
- Fused
- FVd12S12
- FVd17S12
- FVd20S20
- FVd40U0.5
- FVd40U0.75
- FVd50U0.3
- FVd50U0.4
- FVd50U0.5
- FVd50U0.6
- FVD50U0.75
- H-151
- 24НХ (H-25)
- H-66
- H-68
- Св-07Х25Н13 (H-71)
- Св-13Х25Н18 (H-72)
- Св-30Х25Н16Г7 (H-75)
- H-79
- H-94
- Св-06Х25Н12ТЮ (H-95)
- H-96
- H-97
- H-98
- Св-06Х15Н60М15 (H-99)
- H16N25M6AG
- H18N35
- ХН28ВМАБ (H21N28V5M3BAR)
- H23N13
- H23N18
- H23N33USN
- H24N8M2D3L
- H30
- H36
- 37Н11Х (H36X11)
- ЭИ675 (H38X14)
- H40
- H41XTA
- H42
- H43
- H48
- H48X
- ЭП757 (H50N70G5B2T)
- ЭП960 (H5N40G7M8T)
- ЭИ639; (H70M27)
- ЭК27 (H70VTU)
- HA6
- HA8
- Х80А (HA80)
- НВ3 (HB)
- ЭК31 (HB10)
- High Tin Bronze
- ЭП720 (HK30NVMT)
- ЭП260 (HN23MTYUR)
- ХН30В6М5Ю (HN30B6M5YU)
- ЭК40 (HN30B6M5YU)
- HN30MDB
- ЭП437-ВД (HN30VMT-VD)
- HN33KV-VI
- ЭК102 (HN33KVYu)
- HN33KVYU-ID
- ВЖ145-ВИ (HN33KVYU-VI)
- ЭК39 (HN35B6TYu)
- ЭП912-ИД (HN35BB-ID)
- ЭП912-ВД (HN35BB-VD)
- ЭИ612К (HN35KWT)
- ЭП105-ВД (HN35MTY-VD)
- ЭП919 (HN35US)
- ЭИ787-ВД (HN35VTU-VD)
- ЭП150 (HN36MGBTYUR)
- ЭИ703-ВД (HN38VT-VD)
- ЭП337 (HN40B)
- HN40B-Sh
- HN40B-VD
- ЭП337-ВИ (HN40B-VI)
- ЭК173-ИД (HN40M5T2GUBR-ID)
- ЭП937 (HN40MDB)
- ЭП543У (HN40MDTY)
- ЭП543У-ИД (HN40MDTYU-ID)
- ЭП735 (HN40MG3B)
- ЭК156 (HN40MGBTYUR)
- ЭП943 (HN40MTUBR)
- ЭП915-ИД (HN43BMTYU-ID)
- ЭП915-ВД (HN43BMTYU-VD)
- ЭП941-ВИ (HN43MGB-VI)
- ЭП774 (HN45MB)
- ЭП718 (HN45MTUBR)
- ЭП718-ИД (HN45MVTUBR-ID)
- ЭП718-ПД (HN45MVTUBR-PD)
- ЭП718-ВД (HN45MVTUBR-VD)
- ЭК54-ИД (HN45UBTS-ID)
- ЭК167 (HN50KW)
- ЭП963 (HN50MD)
- ЭК1 (HN50MGYU)
- ЭП57 (HN50VMTKFYU)
- ЭП57-ВД (HN50VMTKFYU-VD)
- ЭП648-ИД (HN50VMTYUB-ID)
- ЭП648-ВИ (HN50VMTYUB-VI)
- ЭП969-ИД (HN50VMTYUBK-ID)
- ЭП220 (HN51 VMTYUKFR)
- ЭП741НП (HN51KVMTYUB)
- ЭП975П (HN52KVMTYUB)
- ЭП741П (HN53KVMTYUB)
- ЭП962П (HN54KVMTYUB)
- ЭП881-ИД (HN55KMVYUT-ID)
- ЭП454 (HN55M6VYu)
- ЭП666 (HN55MBU)
- ЭП666-ВД (HN55MBYU-VD)
- ЭИ929-ВД (HN55VMTKYU-VD)
- ЭК62-ИД (HN56MBUD-ID)
- ЭК157 (HN56MDB)
- ЭП199-ВД (HN56VMTYu-VD)
- ЭП590-ВД (HN57MTVYU-VD)
- ЭП590-ВИ (HN57MTVYU-VI)
- ЭК158 (HN58MB)
- ЭК171 (HN58MBU)
- ЭК61-ИД (HN58MBUD-ID)
- ЭК82 (HN59VG)
- ЭК 82–ИД (HN59VG-ID)
- ЭП455 (HN59VMTKYU)
- ЭП800 (HN60KMVYUB)
- ЭП962 (HN60KMYUBVTF)
- ЭП962-ИД (HN60KMYUBVTF-ID)
- ЭП957 (HN60KVYUMB)
- ЭП957-ИД (HN60KVYUMB-ID)
- ЭП957-ВД (HN60KVYUMB-VD)
- ЭП758У (HN60MB)
- HN60MBVYu
- ЭП879-ВД (HN60MKBYuT-VD)
- ЭП487-ВД (HN60MVTYU-VD)
- ЭК174 (HN60MVYUB)
- ЭП487 (HN60MWTY)
- HN60VT-P
- HN60VT-VD
- ЭП742 (HN62BMKTYU)
- ЭП742-ИД (HN62BMKTYU-ID)
- ЭП709-ВД (HN62BMVYU-VD)
- HN62MVKYU-VD
- HN62VMKYU
- ЭП708 (HN62VMYUT)
- ЭП708-ВД (HN62VMYUT-VD)
- 8-22 (HN63MB)
- ЭП758У-ВИ (HN63MB-VI)
- HN63MBU
- ЭК112-ВД (HN63MYUTBV-VD)
- ЭК107-ВИ (HN63VFBYUT-VI)
- ЭК64 (HN65BB)
- ЭП800-ВД (HN65KMVYUB-VD)
- ЭК78 (HN65KVMYuTB)
- ЭК78-ВД (HN65KVMYUTB-VD)
- ЦЖ24 (HN65KVYUTB)
- ЭК114 (HN65MB)
- ЭП760-ВИ (HN65MVU-VI)
- ЭИ 539ЛМУ (HN65VKMBYUTL)
- ЭП886 (HN65VMB)
- ЭП914-ИД (HN65VMBYU-ID)
- HN65VMYUTL
- ЭК106 (HN67MTVTYUB)
- HN67MVTYU-VD
- HN67VMTYU
- ЭК74-ВД (HN68BYuF-VD)
- ЭК-104-ИД (HN68KMBTYU-ID)
- ЭП693 (HN68VMTYUK)
- ЭП693-ВД (HN68VMTYUK-VD)
- ЭК100 (HN69MBYUTVF)
- HN70BDT
- ЭИ598-ВД (HN70MVTUB-VD)
- ЭИ598-ВИ (HN70MVTUB-VI)
- ЭИ 828 (HN70MVYU)
- HN70VMFTYU
- ЭИ826-ВД (HN70VMTUF-VD)
- HN70VMTYu-VI
- ЭИ698П (HN71MTYUB)
- ЭП950 (HN71MVYU)
- ЭИ698 (HN73MBTY)
- ЭИ698-ВД (HN73MBTYU-VD)
- ЭИ869 (HN75TBU)
- ЭИ437Б-ВД (HN77TYuR-VD)
- HN77TYURU-VD
- ЭИ607A (HN80T1B)
- ЭП797 (HN85MYu)
- HNV1
- HNV2
- HNV3
- HR1
- HRM
- Hx
- Hx 9
- HX 9.5
- HX9.5
- HXM 9
- HXM 9.5
- HXM9.5
- HZHN
- ICD 2.5-0.5
- Invar
- ПлИ90-10 (IPT-10)
- ПлИ 85−15 (IPT-15)
- ПлИ 80-20 (IPT-20)
- ПлИ 75−25 (IPT-25)
- ПлИ 70−30 (IPT-30)
- ПлИ 95−5 (IPT-5)
- ISC
- ISTC
- ISTC16-29-1.8
- ЭИ703-Ш (KhN38VT-Sh)
- KhN45MVYUBR
- KhN45YUB
- ЧС94-ВИ (KhN54MVTN-VI)
- ЧС57 (KhN55MVTs)
- ЧС57У (KhN55MVTsU)
- ЭК9-ВД (KhN60KMYuVTB-VD)
- KhN60VG
- ЭК57-ВД (KhN61MTVBY-VD)
- KhNbN1
- KhNbN2
- KhNiMo1
- KhNiMo2
- L-2
- L-2-1
- L-2-2
- L-2-3
- L-3
- L130
- L141
- L145
- L183
- L199
- L47
- L58
- L62
- LA85-0.5
- LAMSH77-2-0.04
- LAMSH77-2-0.05
- LAMts77-2-0.05
- ЛАМц77-2-0,05 (LAMZ)
- ЛАН59-3-2 (LAN)
- LANKMts75-2-2.5-0.5-0.5
- ЛАЖМц (LAZhMTS66-6-3-2)
- ЛМц58-2Л (LC40Mts1.5)
- Lead nickel silver
- LK62-0.5
- LK75-0.5
- LK80-3l
- LKBO62-0,2-0,04-0,5
- LKS80-3-3
- LMC
- LMcAFA
- LMcAZHN
- LMcAZHNK60-3-2-0.3-0.3-0.3
- LMcZh55-3-1
- LMSh68-0.05
- LMts3
- LMts3A
- LMts68-0.05
- ЛМцА57-3-1 (LMtsA)
- LMtsAJKS
- LMtsK
- LMtsKNS
- LMtsKNS58-3-1.5-1.5-1
- LMtsKS
- LMtsNZHA60-2-1-1-1
- LMtsS58-2-2
- ЛМцСКА (LMtsSKA58-2-2-1-1)
- LMtsZh57-1.5-0.75
- LMtsZhS59-1.3-0.9-0.8
- Ln
- LNKM
- LNKMts49-10-0.3-0.2
- LNKOMTS49-9-0.2-0.2
- LNMts60-9-5
- LO
- LOCK
- LOK59-1-0.3
- LOK62-06-04
- LOMNA49-0.5-10-4-0.4
- LOMsh70-1-0.04
- LOMsh70-1-0.05
- Low Tin Bronze
- ЛЦ40С (LS59-1l)
- LS59-3
- LS60-2
- LS63-2
- LSHHNMDd-45
- LSHNMDd-45
- LV
- LVJ
- M-5
- M-6
- M-60
- M-80
- M1E
- M1O
- M1rO
- M4
- M40
- M99.9
- M99.95
- M99.95-MP
- MA0.8
- MA2-1 p.p.
- MA20-1
- MA3
- MA3-1
- MA5Ts1
- MA6C
- MA6Ts3
- MA6Ts3e
- MA8 p.h.
- MA8B
- MA8TSB
- Manganin
- MBVP
- MCH0
- MCH1
- MCH2
- MCH3
- MCH4
- MCH5
- MCH6
- MCNMts
- MEHMARK 45
- Melchior
- MF
- MFTA-D
- Mg
- Mg-90
- mg04u
- mg04uD
- Mg90C
- Mg95C
- MH0.6
- MH15
- MH23
- MH3
- MH6
- МЦр1Н3 (MILLION)
- MIPA
- MIT-MP
- MIV 0.1-0.05
- MK0.2
- MKLA
- MKLB-2
- MKLPS
- MKLV
- ML-MP
- ML4p
- ML5p
- MMc1
- MMN
- MMS
- MN
- MN2.5KoKrKhr
- Mn70A
- Mn75A
- Mn80A
- MNA
- Куниаль Б (MNA6-1.5)
- НА8 (MNA8-1.5)
- MNAKH11-2.5-1.0-0.8
- 538 (MNAKhMts15-3.5-2-3)
- MNC
- MNMts40-1.5
- MNMts43-0.5
- MNMts5-3.7
- MNMts50-10-5
- MNMts55-6-4
- MNMts60-20-20
- MNMts67.5-9-23.5
- MNMts68-4-2
- MNMtsZh40-1,4-0,25
- MNMtsZh40-1.25-0.45
- молибден (MNS)
- MnS1
- MnS12
- MnS17
- MnS22
- MnS25
- MnSf
- MNZHKT5-1-0,2-0,2
- MNZHMts11-1.1-0.6
- Monel
- MP-47
- MP1
- MPD 0.2
- Mr1O
- MSCh-1
- MSCh-2
- MSH-1
- MSH-2
- MSH-V
- MSp0.1
- MSp0.1F
- MT
- Mts2
- Mts5
- MTsNMts30-10-5
- БрЦр0.3 (Mtsr0.3)
- MV-2-MP
- MV-50
- MV10-MP
- MZH
- MZHMts
- N1-MP
- N31K6
- N35HMV
- N36L
- 42НХТЮА (N41XT)
- 44НХТЮ (N43XT)
- N60MFL
- К-монель (N65D29YUT-ISH)
- эп982-ви (N65M-VI)
- N65M30V5-VD
- N65MFL
- N65MV
- N67M28-MP
- ЭП495-ВИ (N70M-VI)
- N70M27F
- ЭП 814А-ВД (N70MFV-ID)
- ЭП814А-ВИ (N70MFV-VI)
- N70MHYU-VI
- NB-1
- NB-2
- NB-3
- NBP-1a
- NBP-1b
- NBP-2a
- NBP-2b
- NBP-3a
- NBP-3b
- NBP-4
- NHK9-0.9
- Nickel silver
- НКа0,07 (NIKA-1)
- НКа0,13 (NIKA-2)
- NIMO-28
- ЭИ639 (NIMO25)
- NiNb1
- NiNb2
- Niobium alloy
- NJ
- НК0,2 (NK)
- NK0,2E
- NK0.04
- NK0.2
- NK0.2Ev
- Силин (NK2.4)
- NK40
- NKa
- NKa0.07
- НИКА-2 (NKa0.13)
- NlCr0.005F
- NlCr0.005FO
- NlMg0.05F
- NlMg0.05FO
- NlOl0.04F
- NlOl0.04FO
- NM
- NM-40A
- ЭП999 (NM23HU)
- NM23YUV-VI
- NMC
- NMc 2.5
- NMCA
- NMcAT
- NMG0.1
- NMg0.1v
- Nmgv
- NMMtsTA
- NMMtsTA 26-1.5-1.1-0.5
- NMtsAT3.0-1.5-0.6
- NMtsATK1.0-1.5-2.5-0.15
- NMZhMts 28-2.5-1.5
- NMZhMts28-2.5-1.5
- NNbMo15.5-6.5
- NP
- Np-03X15H35G7M6B
- Np-Kh15N60
- Np-Kh20N80T
- NP2Ev
- NUS-5-VI
- ON
- PDP 80-20
- PDP 85-15
- ПР-10 (PDP 90-10)
- ПлПд 95−5 (PDP 950-50)
- PDSR 850-130
- PdTsRH 990-0.7
- PFN
- PH2
- PHA
- PHA97.5
- PHA98.5
- PHA99N5
- ЭК122 (PHN7SR)
- PI 82.5-17.5
- Pic 10
- Pic 18
- Pic 30
- Pic 40
- PIC 61
- PIC 61M
- Pic 63
- Pic 9
- Pic 90
- PINK 24
- PL 70-30
- PL 75-25
- PL 80-20
- PL 85-15
- ЮПдМ-15 (PL 850-150)
- ПлИ 90−10 (PL 900-100)
- ПлН-4,5 (PL 95.5)
- PL 950-50
- Pl 99.8
- Pl 99.9
- Pl 99.93
- Pl 990
- Pl 999.5
- Pl 999.8
- ПлИ 82,5−17,5 (PL-17.5)
- ПЛ-Нп-300Х25С4Н2Г2-Б-У (PL-AN101)
- ПЛ-Нп-500Х40Н40С2ГРЦ-Б-С (PL-An111)
- ПЛ-АН101 (PL-Np-300X25S4N2G2-B-U)
- PL-Np-450X31M-B-U
- ПЛ-Ан111 (PL-Np-500X40H40S2GRZ-BS)
- ПлА-00 (PLA-00)
- PLA-2
- PLAB-0
- PLAB-00
- PLAB-1
- PLAB-2
- PLAp-1
- Pldcd 850-120
- ПлПдРд-4-3,5 (Plddr 92.5-4-3.5)
- ПлПдРдРу 81−15−3,5−0,5 (Plddrdru-15-3.5-0.5)
- PLHMc
- ПлИ 900-100 (PLI 90-10)
- PLI 95-5
- PLM 850
- PLM 900
- ПлМ-8,5 (PLM 91.5)
- PLM 950
- PLM 97.5
- ПлМ 97,5 (PLM-2.5)
- ПлМ 91,5 (PLM-8.5)
- PLM-900
- PLM-950
- ПлН 95,5 (PLN-4,5)
- Plpd 850-150
- ПлМ-10 (Plpd 900-100)
- ПлПд 90−10 (PlPd-10)
- ПлПд 85−15 (PlPd-15)
- PlPd-20
- Plpdga 850-140
- Plpdkr 900-70
- Plpdkr 950-30
- ПлПдРдРу-15-3,5-0,5 (Plpdrd 81-15-3.5-0.5)
- ПлПдРд 92,5−4-3,5 (Plpdrd-4-3.5)
- PPlPdRE 900-80lPdRE 900-80
- Plrd 70-30
- Plrd 80-20
- Plrd 850-150
- PLRd 90-10
- Plrd 900-100
- Plrd 93-7
- PLRd 95-5
- Plrd 950-50
- Plrd 98-2
- ПлРд 90−10 (PlRd-10)
- ПлРд 80−20 (PlRd-20)
- ПлРд 70−30 (PlRd-30)
- PlRd-40
- ПлРд 95−5 (PlRd-5)
- ПлРд 93-7 (PlRd-7)
- ПлРд 92,5-7,5 (Plrd-7.5)
- ПлРу 90−10 (PlRu-10)
- PLT
- Plu 90-10
- PlU 92-8
- PlV 950
- ЛЖС58-1-1 (PLW)
- PM-ERH 99.6
- PM-ERH 99.9
- PM-ERH 99.98
- PM-ERH 99.99
- PM-ERH-1-150
- PM-ERH-1-280
- PM-ERH-4-150
- PM-M
- PM99.95
- PMF 7
- PMFN 8.5-8.5
- PMFOCr6-4-0.03
- PMGr12
- PMGrKr4-2.5
- PMGrN10-1.5
- PMGrN5-2.8
- PMGRO10-2.8
- Сплав 417 (PMGrOB10-1-0.1)
- Сплав 483 (PMGROZHKO 10-1-0.1-0.1)
- PMGrT12-0.25
- ПГ-СР3 (PN-KhN80S3R3)
- ПГ-АН1 (PN-U25H30SR)
- ПГ-С27 (PN-U40H28N2S2VM)
- ПГ-ФБХ6-2 (PN-U45H35GSR)
- ПГ-УС25 (PN-U50H38N)
- ПГ-СР2 (PN-XH80S2R2)
- ПГ-СР4 (PN-XH80S4R4)
- PN73X16S3R3
- PN80X7SR
- PNH20K20Y13
- PNK-1L6
- PNK-1L7
- PNK-1L8
- П200А (POC 10)
- POC 60
- POIN 52
- POMK
- POS 36-17
- POS 50-18
- POSIN 30-25
- POSK 2-18
- POSS 4-6
- POSSU 10-2
- POSSU 15-2
- POSSU 18-0.5
- POSSU 18-2
- POSSU 25-0.5
- POSSU 25-2
- POSSU 30-0.5
- POSSU 30-2
- POSSU 35-0.5
- POSSU 35-2
- POSSU 4-4
- POSSU 4-6
- POSSU 40-0.5
- POSSU 40-2
- POSSU 5-1
- POSSU 50-0.5
- POSSU 61-0.5
- POSSU 8-3
- POSSu50-0.5
- POSU 95-5
- Сплав Розе (POSV-50)
- POTsG 10-1
- POVi 0.5
- PP-AN177
- PP-AN177A
- Pr-3V14KB
- PR-65H25G13N3
- PR-80N12M
- PR-80N15M
- PR-81N3M
- PR-B83
- PR-BrA9
- PR-BrAMts9-2
- CuAl9Fe4 (PR-BrAZh9.5-1)
- PR-BrAZhNMts 8.5-1.5-5-1.5
- PR-BrAZhNMts8.5-4-5-1.5
- PR-BrH
- CuSi3Mn1 (PR-BrKMts3-1)
- PR-BrN15Ol8PSR
- PR-BrO10S10
- PR-BrO4TS4S17
- PR-BrO5TS5S5
- PR-BrO7S10
- PR-BrOF10-1
- PR-BrOF8-0.3
- PR-BrOl8NSR
- PR-BrON8,5-3
- PR-BrOS10-1.5
- PR-HX13SR3
- PR-HX17SR4
- PR-HX31SR
- PR-HX7S4R3
- PR-KX27V4S
- АН35 (PR-KX30N26VS)
- АН34 (PR-KX30N6VSR)
- В3К (PR-KX30VS)
- PR-KX33V18S
- PR-L63
- PR-M2
- PR-ND42SR
- ПГ-АН9 (PR-NH8D6SRP)
- PR-NHX13SR
- PR-NHX16SR4MD3
- PR-NHX25SR3
- PR-NS2R
- ПС22 (PR-NS2R2)
- PR-NS2RP
- PR-NU5
- ПГ-12Н-02 (PR-NX15SR2)
- PR-NX16SR-U
- PR-NX16SR3
- PR-NX7S4R3MD
- PR-NX9S3R2
- PR-POS61
- ПрН-У45Х28Н2СВМ (Pr-S27)
- Pr-V3K
- ПрН-У20ХК57В10 (Pr-V3K-R)
- PR-X20N80
- PR-X30SRNDU
- PR-НХ17СР4-Р
- PR-НХ17СР4-Р
- PR-НХ18С5Р4
- PR-НХ21С5Р
- PR-НХ3С3Р2
- PR-НХ4С3Р
- PRANMts0.6-4-2
- PrMNMts68-4-2
- МцФЖ24-6-0,75 (PrMTsFZh24-6-0.75)
- Пр-В3К (PrN-U10HK63V5)
- Пр-В3К-Р (PrN-U20HK57V10)
- Пр-С27 (PrN-U45H28N2SVM)
- PRV-BrO10
- PRV-BrO15
- PRV-BrO20
- PRV-BrO4
- PRV-BrO4Ts8S5
- PRV-BrO5TS5S5
- PRV-BrZh3
- PRV-D30
- PRV-L63
- PRV-L70
- PRV-L80
- PRV-L90
- PRV-X20N80
- PS22
- PSIN 25
- П250А (Psin 5)
- PSOC 10-1.5
- PSR 1
- PSR 1.5
- PSR 10
- PSr 12M
- PSR 15
- PSR 2
- PSR 2.5
- PSR 2.5C
- PSR 21.5
- PSR 25
- PSr 25F
- PSR 37.5V
- PSr 3cd
- PSR 62
- PSR 63
- PSR 65
- PSR 70
- PSR 71
- PSR 72
- PSr 72V
- PSR 82
- PSR 99.9V
- PSrF 1.0-7.5
- PSrF 1.7-5.5
- PSrF 5-5
- PSrFOl 10-5-5
- PSrGl 3.0-0.01
- PSrKdM 50-34-16
- PSrKdMg 3
- PSrKdNTSrMg 2
- PSrKdTs 1
- PSrKdTs 1-20
- PSrKdTSrMg 3
- PSrLNM 72
- PSrM 25-75
- PSrMGr 15V
- PSrMGrin 40
- PSrMGrin 40V
- PSrMin 49
- PSrMin 63V
- PSrMK 72V
- PSrML 96
- PSrMNTS 38
- PSrMNTS 55
- PSrMO 5
- PSrMO 68-27-5
- PSrMOF 15
- PSrMOGl 70-27-2-1V
- PSrMOin 1
- PSrMOTs 70
- PSrMPd 52-28-22V
- PSrMPd 59-31-10V
- PSrMPd 65-15-19V
- PSrMPd 65-20-15V
- PSrMPd 68-27-5V
- PSrMSu 1.5-24-15
- PSrMSu 22
- PSrMSuF 60
- PSrMTSKd 40
- PSrMTSKd 45-15-16-24
- PSrMtsMN 23
- PSrMtsMN 86.8
- PSrN 39
- PSrO 10-90
- PSro 23
- PSrO 3-97
- ВПР-12 (PSro 5-40)
- PSrOS 2-58
- PSrOS 3-58
- PSrOS 3.5-95
- PSrOSu 8
- PSrS 1
- PSrSu 1-2
- PSrT 29.5
- PSrTsla 12-31-0.05
- PSrTSOA 1,5-41
- PSViO 25-30
- PT-1MB
- PT-3B
- Т7 (PT-7M)
- Ti51Zr49 (PT51T49)
- PTB-56
- Ti70V30 (PTF)
- PTK-1
- PTK-2
- PTM (A) -2
- PTM-1
- PTM-2
- PTOM-1
- PTOM-2
- PTS-1
- PTS-2
- PZlSrKdM750-30
- PZlSrPd 750-75-100
- Resist 30
- Resist 60
- Resist 70
- Resist 80
- RN-6
- S-20
- S-27
- S-30
- S18000
- S18150
- S18200
- 1019 (SAP1)
- 1029 (SAP2)
- 1039 (SAP3)
- SCCR2
- SDP-1
- SDP-11
- SDP-11A
- SDP-12
- SDP-13
- SDP-2
- SDP-3
- SDP-3A
- SDP-4
- SDP-6
- SDP-8
- АК12пч (SIL-0)
- АК12оч (SIL-00)
- АК12ч (SIL-1)
- АК12ж (SIL-2)
- Sintered
- SK10Mg6
- SK10Mg9
- SK15A2
- SK15Mg6
- SK15Mg9
- SKBA5
- SKTi10
- SKTi15
- SKTi5
- SkVd4
- SLSr 100
- SLSr 1000
- SLSr 250
- SLSr 50
- SLSr 500
- Solder A
- SP 17
- ПТ-3В (SP-3V)
- SP15
- SPD2-VI
- Spheremage 7
- Spheromag 500
- Spheromag 5212
- Spheromag 600
- Spheromag 6004
- Spheromag 600P
- Spheromag 610LSi
- Spheromag 611
- Spheromag 611LSi
- Spheromag 621LSi
- Spheromag 6509
- Spheromag 700
- Spheromag 731
- Spheromag 9104
- Spheromag 921
- Spheromag 923
- Spheromage 7103
- Spheromage 711
- Spheromax
- Spheromax 915
- Sprabond
- Spraying
- SRCR 998
- SRCR 998M
- SRK20
- SRKd 86-14
- SRKdG 1-1
- SRKdin 72.5
- SRKdN 755
- SRM 50
- SRM 75
- SRM 8-92
- SRM 80
- СрМ 80 (SRM 800)
- СрМ 83 (SRM 830)
- СрМ 875 (SRM 87.5)
- СрМ 87,5 (SRM 875)
- SRM 90
- СрМ 916 (SRM 91.6)
- СрМ 91,6 (SRM 916)
- СрМ 925 (SRM 92.5)
- SRM 925V
- SRM 930
- SRM 94
- SRM 95
- SRM 96
- СрМ 97 (SRM 970)
- SrMgN 99
- SRMgntsr 99
- SrMgtsr 99
- SRMTs 80
- SRMts 85
- SRN 70
- SRN 90
- Srncrnb 89
- SRNM 2-20
- SRNMB 78
- SRNMin 78
- SRPd 60-40
- SRPd 70-30
- SRPd 80-20
- SRPd 84.5-14.5
- Srpd-20
- СрПд 80−20 (SRPd20)
- Srpdm 50-20
- SrPdM-30-20
- SrPdMg 20-0.3
- Srpl 88-12
- Srpl 96-4
- SrPL-12
- СрПл 96−4 (SrPL-4)
- SRRC 89
- SRSm 98-2
- SS3M-1
- SS3M-2
- SShr 1
- SShr 10
- SShr 20
- SShr 5
- SShr 50
- SShSr 100
- SShSr 250
- SSu10MT
- SSu80l16MT0.1
- SSuA8
- SSuS
- SSuS1
- SSuS2
- SSZP-1
- SSZP-2
- ST00
- STAINLESS
- ЭИ439 (Steel 15X25T)
- STR 1C
- STR 2C
- Superinvar
- Superpermendure
- SUPPORT 36-4
- SUPPORT 42-10.5
- Sv1557pch
- Svr 20
- Svr 40
- Svr 50
- SvSrM 100
- SvSrM 40
- Syn 20
- Syn 50
- ХН63МЮТБВ-ВД (SZHL800-VD)
- T-590
- T-MF
- T-SM
- T00
- T10
- T100
- ВТ1-1 (T11)
- ВТ1-2 (T12)
- ВТ14 (T14)
- ВТ16 (T16)
- ВТ20 (T20)
- ВТ22 (T22)
- ВТ23 (T23)
- ВТ25 (T25)
- T27U63-MP
- T3
- ВТ32 (T32)
- T4
- T43Y49K8-MP
- T43Y57-MP
- T47YU53-MP
- ВТ5 (T5)
- T51
- T54Y46-MP
- T59Y41-MP
- T6
- T64Y36-MP
- ПТ-7М (T7)
- T8
- МН16 (TB alloy)
- ТГ-100 (TG-100M)
- ТГ-110 (TG-110M)
- ТГ-120 (TG-120M)
- ТГ-130 (TG-130M)
- ТГ-150 (TG-150M)
- ТГ-90 (TG-90M)
- ТГ-Тв (TG-TVM)
- TGP-56
- TH-1
- TL3
- TL5
- TN-1K
- МН0,6 (TP alloy)
- TS
- TsAM0.2-4
- TsAM10
- TsAM10-1
- TsAM10-5CH
- TsAM4
- ЦА4М3 (TsAM4-3)
- TsAM41
- TsAM43
- TsAM5-10
- TsAM9
- ЦАМ9-1,5Л (TsAM9-1,5)
- TsAM9-1,5Ch
- ЦАМ9−1,5 (TsAM9-1,5L)
- TShG-56
- TShH-56
- TShP-56
- TsL-25/1
- TsL-25/2
- TsM-10VD
- TsM-2A
- TsM-6
- TSM-7
- TsN-2
- TsN0.5
- TsNA
- ХН70КВМЮТЛ (TsNK17P)
- ХН60КВМЮТБЛ (TsNK21P)
- ХН60КВМЮТЛ (TsNK7P)
- ХН58ВКМТЮБЛ (TsNK8MP)
- TsS-1
- 10Х15Н24В5ТЮРЛ (TsZh11R)
- TT 48-4206-33-11
- TU
- TU 1870-258-00196109-01
- TU 48-19-245-84
- TU 48-19-315-89
- TV 56
- TV-MP
- TYPE-56
- Ultrapure metal
- UN13DK25A
- UN13DK25BA
- UN14DK25A
- UND4
- UND8
- UNDK31T3BA
- UNDK34T5
- UNDK35T5
- UNDK35T5AA
- UNDK38T7
- UNDK40T8
- ЮНДКТ8АА (UNDK40T8AA)
- Алниси (UNS)
- UONI-13 / N1-BK
- US-1
- УС-1СМ (US-1M)
- УС-1М (US-1SM)
- UT-1
- UT-2
- UT-3HP
- UT-3PM
- UT-4
- Wed 10
- Wed 10
- Wed 99.9
- Ср 999,9 (Wed 99.99)
- Wed 99.99An
- Ср 99,90 (Wed 999)
- Ср 99,99 (Wed 999.9)
- Wed 999.9
- Wed 999.9 m
- СрПд 70−30 (Wed-30)
- СрПд 60−40 (Wed-40)
- СрПл 88−12 (Wedpl 12)
- Wood Alloy
- ЭП595 (X11H60M23)
- ЭИ696М (X12N22T3MR)
- ЭП873 (X14N27M9G6B)
- X15H24V4T
- ЭП700 (X15H27T3MR)
- X15H55M16B
- X15H60M15
- X15H60T
- ЭП548 (X15N60YU3A)
- ЭП643 (X15N70M10B2TYu)
- ЭП131 (X18K60V14N11)
- X20H80 99.9-MP
- ЭП998 (X20N73YUM)
- X20N75YU-VI
- X20N80T3
- X25
- X25N13ATL
- X25N16G7AR
- X25N20C2
- X25N28M3D3
- X25N40M7
- ВХ-6 (X25N45V30)
- X25N6ATMF
- X25T
- X27U5
- X28
- X28-VI
- X28N48V5
- X28N48V5L
- X28N6M3AG2
- X28N8
- X32N8
- ХА2 (X60A)
- ХА1 (X70A)
- X75A
- X75B
- ХА80 (X80A)
- X80Ni20A
- X80Ni20B
- X80Ni20V
- X97.5
- X98.5
- Х70А (XA1)
- Х60А (XA2)
- ЭП126-ВД (XH28VMAB-VD)
- XH30V5MT
- ЭП437 (XH30VMT)
- ЭП985 (XH32TY)
- ЭК 63 (XH33TMDYU)
- ЭИ612-ВД (XH35VT-VD)
- XH40B- (RI + VD)
- XH40MTYUBF
- XH40MTYUBFR
- ВВ750П (XH50KVMTYUB)
- ЭП99-ИД (XH50MVKTYUR-ID)
- ЭП99 (XH50VMKTYUR)
- ЭП648 (XH50VMTYUB)
- XH50VMTYUB-VD
- XH50VTMUB-VD
- XH51MTYUKFR
- ВЖ175 (XH54K15MBYuVT)
- ЭК101 (XH54TY)
- ЭК151 (XH55K15MBYuVT)
- ЧС69-ВИ (XH55KVYUMBL-VI)
- XH55MTYUB
- ЭП881 (XH55MVKTYUR)
- XH55VMKYU
- XH55VMTFKYU
- XH55VMTKYUA
- XH55VMYUBT
- ВЖ172 (XH56K16MBVYUT)
- 8-11 (XH56KMYUBVT)
- ВВ751П (XH56KVMTYUB)
- ЭК155 (XH56KVTYUBM)
- XH56MBUD-VD
- XH56VMKTYUF
- ЭП109-ВД (XH56VMKYU-VD)
- Чс88-ВИ (XH57KVYUTMBL-VI)
- ЧС88У-ВИ (XH57KVYUTMBLL-VI)
- XH57VKYUTMBL-VI
- ЧС91-ВИ (XH57VMTUBL-VI)
- ЧС104-ВИ (XH58KTVYUMBL-VI)
- ЧС70У-ВИ (XH58KVTUMBL-VI)
- ЭК61-ВД (XH58MBUD-VD)
- ЭК16 (XH58MTVE)
- ЦНК8МП (XH58VKMTYUBL)
- ЭП975 (XH59KVYUMBT)
- XH60KMVTYUB-ID
- ЧС71-ВИ (XH60KMVYUTB-VI)
- XH60KMYuVTBR-VD
- ЦНК21П (XH60KVMYUTBL)
- ЦНК7П (XH60KVMYUTL)
- XH60M
- ЭИ618 (XH60VMTYUR)
- ЭК22 (XH64KBMYUVF)
- ЗМИ3 (XH64VMKYUTL)
- XH65KMVYUTL
- ЭИ893Л (XH65VMTUL)
- ЭИ698МП (XH66VMTYUB)
- ЭК74-ИД (XH68BUYF-ID)
- XH68MVKYUTB
- XH68VKTYU
- XH70BT
- ЦНК17П (XH70KVMYUTL)
- ЭК109-ВИ (XH70M-VI)
- ЧС70 (XH70VMTKB)
- XH70VMTYUF-VI
- ЭИ444 (XH72MTU)
- XH75MT
- XH75VMFU
- XH80TBUA
- МЖЖ9.3-0.5
- МНАЖМц6-0.8-0.8-0.6
- 546 (МНАХМц20-4-2.3-4)
- МНАХМц4,5-4,5-0,7-2,5
- МНМцАЖ3-12-0.3-0.3
- Н33Ю1
- ЭП922 (Н90Ю)
- ЭП711 (Н95С3Ю)
- ЭК121 (ПЖК35)
- САВ1
- САВ2
- ФХ010Н1А
- ФХ010Н1Б
- ФХ010Н1СБ
- ФХ010Н2А
- ФХ010Н2Б
- ФХ010Н2СБ
- GS 40 (Х20Н30СЮ-Н-ВИ)
- Х20Н32Т
- ЭК115 (Х20Н40СЮ)
- ЭП350 (Х20Н46Б)
- ЭП453 (ХН22МТ)
- ХН30ВМЮ
- ХН35МВТ
- ХН46Б
- ХН50МБВЮ
- ХН55МВБЦАР-ВИ
- ЭП958-ВД (ХН57МКЮВТБР-ВД)
- ХН60ВМТКЮ
- ЭК116вд (ХН60КМБЮТВФ)
- ЭП539 (ХН60МЮВТ)
- ЭП914 (ХН65ВМБЮ)
- ХН65ВМЮТ
- ХН65МВТЮ
- ХН67ВТЮ
- ЭК100-ВД (ХН69МБТЮВФ-ВД)
- ЭИ442 (ХН70)
- ЭИ334 (ХН80)
- ЭК50 (ХН80МТЮ)
- ШВВ-1
-
Corrosion-resistant ordinary steel
- 02H18N11
- ЭИ844 (03H16N15M3)
- 00Х16Н15М3Б (03H16N15M3B)
- 03H18N11
- 000Х18Н12 (03H18N12)
- ЗИ133 (03H18N16M3)
- ЗИ35 (03H21N21M4GB)
- ЗИ67 (03H22N6M2)
- ЗИ68 (03H23N6)
- 04H17T
- ЭП550 (04H18N10)
- ЭИ684 (06H18N11)
- 07H16N4B
- ЭП288 (07H16N6)
- 0Х10Н20Т2 (08H10N20T2)
- 0Х17Н13М2Т (08H17N13M2T)
- ЭИ580 (08H17N15M3T)
- ЭИ925 (08H17N5M3)
- ДИ21 (08H17N6T)
- КО3 (08H18G8N2T)
- ЭИ402 (08H18N12B)
- 0Х18Н12Т (08H18N12T)
- ДИ77 (08H18Tch)
- ЭП53 (08H22N6T)
- 08HGSBDP
- 08ХГСДП
- 09Х15Н8Ю1 (09H15N8YU)
- ЭП56 (09H16N4B)
- 0Х17Н7Ю (09H17N7YU)
- 0Х17Н7Ю1 (09H17N7YU1)
- НН3Б (0H18N5G12AB)
- НН3 (0H20N4AG10)
- Х14АГ15 (10H14AG15)
- Х14Г14Н3 (10H14G14N3)
- ЭИ432 (10H17N13M3T)
- ЭИ448 (10X17H13M2T)
- ЭИ878 (12H17G9AN4)
- ЭП47 (12H18N10E)
- ЭИ811 (12H21N5T)
- ЭП213 (15H17AG14)
- ЭП502 (15H18N12S4TYU)
- 2Х18Н9 (17H18N9)
- ЭИ100 (20H13N4G9)
- ЭП210 (20H17N2)
- 2Х14Н2 (25H13N2)
- 25Х17Н2В (25H17N2V-W)
- 30H10G10
- 35K
- 65H13
- ЭИ229 (95X18)
- 12Х15Г9НД (AISI 201)
- 12Х17Г9АН4 (AISI 202)
- 12Х18Н10Е (AISI 303S)
- 03Х18Н11 (AISI 304L)
- 03Х17Н14М3 (AISI 316)
- 03Х16Н15М3 (AISI 316L)
- 10Х17Н13М2Т (AISI 316Ti)
- BOF6
- BOF7
- EI15
- EI287
- EI635
- EP60
- Plpdre 950-25
- Plrd 60-40
-
-
Electrical steel
-
Ferroalloys
-
ferro
-
Ferroboron
-
ferrochrome
- FeCr50C01
- FeCr50C01LP
- FeCr50C03
- FeCr50C03LP
- FeCr50C05
- FeCr50C05LP
- FeCr50C1
- FeCr50C10
- FeCr50C10LP
- FeCr50C1LP
- FeCr50C1N3
- FeCr50C1N7
- FeCr50C1N7Si
- FeCr50C2
- FeCr50C20
- FeCr50C20LP
- FeCr50C2LP
- FeCr50C40
- FeCr50C40LP
- FeCr50C5
- FeCr50C50
- FeCr50C50LP
- FeCr50C50LS
- FeCr50C50LSLP
- FeCr50C50Si2
- FeCr50C50Si2LP
- FeCr50C50Si2LS
- FeCr50C50Si2LSLP
- FeCr50C50Si4
- FeCr50C50Si4LP
- FeCr50C50Si4LS
- FeCr50C50Si4LSLP
- FeCr50C50Si7
- FeCr50C50Si7LP
- FeCr50C5LP
- FeCr50C70
- FeCr50C70LP
- FeCr50C70LS
- FeCr50C70LSLP
- FeCr50C70Si2
- FeCr50C70Si2LP
- FeCr50C70Si2LS
- FeCr50C70Si2LSLP
- FeCr50C70Si4
- FeCr50C70Si4LP
- FeCr50C70Si4LS
- FeCr50C70Si4LSLP
- FeCr50C70Si6
- FeCr50C70Si6LP
- FeCr50C90
- FeCr50C90LP
- FeCr50C90LS
- FeCr50C90LSLP
- FeCr50C90Si2
- FeCr50C90Si2LP
- FeCr50C90Si2LS
- FeCr50C90Si2LSLP
- FeCr50C90Si4
- FeCr50C90Si4LP
- FeCr50C90Si4LS
- FeCr50C90Si4LSLP
- FeCr60C01
- FeCr60C01LP
- FeCr60C03
- FeCr60C03LP
- FeCr60C05
- FeCr60C05LP
- FeCr60C1
- FeCr60C10
- FeCr60C10LP
- FeCr60C1LP
- FeCr60C1N3
- FeCr60C1N7
- FeCr60C1N7Si
- FeCr60C2
- FeCr60C20
- FeCr60C20LP
- FeCr60C2LP
- FeCr60C40
- FeCr60C40LP
- FeCr60C5
- FeCr60C50
- FeCr60C50LP
- FeCr60C50LS
- FeCr60C50LSLP
- FeCr60C50Si2
- FeCr60C50Si2LP
- FeCr60C50Si2LS
- FeCr60C50Si2LSLP
- FeCr60C50Si4
- FeCr60C50Si4LP
- FeCr60C50Si4LS
- FeCr60C50Si4LSLP
- FeCr60C50Si7
- FeCr60C50Si7LP
- FeCr60C5LP
- FeCr60C70
- FeCr60C70LP
- FeCr60C70LS
- FeCr60C70LSLP
- FeCr60C70Si2
- FeCr60C70Si2LP
- FeCr60C70Si2LS
- FeCr60C70Si2LSLP
- FeCr60C70Si4
- FeCr60C70Si4LP
- FeCr60C70Si4LS
- FeCr60C70Si4LSLP
- FeCr60C70Si6
- FeCr60C70Si6LP
- FeCr60C90
- FeCr60C90LP
- FeCr60C90LS
- FeCr60C90LSLP
- FeCr60C90Si2
- FeCr60C90Si2LP
- FeCr60C90Si2LS
- FeCr60C90Si2LSLP
- FeCr60C90Si4
- FeCr60C90Si4LP
- FeCr60C90Si4LS
- FeCr60C90Si4LSLP
- FeCr70C01
- FeCr70C01LP
- FeCr70C03
- FeCr70C03LP
- FeCr70C05
- FeCr70C05LP
- FeCr70C1
- FeCr70C10
- FeCr70C10LP
- FeCr70C1LP
- FeCr70C1N3
- FeCr70C1N7
- FeCr70C1N7Si
- FeCr70C2
- FeCr70C20
- FeCr70C20LP
- FeCr70C2LP
- FeCr70C40
- FeCr70C40LP
- FeCr70C5
- FeCr70C50
- FeCr70C50LP
- FeCr70C50LS
- FeCr70C50LSLP
- FeCr70C50Si2
- FeCr70C50Si2LP
- FeCr70C50Si2LS
- FeCr70C50Si2LSLP
- FeCr70C50Si4
- FeCr70C50Si4LP
- FeCr70C50Si4LS
- FeCr70C50Si4LSLP
- FeCr70C50Si7
- FeCr70C50Si7LP
- FeCr70C5LP
- FeCr70C70
- FeCr70C70LP
- FeCr70C70LS
- FeCr70C70LSLP
- FeCr70C70Si2
- FeCr70C70Si2LP
- FeCr70C70Si2LS
- FeCr70C70Si2LSLP
- FeCr70C70Si4
- FeCr70C70Si4LP
- FeCr70C70Si4LS
- FeCr70C70Si4LSLP
- FeCr70C70Si6
- FeCr70C70Si6LP
- FeCr70C90
- FeCr70C90LP
- FeCr70C90LS
- FeCr70C90LSLP
- FeCr70C90Si2
- FeCr70C90Si2LP
- FeCr70C90Si2LS
- FeCr70C90Si2LSLP
- FeCr70C90Si4
- FeCr70C90Si4LP
- FeCr70C90Si4LS
- FeCr70C90Si4LSLP
- FeCr80C01
- FeCr80C03
- FeCr80C05
- FeCr90C01
- FeCr90C03
- FeCr90C05
- FH001A
- FH001B
- FH002A
- FH002B
- FH003A
- FH003B
- FH004A
- FH004B
- FH005A
- FH005B
- FH006A
- FH006B
- FH010A
- FH010B
- FH015A
- FH015B
- FH025A
- FH025B
- FH050A
- FH050B
- FH100A
- FH100B
- FH200A
- FH200B
- FH400A
- FH400B
- FH650A
- FH650B
- FH800A
- FH800B
- FH850A
- FH850B
- FH900A
- FH900B
- FHN100A
- FHN100B
- FHN200A
- FHN200B
- FHN400A
- FHN400B
- FHN600A
- FHN600B
-
ferromanganese
- FeMn70C05N5
- FeMn70C05N5LP
- FeMn70C10N5
- FeMn70C10N5LP
- FeMn75C80HP
- FeMn75C80LP
- FeMn75C80MP
- FeMn75C80VHP
- FeMn75C80VLP
- FeMn80C01
- FeMn80C01LP
- FeMn80C05
- FeMn80C05LP
- FeMn80C05N2
- FeMn80C10
- FeMn80C10LP
- FeMn80C15
- FeMn80C15LP
- FeMn80C20
- FeMn80C20LP
- FeMn90C01
- FeMn90C01LP
- FeMn90C05
- FeMn90C05LP
- FeMn90C10
- FeMn90C10LP
- FeMn90C15
- FeMn90C15LP
- FeMn90C20
- FeMn90C20LP
- FMn70 (A)
- FMn70 (B)
- FMn78 (A)
- FMn78 (B)
- FMn88 (A)
- FMn88 (B)
- FMn90 (A)
- FMn90 (B)
-
ferroniobium
-
ferrosilicium
-
ferrosilicochrome
-
ferrosilicomanganese
-
ferrotitanium
-
ferrotungsten
-
Ferrovanadium
-
Metallic and nitrated manganese
-
silicocalcium
-
-
Heat resistant steels and alloys
-
Heat resistant alloys
- 10H15N35V3TYU
- 58NHVKTBYU
- ЭП877-ВИ (58NHVKTBYU-VI)
- Сплав ЭП974 (32Н6ХЮ)
- Н70МФ (EP496)
- Х28-ВИ (EP602-VI)
- EP604
- EP605
- Св-08Х25Н60М10 (EP606)
- EP612
- ХН77СР1 (EP615)
- НХ16С2Р2 (EP616)
- 02Х15Н65М13В3ТЮ (EP642)
- EP642-VD
- СВ-02Х15Н65М13В3ТЮ-ВИ (EP642-VI)
- EP645
- ЭП975ИД (EP975-ID)
- 44НХМТ (EP977)
- 03ХН25МДГБ (EP978)
- Св-03ХН25МДГ (EP979)
- ХН32ТЮ (EP985)
- EP986
- 10Х28Н11С4АД (EP988)
- ХН50МВКТЮР (EP99)
- ХН50МВКТЮР-ИД (EP99-ID)
- 80Х20НС (EP992)
- 18Х12ВМБФР (EP993)
- Сплав ХН56ВМКТЮФ (Alloy EP994-ID)
- ЖС30-ВИ (HA30)
- НХ26С2Р2 (EP616A alloy)
- Сплав Х20Н73ЮМ (Alloy EP998)
- Сплав НМ23ХЮ (EP999 alloy)
- Alloy ANV-300
- ЭП126 (HN28VMAB)
- ЭП670 (HN32T)
- HN33BS
- ЭИ612 (HN35VT)
- ЭИ725 (HN35VTR)
- ЭИ787 (HN35VTYU)
- ЭИ703Б (HN38VB)
- ЭИ703 (HN38VT)
- ЭП747 (HN45YU)
- ЭП220-ВД (HN51VMTYUKFR-VD)
- ХН55М6ВЮ (HN55MVYU)
- ЭИ929 (HN55VMTKYU)
- ЭП109 (HN56VMKYU)
- ЭП199 (HN56VMTYU)
- ЭП590 (HN57MTVYU)
- ЭП238-ВД (HN58VMKYUR-VD)
- ЭП539-ВД (HN60MYUVT-VD)
- ЭИ868 (HN60VT)
- ЭИ559А (HN60YU)
- ЭИ867 (HN62MVKYU)
- ЭИ893 (HN65VMTYU)
- ЭИ202 (HN67MVTYU)
- ЭИ598 (HN70MVTYUB)
- ЭИ617 (HN70VMTYU)
- ЭИ826 (HN70VMTYUF)
- ЭИ765 (HN70VMYUT)
- ЭИ652 (HN70YU)
- ЭИ602 (HN75MBTYU)
- ЭИ827 (HN75VMYU)
- ЭИ437А (HN77TYU)
- ЭИ437Б (HN77TYUR)
- ЭИ437БУ (HN77TYURU)
- ЭИ607А (HN80TBYU)
- L114
- LK4
- Alloy 24NK
- alloy 30BTC-VD
- Steel 1H16N25V5TYu2R
- Steel 250X25V3TL
- V3K
- ВХ4Л-ВИ (VH4L)
- VH4L-VI
- VH6
- ВХ9Л-ВИ (VH9L)
- VH9L-VI
- VHH1
- VK-102
- VZH145-ID
- VZH145-VI
- VZH151-VI
- VZH153-ID
- VZH155
- ВЖЛ1-ВИ (VZHL1)
- VZHL1-VI
- ВЖЛ12Э-ВИ (VZHL12E)
- VZHL12E-VI
- ВЖЛ12У-ВИ (VZHL12U)
- VZHL12U-VI
- VZHL14
- VZHL14-VI
- ВЖЛ14Н-ВИ (VZHL14N)
- VZHL14N-VI
- VZHL16-VI
- ВЖЛ18-ВИ (VZHL18)
- VZHL18-VI
- ВЖЛ2-ВИ (VZHL2)
- VZHL2-VI
- VZHL8
- VZHM4-VI
- VZK
- ЭИ435 (XH78T)
- ЖС16-ВИ (ZHS16)
- ЖС16 (ZhS16-VI)
- ZhS26-VI
- ZhS26U-VI
- ЖС3-ВИ (ZHS3)
- ЖС3 (ZhS3-VI)
- ЖС30 (ZhS30-VI)
- ЖС30М (ZhS30M-VI)
- ZhS32-VI
- ZhS32E-VI
- ZhS36
- ЖС3ДК-ВИ (ZhS3DK)
- ЖС3ДК (ZhS3DK-VI)
- ZHS3LS
- ZhS40
- ZhS47
- ZhS6-KP
- ZhS6F-VI
- ЖС6К-ВИ (ZhS6K)
- ЖС6К (ZHS6K-VI)
- ZhS6N-VI
- ЖС6У-ВИ (ZhS6U)
- ЖС6У (ZhS6U-VI)
- ZhS6UD
-
Heat resistant high alloy steel
- 00Х18Н10Т (03H18N10T)
- 0Х18Х10Т (05H18N10T)
- 06Х16Н15М3Б-ИД (06H16N15M3B)
- ЭП164 (08H15N24V4TR)
- 08H15N25M3TYUB
- 08H16N11M3
- ЭИ680 (08H16N13M2B)
- Х16Н9М2 (08H16N9M2)
- ЭИ732 (08H20N14S2)
- ЭП54 (08H21N6M2T)
- ЭИ694 (09H14N16B)
- ЭИ695Р (09H14N19V2BR)
- ЭИ726 (09H14N19V2BR1)
- ЭИ847 (09H16N15M3B)
- ЭП184 (09H16N16MV2BR)
- 10GN2MFA
- 10ГН2МФА-ВД (10GN2MFA-W)
- ЭИ696-А (10H11N20T2R)
- ЭИ696А (10H11N20T3R)
- ЭП33 (10H11N23T3MR)
- 10Х13П2БС2Н2Д2 (10H13G12BS2N2D2)
- ЭИ404 (10H13SYU)
- 10H15N25M3V3TYUK
- 10H15N25V3TYU
- ЭП841 (10H18N18YU4D)
- 0Х23Н18 (10H23N18)
- 10H25N25TR
- ЭП505 (10H7MVFBR)
- ЭИ962 (11H11N2V2MF)
- ЭП752 (12H12MVFBR)
- 12H14N14V2M
- ЭИ835 (12H25N16G7AR)
- ЭП503 (12H2MV8FB)
- 1Х8ВФ (12H8VF)
- ЭИ961 (13H11N2V2MF)
- ЭИ736 (13H14N3V2FR)
- ЭП369 (15H11MF)
- ЭИ802 (15H12VNMF)
- ЭИ484 (15H18SYU)
- ЭИ962А (16H11N2V2MF)
- ЭП291 (18H11MNFB)
- ЭИ993 (18H12VMBFR)
- 20H12N2V2MF
- ЭП428 (20H12VNMF)
- ЭИ211 (20H20N14S2)
- 3Х13Н7С2 (30H13N7S2)
- ЭИ572 (31H19N9MVBT)
- Сталь ЭП488 (35G26H14M)
- ЭИ481 (37H12N8G8MFB)
- ЭИ107 (40H10S2M)
- ЭИ388 (40H15N7G7F2MS)
- 4Х9С2 (40H9S2)
- эи69 (45H14N14V2M)
- 45H14NMV2M
- ЭП48 (45H22N4M3)
- ЭИ303 (55H20G9AN4)
- ЭП303Б (55H20G9AN4B)
- НХ10С2Р2 (EP616V alloy)
- EP618
- 46НХТ (EP619)
- Св-08Х25Н25М3 (EP622)
- 42ХНМ (EP630U)
- EP635
- EP644
- ХН50ВМТЮБ-ВД (EP648-VD)
- Н65М-ВИ (EP982-VI)
- 02Х20Н25ГМ4Б (EP991)
- Steel 20X25H25TYU
- Steel 20H25N13ATL
- Steel 20H25N19S2L
- Steel 20H25N25TYUL
- Steel 20H25N20SL
- ЭИ319 (Steel 20X23H13)
- ЭИ283 (Steel 20Х25Н20С2)
- ЭИ417 (Steel 20X23H18)
- Steel 30Х23Н7С
- ЭЯ3С (Steel 36X18H25C2)
- Steel 15H25N19S2L
- Steel 15H25N40M2VTL
- VKL-1
-
Heat resistant low alloy steel
-
Heat-resistant relaxation-resistant steel
-
-
Magnesium
-
Materials for welding and soldering
-
Steel welding wire
- 01H23N28M3D3T
- ЭП803 (Alloy 36NGMT)
- Saint-HN23MTYUR
- Saint-HN30V5MT
- Saint-HN50VMTYUB-VI
- ЧС40 (Saint-HN60MVYU)
- Saint-HN77TYuR
- ЭП797-ВИ (Saint-HN85MYU-VI)
- ER308LSi (St-01H19N9)
- ЭП-516 (St-01H23N28M3D3T)
- ER316LSi (St-04H19N11M3)
- ER 308 (St-04H19N9)
- Н-59 (St-04H19N9S2)
- St-04H2MA
- Н-61 (St-05H19N9F3S2)
- ЭИ-649 (St-05H20N9FBS)
- St-06H14
- ЭП-367 (St-06H15N60M15)
- Н-67 (St-06H19N10M3T)
- Н-60 (St-06H19N9T)
- ЭП-89 (St-06H20N11M3TB)
- ЭП-87 (St-06H25N12TYU)
- St-06N3
- Н-62 (St-07H18N9TYU)
- ER347Si (St-07H19N10B)
- ЭП-75 (St-07H25N12G2T)
- ER309LSi (St-07Kh25N13)
- St-08
- St-08AA
- St-08G2S
- St-08GA
- St-08GSMT
- Н-85 (St-08H14GNT)
- ЭП-377 (St-08H16N8M2)
- ЭП-307 (St-08H18N8G2B)
- ЭИ-898 (St-08H19N10G2B)
- St-08H19N10M3B
- Н-63 (St-08H19N9F2S2)
- Н-74 (St-08H20N9G7T)
- Н-73 (St-08H21N10G6)
- ЭП-389 (St-08H25N13BTYU)
- Н-54 (St-08H3G2SM)
- St-08HG2S
- St-08HGSMA
- St-08HGSMFA
- St-08HM
- St-08HMFA
- Н-49 (St-08HMNFBA)
- Н-84 (St-08HN2G2SMYU)
- ЭП-111 (St-08HN2GMTA)
- Н-83 (St-08HN2GMYU)
- St-08HN2M
- St-08HNM
- St-08MH
- St-08N50
- ЭИ-981А (St-09H16N25M6AF)
- St-10 ha
- St-10G2
- St-10G2SMA
- St-10GN
- St-10GSMT
- Н-58 (St-10H11NVMF)
- ЭИ395 (St-10H16N25AM6)
- ЭИ 645 (St-10H17T)
- Н-70 (St-10H20N15)
- St-10H5M
- Н-50 (St-10HG2SMA)
- St-10HM
- St-10HMFA
- Н-51 (St-10HMFT)
- ЭИ-984 (St-10HN2GMT)
- St-10MH
- St-10NMA
- Н-57 (St-12H11NMF)
- St-12H13
- Н-72 (St-13H25N18)
- Н-79 (St-13H25T)
- Н-55 (St-13H2MFT)
- ЭП-439 (St-15GSTYUTSA)
- St-18HGS
- St-18HMA
- St-20GSTYUA
- St-20X13
- Н-75 (St-30H25N16G7)
- St-36NGT
- St. HN38VT
- ЭИ648-ВИ (St. HN60VT)
- St. HN80
- St.-HN28VMAB
- St.-HN28VMAB-VD
- St.-HN38BB
- St.-HN70Yu
- St.-HN70Yu-N
- St.-HN75MBTY
- St.-HN77TYu
- St.-HN78T
- ЭК38 (Steel 20Х27Н6М3АГВ)
- ЧС84 (Sv-01H25N19G5AM4)
- Sv-01H26N14GT
- ЧС83 (Sv-01H29N35G8AM4D)
- ЭП642-ВИ (Sv-02H15N65M13V3TU-VI)
- ЭП642 (Sv-02H15N65M13V3TYu)
- ЭП642-ВД (Sv-02H15N65M13V3TYu-VD)
- Sv-03H15N35G7M6B
- ЭП953 (Sv-03H20N45G6M6B-VI)
- ЭК32 (Sv-03H20N65G5M4B3V)
- Sv-03H20N70G3B3TU
- Sv-03H23N28M3D3T
- Sv-05H30N40M6TB
- ЭП582 (Sv-06H15N35G7M6B)
- Sv-06H20N25M8G8
- ЭП401 (Sv-06H24N6TAFM)
- Sv-06H25N12TYuA
- Sv-07H25N13U
- Sv-08A
- Sv-08G32H10
- Sv-08G35Yu6M2
- Sv-08GS
- ЭП88 (Sv-08H15N23V7G7M2)
- Sv-08H1DYu
- ЭП533-ИД (Sv-08H20N57M8V8T3R-ID)
- ЭП532 (Sv-08H25N20S3R1)
- ЭП622 (Sv-08H25N25M3)
- ЭП673 (Sv-08H25N40M7)
- ЭП606 (Sv-08H25N50M10)
- ЭП787 (Sv-08H4N70M12G6T)
- ЭП705 (Sv-08N60G8M7T)
- Sv-1
- Sv-10H16N25G5AM6
- ЗИ112 (Sv-10H16N25M6AF)
- ЭП521 (Sv-10H16N25M6G6)
- 12ГС (Sv-12GS)
- Sv-12H25N16G7AR
- Sv-12H25N16G7AR-Sh
- Sv-2
- ЭА-40 (Sv-30H26N32S2B-Sh)
- Sv-36NHTYU
- Sv-H11N60M23
- Steel 30Х15Н35В3Б3Т
- ВНС-16 (ZI112)
- 03ХН25МДГ (Св-03ХН25МДГ)
- Св-03ХН25МДГБ
-
-
Metals and alloys
-
Nickel, nickel alloys
-
Granulated nickel superalloy Alloy
-
Low alloyed nickel alloys
-
Nickel alloys
- A-1
- A-2
- CCM
- DNK-0
- DNK-1
- EP601
- EP611
- GOST 31570-2012
- GOST R 51767-01
- K-monel
- Хромель К (NH9)
- NH9.5
- NHC
- Хромель КМ (NHM9)
- NHM9.5
- NK0.2
- NMts1
- NMts2
- NMts2.5
- NMts5
- Алюмель (NMtsAK2-2-1)
- PANCH11
- PV-N55T45
- PV-N70YU30
- PV-N75YU32V
- PV-N85YU15
- PV-NH16Yu6it
- PV-NHX20S
- PV-NX20YU10
- PV-X25YU10
- PV-X25YU6
- VDS-75
- VKLS20-VI
- VKNA-25
- VKNA2L-VI
- VKNA2LK-VI
- VKNA4-VI
- VUKS1
- VZH121
- VZH13
- VZH131-ID
- VZH135-VI
- ZMI3
- ZMI3U
-
Prefabricated Nickel
-
Primary nickel
-
-
Powder metallurgy
-
Aluminum Lumpy Powder
-
Ceramic tools
-
Copper Electrolytic Powder
-
Copper, base powder. Antifriction materials
-
High alloy steels and alloys, powder
-
High speed steel produced by powder metallurgy
-
Iron base powder. Antifriction materials
- ЖК0.3 (PA-LCD)
- ЖД2.5 (PA-Train)
- ЖД5 (PA-ZHD5)
- ЖД3К0.3 (PA-ZHDK)
- ЖФ1К1 (PA-ZHF1K)
- ЖФ0.5К1 (PA-ZHFK)
- ЖФ1К1М2.5 (PA-ZHFKM)
- ЖГр1 (PA-ZhGr)
- ЖГр2 (PA-ZhGr2)
- ЖГр2Д2.5 (PA-ZhGr2D)
- ЖГр3К0.8 (PA-ZhGr2K)
- ЖГр3-20 (PA-ZhGr3)
- ЖГр3М15 (PA-ZhGr3M)
- ЖГрЦс4У (PA-ZhGr3Tss)
- ЖГр0.5Д2.5 (PA-ZhGrD)
- ЖГр1.5Д10 (PA-ZhGrD5)
- ЖГр0.6Д2.8К0.3Ф0.3 (PA-ZhGrDFK)
- PA-ZhGrDFMs
- ЖГр1Д2.5К0.4 (PA-ZhGrDK)
- ЖГр0.5Д3К0.8 (PA-ZhGrDK1)
- ЖГр1.5Д3 (PA-ZhGrDK6)
- PA-ZhGrDMs
- ЖФ1К1Гр0.8 (PA-ZhGrF1K)
- ЖФ0.5К1Гр0.8 (PA-ZhGrFK)
- ЖГр1К0.8 (PA-ZhGrK)
- ЖГр1.5Л (PA-ZhGrL)
- ЖГр(1.0-1.5)Цс4 (PA-ZhGrTss)
- ЖГр1.5Цс401К1 (PA-ZhGrTssOK)
- Х18Н15КБ (PA-ZHH18N15KB)
- Х20КБ (PA-ZHH20KB)
- МГ30ЖН1К (PA-ZhNGr10Tss)
- ЖНГр3М15 (PA-ZhNGr3M)
- Жпор (PAGE)
-
Iron base powder. Materials of construction
- ПК10-6.0 (PK10)
- ПК10Д2Ф-6.0 (PK10D2F)
- ПК10Д3-6.0 (PK10D3)
- ПК10Д3К-6.0 (PK10D3K)
- ПК10Д5-6.0 (PK10D5)
- ПК10Ф-6.8 (PK10F)
- ПК10Х13М2-7.4 (PK10H13M2)
- ПК10Х17Н2-6.8 (PK10H17N2)
- ПК10Х18Н15-6.4 (PK10H18N15)
- ПК10Х18Н9Т-6.4 (PK10H18N9T)
- ПК10Х25-7.4 (PK10H25)
- ПК10Н2Д2-6.4 (PK10N2D2)
- ПК10Н2Д6М-7.4 (PK10N2D6M)
- ПК10Н2М-6.8 (PK10N2M)
- ПК10Н4Д4-6.4 (PK10N4D4)
- ПК20Х13-6.4 (PK20H13)
- ПК40-6.0 (PK40)
- ПК40Д3-6.0 (PK40D3)
- ПК40Д3К-6.0 (PK40D3K)
- ПК40Д3КФ-6.0 (PK40D3KF)
- ПК40Г2-7.4 (PK40G2)
- ПК40Х13М2-7.4 (PK40H13M2)
- ПК40Х2-6.4 (PK40H2)
- ПК40ХН2Г-6.4 (PK40HN2G)
- ПК40Н2Д2-6.4 (PK40N2D2)
- ПК40Н2Д2М-6.8 (PK40N2D2M)
- ПК40Н2М-6.4 (PK40N2M)
- ПК40Н3Д2Х-6.4 (PK40N3D2H)
- ПК40Н4Д2М-6.8 (PK40N4D2M)
- ПК40НМ-6.8 (PK40NM)
- ПК70-6.0 (PK70)
- ПК70Д3-6.0 (PK70D3)
- ПК70Х3-6.4 (PK70H3)
- ПК70Н2Д2-6.4 (PK70N2D2)
- ПКГ13-7.4 (PKG13)
- ПКХ6-7.4 (PKH6)
-
Iron powder
-
Molybdenum powder material
-
Nickel powder
-
Rhenium powder
-
Stainless chromium-nickel steel and nickel powder
-
Tin powder
-
Zinc powder
-
-
Precious metals
-
Gold jewelery
- Zl 999,9
- ZlNTsM585-12.5-4
- ZlNTsM750-7.5-2.5
- ЗлСр 58,5-41,5 (ZlSr585-415)
- ЗлСр 75-25 (ZlSr750-250)
- ЗлСрМ 37,5-10 (ZlSrM 375-100)
- ЗлСрМ 37,5-16 (ZlSrM 375-160)
- ЗлСрМ 37,5-2 (ZlSrM 375-20)
- ЗлСрМ 37,5-25 (ZlSrM 375-250)
- ЗлСрМ 50-10 (ZlSrM 500-100)
- ЗлСрМ 50-20 (ZlSrM 500-200)
- ЗлСрМ 58,5-20 (ZlSrM 585-200)
- ЗлСрМ 58,5-30 (ZlSrM 585-300)
- ЗлСрМ 58,5-8 (ZlSrM 585-80)
- ЗлСрМ 75-12,5 (ZlSrM 750-125)
- ЗлСрМ 75-15 (ZlSrM 750-150)
- ЗлСрМ 90-4 (ZlSrM 900-40)
- ЗлСрМ 93-4,5 (ZlSrM 930-45)
- ЗлСрМ 95-2,5 (ZlSrM 950-25)
- ЗлСрМ 95,8-2 (ZlSrM 958-20)
- ЗлСрМ 96-3 (ZlSrM 960-30)
- ЗлСрМ 97-2 (ZlSrM 970-20)
- ЗлСрМ 98-1,5 (ZlSrM 980-15)
- ЗлСрМ 99-0,5 (ZlSrM 990-5)
- ZlSrNcM 585-80-8,2-2,5
- ZlSrNTs 750-150-7,5
- ЗлСрПд 75-10-15 (ZlSrPd 750-100-150)
- ЗлСрПд 58,5-25,5-16 (ZlSrPd585-255-160)
- ЗлСрПдЦ 58,5-28,7-10 (ZlSrPdC 585-287-100)
- ЗлСрПдКд 58,5-28-10 (ZlSrPdKd585-280-100)
- ЗлСрПдМ 37,5-10-3,8 (ZlSrPdM 375-100-38)
- ЗлСрПдН 75-7-14 (ZlSrPdN 750-70-140)
- ЗлСрПдН 75-9-14 (ZlSrPdN 750-90-140)
- ЗлСрПдНКд 75-9-8,5-4 (ZlSrPdNKd 750-90-85-4)
- ЗлСрПлМ 75-8-9 (ZlSrPlM 750-80-90)
- ZlSrSu 1
- ZlSu 0.1
- ZlSu 1.0
-
Gold, gold alloys
- Evil 2
- Evil 3
- Зл999,9м (Evil-1)
- Evil-1P
- POSOL 78.5
- PZl 583-I
- PZl 583-II
- PZl 583-III
- PZl 583-IV
- PZl 583-V
- PZl 585-I
- PZl 585-II
- PZl 585-III
- PZl 585-IV
- PZl 585-V
- ПЗл585-6 (PZl 585-VI)
- ПЗл 585-VI (PZl585-6)
- PZl585S
- PZl750
- Pzlgr 880
- PZlGrA 88-12-0.2
- PZlKr 970
- PZlKr 980
- PZlM 35V
- PZlM 37.5V
- PZlM 50V
- PZlM 60V
- PZlM 80V
- PZlM 94V
- PZlMN 81.5V
- PZlMSr 69V
- PZlMSr 75V
- PZlN 82.5V
- PZlSr 750-70
- PZlSr 750-95
- PZlSr 750-97
- Зл 99,99Ан (Zl 99.99 An)
- ЗлА-1 (Zl 999,9m)
- Зл999 (Zl99.9)
- Zl99.99
- Зл 99,99 Ан (Zl99.99An)
- ZlA-4
- Zlk 990
- ЗлМ583 (ZlM 58,3)
- ЗлМ 58,3 (ZlM 583)
- ЗлМ900 (ZlM 90)
- ЗлМ 90 (ZlM 900)
- ЗлМ 916 ГОСТ 6835-80 (ZlM 91,6)
- ZlM 916
- ZlM 98
- ZlM 980
- ЗлМ916 (ZlM91.6)
- ЗлМ980 (ZlM98)
- ZlMNC-12.5-10-2.5
- ZlN 75-25
- ZlN 95
- ZlN 95-5
- Zln-5
- ЗлН-5 (ZlN95)
- ZlNCM 585-12.5-4
- ZlPd 60-40
- ZlPd 80-20
- Zlpd 84-16
- ZlPd-16
- ZlPd-20
- ZlPd-40
- ЗлПд-40 (ZlPd60-40)
- ЗлПд-20 (ZlPd80-20)
- ЗлПд-16 (ZlPd84-16)
- ZlPdPl 60-30-10
- ZlPdPl-30-10
- ЗлПдПл-30-10 (ZlPdPl60-30-10)
- ZlPdSr 583
- ZlPdSr 585
- ZlPl 10
- ZlPl 2
- ZlPl 5
- ZlPl 7
- Zlpl 90-10
- ZlPl 93-7
- Zlpl 95-5
- Zlpl 98-2
- ZlPl-10
- ZlPl-2
- ZlPl-5
- ZlPl-7
- ЗлПл-10 (ZlPl90-10)
- ЗлПл-7 (ZlPl93-7)
- ЗлПл-5 (ZlPl95-5)
- ЗлПл-2 (ZlPl98-2)
- ZlPlSrM 750-90-80
- ЗлСр583-417 (ZlSr58.3-41.7)
- ЗлСр 58,3-41,7 (ZlSr 583-417)
- ZlSr 585-415
- ЗлСр600-400 (ZlSr 60-40)
- ЗлСр 60-40 (ZlSr 600-400)
- ЗлСр 750-250 (ZlSr 75-25)
- ZlSr 750-150
- ZlSr 750-250
- ZlSr 750-87
- ZlSr 920
- ЗлСр990-10 (ZlSr 99-1)
- ЗлСр 99-1 (ZlSr 990-10)
- ZlSrCM 585-35
- ZlSrCNM 585-35
- ZlSrKdM 750-30
- ЗлСрМ333-333 (ZlSrM 33,3-33,3)
- ЗлСрМ 33,3-33,3 (ZlSrM 333-333)
- ЗлСрМ 375-100 (ZlSrM 37,5-10)
- ЗлСрМ 375-160 (ZlSrM 37,5-16)
- ЗлСрМ 375-20 (ZlSrM 37,5-2)
- ЗлСрМ 500-100 (ZlSrM 50-10)
- ЗлСрМ 500-200 (ZlSrM 50-20)
- ЗлСрМ 585-200 (ZlSrM 58,5-20)
- ЗлСрМ 585-300 (ZlSrM 58,5-30)
- ЗлСрМ 585-80 (ZlSrM 58,5-8)
- ZlSrM 583-200
- ЗлСрМ 58,3-30 (ZlSrM 583-300)
- ЗлСрМ 58,3-8 (ZlSrM 583-80)
- ЗлСрМ 750-125 (ZlSrM 75-12,5)
- ЗлСрМ 900-40 (ZlSrM 90-4)
- ЗлСрМ 930-45 (ZlSrM 93-4,5)
- ЗлСрМ 958-20 (ZlSrM 95,8-2)
- ЗлСрМ 950-25 (ZlSrM 95-2,5)
- ЗлСрМ 960-30 (ZlSrM 96-3)
- ЗлСрМ 970-20 (ZlSrM 97-2)
- ЗлСрМ 980-15 (ZlSrM 98-1,5)
- ЗлСрМ 990-5 (ZlSrM 99-0,5)
- ZlSrMgN 2-97
- ZlSrNcM 750-7,5-2,5
- ZlSrPd 585-285-160
- ZlSrPdKd 585-287-100
- ZlSrPdM 375
-
Iridium, iridium alloys
-
Osmium, osmium alloys
-
Palladium jewelry
-
Palladium, palladium alloys
- Пд99.8 ГОСТ 13462-79 (PD 99.8)
- Пд99.9 (PD 99.9)
- Пд 99.8 (Pd99.8)
- Пд 99.9 (Pd99.9)
- ПдА-0 (PDA-0)
- ПдА-1 (PdA-1)
- ПдА-2 (PDA-2)
- Pdab-0
- Pdab-1
- Pdab-2
- ПдАП-0 (PdAP-0)
- ПдАП-1 (PdAP-1)
- ПдАП-2 (PdAP-2)
- ПдИ-18 (PDI 82-18)
- ПдИ-10 (PDI 90-10)
- PDI 900-100
- PDI 950-50
- ПдИ 90-10 (PDI-10)
- ПдИ 82-18 (PDI-18)
- PdINM 900-5
- PDINM 950-2,5
- PDKin 950-4
- PDKM 850-10
- PDKM 850-7,5
- PDKM 900-5
- PDKM 950-3
- PdKNCInM 950-2-0,5-0,5
- PDM 850
- PDMKr 850-12
- PDMKr 900-8,5
- PdNcinm 850-3,5-1-0,5
- PdNCinM 900-3,5-0,8-0,5
- PdNcinm 900-4,5-2-1
- PDNCM 850-4-1,5
- PDNH 990--0,6
- PDRE 950
- PDRu 950-50
- PDRuIt 990-5
- ПдСрН-45−5 (PDSR 500-450)
- ПдСр-40 (Pdsr 60-40)
- ПдСр-20 (PdSr 80-20)
- PDSr 900-100
- ПдСр 80-20 (PdSr-20)
- ПдСр 70-30 (PdSr-30)
- PdSr-40
- ПдСрК-35-5 (PDSrK 60-35)
- ПдСрК 60-35 (PdSrK-35-5)
- PDSrKGa 950-35-0,8
- PdSrKrCM 500-305-0,8-0,3
- ПдСрМ-36-4 (PDSrM 60-36)
- PDSrM 950-25
- PdSrM-36-4
- ПдВ 80-20 (PDV-20)
- PDVit 990-0,5
- Pl99.93
- ПдСр-30 (Sdsr 70-30)
-
Platinum jewelery
-
Platinum, platinum alloy
- ПлИ-15 (PL85-15)
- PL90-10
- ПлРд-2 (PL9898-2)
- Pl99.8
- Pl99.9
- Пл999.8 (Pla 0)
- ПлАП-00 (Pla 00)
- ПлАП-1 (Pla-1)
- ПлАП-2 (PLA-2)
- ПлРу-10 (Plan 90-10)
- PlAP-0
- ПлРд-40 (PLD60-40)
- ПлРд-30 (PLD70-30)
- ПлРд-20 (PLD80-20)
- ПлРд-7.5 (PLD92.5-7.5)
- PLD95-5
- ПлИ-30 (PLI70-30)
- ПлИ-25 (PLI75-25)
- ПлИ-20 (PLI80-20)
- ПлИ-17.5 (PLI82.5-17.5)
- PLI95-5
- ПлМ-8.5 (PLM91.5)
- ПлМ-2.5 (PLM97.5)
- ПлН-4.5 (PLN95.5)
- ПлПд-20 (PLPd80-20)
- ПлПд-15 (PLPd85-15)
- ПлПд-10 (PLPd90-10)
- ПлПдРд-4-3.5 (PLPdRd92.5-4-3.5)
- ПлПдРдРУ-15-3.5-0.5 (Plpdrdru81-15-3.5-0.5)
- ПлРд-7 (PLR9393)
- ПлРд-10 (PLRd90-10)
- ПлРу-8 (PLRu92-8)
- ПлРд 90-10 (PR-10)
- ПлРд 87-13 (PR-13)
- PR-30
- ПлРд 94-6 (PR-6)
-
Rhodium, rhodium alloys
-
Ruthenium, Ruthenium Alloys
-
Silver
-
Silver solders
-
Silver, silver alloys
- СрМ87.5 (CpM875)
- СрМ 92.5 (CpM925)
- Pd 250
- Pd190
- СрМ 500 (SrM50)
- СрМ 750 (SrM75)
- СрМ 770 (SrM77)
- СрМ 800 (SrM80)
- СрМ80 (SrM800)
- СрМ83 (SrM830)
- СрМ875 (SrM87.5)
- СрМ 900 (SrM90)
- SrM91.6
- SrM92.5
- СрМ 940 (SrM94)
- СрМ 950 (SrM95)
- СрМ 960 (SrM96)
- СрМ 96 (SrM960)
- СрМ 970 (SrM97)
- СрПд-40 (SrPd60-40)
- СрПд-30 (SrPd70-30)
- СрПд-20 (SrPd80-20)
- СрПдМ-30-20 (SrPdM50-30)
- СрПл-12 (SrPl88-12)
- СрПл-4 (SrPl96-4)
-
-
Precision alloys
-
Magnetic Hard Precision Alloys
- 35KF10N
- 52K10F
- 52K11F
- 52K12F
- 52K13F
- 52КФ5 (52K5F)
- 52КФ7 (52K7F)
- 52КФ9 (52K9F)
- 52K9F-SG
- 52KF11
- 52К5Ф (52KF5)
- 52К7Ф (52KF7)
- 52К9Ф (52KF9)
- 52К13Ф (52KFA)
- 52К12Ф (52KFB)
- 52KFTM
- 52К11Ф (52KFV)
- Alloy 35KH6F
- EB6
- EH3
- EH5K5
- EH9K15M2
- Alloy 25KF14N
- Alloy 35KH8F
- Alloy 35KH4F
- Alloy 25KFN14
- Alloy 26H15KMT
- UHCI
- UNDC
- UNTSO
- YUNDCH
- YUNDKBA
- YUNDKT5
- YUNDKT5AA
- YUNDKT5BA
- YUNDKT8
-
Precision alloys superconducting
-
Soft Magnetic Precision Alloys
- 16X
- 34H2X
- Сплав 34НВМП (34NKM)
- Сплав ЭП255 (34NVMP)
- ЭП318 (Alloy 40N)
- 47NK
- 47NKH
- ЭП207 (49K2F)
- 49K2FA
- 49KF
- 49KF-VI
- 49KF2-VI
- 49KFA
- 49KFC
- ЭИ676 (50H)
- 50HNS
- 50NHS
- пермаллой (50NP)
- 65Н (64n)
- 68НМП (68NM)
- 68NMP
- 74NMD
- 76NHD
- ЭП233 (77NMD)
- 77NMDP
- ЭП252 (78N)
- 79N3M
- 79НМП (79NM)
- 79NMP
- 80MNP-VI
- 80N2M
- 80NH15R
- 80NHS
- ЭП265 (80NM)
- 80NMV
- 80NMVH3
- 81NMA
- 83NF
- 83NF-W
- 34NKMP
- 33НКМС (EP61)
- K50F2
- Сплавы ПН80Х7СР и ПХН7СР (Alloy 30NGHKR)
- Alloy 30HGTUM
- Alloy 31NX3G2
- Alloy 45N
- Alloy 27KH
- Alloy 35NKHSP
- Alloy 32N14K
- Alloy 40NKM
- Alloy 30NK
- Alloy 30NKF
- Alloy 30NG
- Steel 36KNM
-
Thermobimetals
-
With given TCLE
- ЭП139 (33NK)
- 34NK
- 36Н-ВИ (36H)
- 38НКД-ВИ (38NKD)
- 47N3H
- 47НД-ВИ (47ND)
- ЭИ677 (47NH)
- 47NHR
- 48NH
- 52H
- 52N-VI
- 56DGNH
- 58N
- 58N-EL
- 58n-VI
- 32NK-EL
- Сплав 32НКА (32NK)
- Сплав ЭП475 (32NKA)
- ЭИ630А (32NKD)
- Сплав ЭП547 (33NH3)
- 33H2X
- 33NK-VI
- 33 NKGD
- Сплав ЭП546 (32НХ3)
- 42Н-ВИ (Alloy 42H)
- 33N5X
- Alloy 36HX
- Kovar
- Alloy 35NKT
- Alloy 39H
- Сплав ЭК33 (Alloy 25X15KYUBF)
- Сплав ВУС-15 (Alloy 29KNBVTU)
- Alloy 29KNBVTU-VI
- 29НК-ВИ (Alloy 29NK)
- Alloy 29NK-VI
- Alloy 30K4M-VI
- 30НКД-ВИ (Alloy 30NKD)
- Alloy 31N3X
- Alloy 31N4X
- Alloy 31N6X
- Alloy 31N8X
- Alloy 31NX3G
- Alloy 31NK
- Alloy 42NA-VI
-
With high electrical resistance
-
With preset elastic properties
- 17HNGT
- ЭП578 (68NHVKTYU)
- 68NHVKTYU-VI
- ЭИ996М (95NLM-VI)
- ЭИ996В (95NLVF-VI)
- ЭИ996 (97NL)
- Сплав ЭИ674 (33Nude)
- ЭП52 (Alloy 36NHTYU8M)
- Alloy 42NHTY
- Alloy 36NHTYU5M
- Alloy 40KNHMVTYU
- Alloy 40KHNM
- ЭИ702 (Alloy 36NHTY)
- Alloy / surfacing powder 43NKTU
- Alloy 25N10GHTY
- Alloy 29N26KHBTY
- Alloy 30N25KTYU
- Alloy 42NHTUA
- Alloy 44NHTY
- Alloy 30NVKH
-
-
Rare earth metals and their alloys
-
Refractory metals, carbide
-
Beryllium
-
Chromium metal
-
Germanium
-
Hafnium iodide
-
Hard sintered alloys
- ВК11В (BK11-B)
- ВК11ВК (BK11-VC)
- BK3
- ВК3М (BK3-M)
- ВП3325 (BK8)
- ВК8В (BK8-In)
- ВК8ВК (BK8-VC)
- T14K8
- T15K6
- T30K4
- T5K10
- T8K7
- ТТ10К8-Б (TT10K8B)
- TT20K9
- ВП1255 (TT7K12)
- TT8K6
- VK10
- ВК10ХОМ (VK10-HOM)
- ВК10КС (VK10-KS)
- VK15
- VK20
- ВК20КС (VK20-KS)
- ВК4В (VK4-In)
- ВП3115 (VK6)
- ВК6В (VK6-In)
- ВК6М (VK6-M)
- ВК6ОМ (VK6-OM)
-
Hard Sintered Tungsten Free Alloys
-
Molybdenum
-
Niobium
-
Pressure treated vanadium
-
Rhenium, alloys with rhenium
-
Tantalum
-
Tellurium
-
Tungsten
-
Zirconium iodide
-
Zirconium wrought
-
-
Steels and alloys for castings
-
Ordinary steel for castings
- 03N12H5M3TL
- 03N12H5M3TYUL
- 07H18N10G2S2M2L
- ВНЛ-4 (07H21N9S2ML)
- ВКЛ-1 (07H24N8M2D3L)
- 08G2DNFL
- 08GDNFL
- 08H12N4GSML
- ВНЛ-3 (08H14N5M2DL)
- 5Х17Н34В5Т3Ю2Л (08H17N34V5T3YU2L)
- Г13Л (110G13L)
- 120G13H2BL
- 12DHN1MFL
- 12DN2FL
- 12H7G3SL
- 13HNDFTL
- 13NDFTL
- 14H2GMRL
- 15GL
- 15GNL
- 15HL
- 15L
- 20DHL
- 20FL
- 20ГФЛ (20G1FL)
- 20GL
- 20GNMFL
- 20GNMYUL
- 20GSL
- 20HGSFL
- 20HGSNDML
- 20HMFL
- 20HML
- 20L
- 23HGS2MFL
- 25GSL
- 25H2G2FL
- 25H2GNMFL
- 25H2NML
- 25HGL
- 25L
- 27H5GSML
- 30GL
- 30GSL
- 30H3S3GML
- 5МФРЛ (30HG1)
- 30HGFRL
- 30HGSFL
- 30HL
- 30HML
- 30HNML
- 30L
- 32H06L
- 35GL
- 35ХГФ (35HGFL)
- 35HGL
- 35HGSL
- 35HMFL
- 35HML
- 35HN2ML
- 35HNL
- 35L
- 35NGML
- 5ФЛ (40G1)
- 40GTL
- 40HFL
- 40HL
- 40HML
- 40HN2L
- 40HNL
- 40L
- 45FL
- 45GL
- 45L
- 50HGL
- 50L
- 55l
- 55SL
- 60HGL
- 70GL
- 70H2GL
- 75HNMFL
- 80GSL
-
Steel for casting with special properties
- 07H17N16TL
- 5Х18Н9Л (07H18N9L)
- ВНЛ-1 (08H14N7ML)
- 08H14NDL
- 08H15N4DML
- 08H17N34V5T3YU2RL
- 10Х16Н4БЛ (09H16N4BL)
- 10Х17Н3СЛ (09H17N3SL)
- 0Х12НДЛ (10H12NDL)
- ВНЛ-2 (10H14N5M2L)
- 5Х14НДЛ (10H14NDL)
- ЭИ402МЛ (10H17N10G4MBL)
- 5Х18Н11БЛ (10H18N11BL)
- 0Х18Н3Г3Д2Л (10H18N3G3D2L)
- Х18Н9БЛ (10H18N9BL)
- 10H18N9L
- 110G13FTL
- 110G13H2BRL
- 110G13HBRL
- 120G10FL
- 10Х18Н12БЛ (12H18N12BL)
- 12H18N12M3TL
- 10Х18Н9ТЛ (12H18N9TL)
- 12H19N7G2SAL
- 12H21N5G2SAL
- 12H21N5G2SL
- 12H21N5G2SM2L
- 12H21N5G2STL
- 10Х25Н5ТМФЛ (12H25N5TMFL)
- 12HGFL
- 130G14HMFAL
- ЭИ961Л (13H11N2V2MFL)
- 513Л (13H14N3V2FRL)
- ЭИ268Л (14H17N2L)
- 10Х18Н4Г4Л (14H18N4G4L)
- 10Х13Л (15H13L)
- 15H14NL
- 15H18N10G2S2M2L
- 15H18N10G2S2M2TL
- 15H18N12S4L
- ЭИ654Л (15H18N12S4TYUL)
- 15H18N22V6M2L
- 15H18N22V6M2RL
- 15H23N18L
- ЭИ654ЛК (16H18N12S4TYUL)
- 20FTL
- 20H12VNMFL
- 20H13L
- 20H20N14S2L
- 20H21N46V8L
- Steel 20H21N46V8RL
- 20H5ML
- 20H5TL
- 20H8VL
- 27ХГСНМДТЛА (27HGSNMDTL)
- 27HN2MFL
- 30HG2STL
- ЭИ572Л (31H19N9MVBTL)
- 40H9S2L
- 45H17G13N3YUL
- 55H18G14S2TL
- Р6М5Л (85H4M5F2V6L)
- Р6М4Ф2Л (90H4M4F2V6L)
- Steel 15X25TL
- 30Х24Н12СЛ (Steel 40X24N12SL)
- 15Х25Н19СЛ (Steel 18Х25Н19СЛ)
- 15Х25Н19С2Л (Steel 20Х25Н19С2)
- 25Х23Н7СЛ (Steel 35X23H7SL)
- 30Х18Н24С2Л (Steel 35X18H24S2L)
-
-
Steels for special purposes
-
Steel for building structures
-
Steel for rail transport
- 1
- 76F
- 76T
- М76Ц (76TS)
- A1
- A2
- A3
- A4
- Alloy 2
- Alloy 3
- Alloy 63
- Alloy 76
- E76
- E76F
- Сталь 76Т (E76T)
- E78HSF
- E86F
- H50
- 63 (K63)
- K76
- K76F
- K76T
- K78HSF
- K86F
- Сталь 54 (M54)
- Сталь 68 (M68)
- Сталь 73Т (M73T)
- Сталь 73Ц (M73TS)
- Сталь 73В (M73V)
- Сталь 74 (M74)
- Сталь 74Т (M74T)
- Сталь 74Ц (M74TS)
- Сталь 76 (M76)
- M76F
- M76T
- Сталь 76Ц (M76TS)
- Сталь 76В (M76V)
- Сталь 76ВТ (M76VT)
- operating system
- PT70
- StalGOST5257-98
- T60
-
Steels for shipbuilding
- A
- A27S
- A27SW
- A27SZ25
- A27SZ35
- A32
- A32W
- A32Z25
- A32Z35
- A36
- A36W
- A36Z25
- A36Z35
- A40
- A40S
- A40SW
- A40W
- A40Z25
- A40Z35
- AT
- BW
- BZ25
- BZ35
- D
- D27S
- D27SW
- D27SZ25
- D27SZ35
- D32
- D32W
- D32Z25
- D32Z35
- D36
- D36W
- D36Z25
- D36Z35
- D40
- D40S
- D40SW
- D40W
- D40Z25
- D40Z35
- D460W
- D500W
- DW
- DZ35
- E
- E27S
- E27SW
- E27SZ25
- E27SZ35
- E32
- E32W
- E32Z25
- E32Z35
- E36
- E36W
- E36Z25
- E36Z35
- E40
- E40S
- E40SW
- E40W
- E40Z25
- E40Z35
- E460W
- E500W
- EW
- EZ25
- EZ35
- F32W
- F36SW
- F36W
- F40SW
- F40W
- F460W
- F500W
- FW
-
-
Structural steel
-
Alloyed structural steel
- 05G4MNF
- 06H1
- 06HF
- 08GDNF
- 08ХМЧ (08HMCHA)
- 08ХМФЧ (08HMFCHA)
- 09ГСФА (09GSF)
- 09СФ (09SFA)
- 10G2
- 10G2A
- 10Х2ГНМА (10H2GNM)
- 10Х2М-ВД (10H2M)
- 12G2
- 12Х2М-ВД (12H2M)
- 12H2NM1FA
- 12H2NMFA
- ЭИ712 (12H2NVFA)
- ЭИ712М (12H2NVFMA)
- 12HN
- 12HN2
- 12HN2A
- 12HN2MDF
- 12HN3A
- 12HNVFA
- ЭИ83 (12Kh2N4A)
- 13ХФ (13HFA)
- 13N2HA
- 13N5A
- 14H2GMR
- 14H2N3MA
- 14HGN
- 15Г1 (15G)
- 15H2GN2TA
- 15H2GN2TRA
- 15HA
- 15ХФА (15HF)
- 15ХФ (15HFA)
- 15ХГНТА (15HGN2TA)
- 15ХМФ (15HMFA)
- 15НМ (15N2M)
- 15X
- 16G2
- ЭИ274 (16HGTA)
- 16HSN
- 18Х2Н4ВА (18H2N4MA)
- 18X2H4MA (18H2N4VA)
- 18HG
- 18HGT
- 19H2NMFA
- ЭИ763 (19H2NVFA)
- 19HGN
- 20ФА (20F)
- 20Ф (20FA)
- 20G
- 20G2
- ЭИ429 (20H12N12G6)
- 20H14
- 20H17N3M
- 20H2N4A
- 20ХФА (20HF)
- 20ХФ (20HFA)
- 20HGNM
- 20HGNR
- 20HGNTR
- 20HGR
- 20HGSA
- 20HM
- 20HN
- 20ХНМ (20HN2M)
- 20HN3A
- 20ХН3МФ (20HN3MFA)
- 20HN4FA
- 20HNR
- 20НМ (20N2M)
- 20X
- 20ЮЧА (20YUCH)
- 20ЮЧ (20YUCHA)
- 21H2NMFA
- ЭИ712К (21H2NVFA)
- 22HNM
- 23G2D
- 23H2NMFA
- ЭИ659 (23H2NVFA)
- 25G
- 25H2GNTA
- 25H2N4MA
- 25Х2Н4МА (25H2N4VA)
- 25HGM
- 25ХГНМТА (25HGNMT)
- 25HGSA
- 25HGT
- 27HGR
- 28HG2TR
- 30G
- 30G2
- 30H10G10T
- 30H2NMA
- 30Х2НМФ (30H2NMFA)
- 30H2NVA
- 30H2NVFA
- 30H3MA
- 30H3MF
- 30Х3ВА-Ш (30H3VA)
- 30H5
- 30ХГСА (30HGS)
- 30ХГСНА (30HGSN2A)
- 30ХГСН2МА (30HGSN2MA-VD)
- 30HGSNMA
- 30HGT
- 30ХНМА (30HN2MA)
- 30ХН2ВФА (30HN2MFA)
- 30HN2VA
- 30ХН2МФА (30HN2VFA)
- 30HN3A
- 30ХН3М2Ф (30HN3M2FA)
- 30HRA
- 30ХГС (30KhGSA)
- 30X
- 32G2M
- 32G2S
- 32Г2
- 33HS
- 34ХМА (34HM)
- 34ХН1МА (34HN1M)
- 34ХН1М (34HN1MA)
- 34HN3M
- 0ХН3М (34HN3MA)
- 35g
- 35G2
- 35G2F
- 35G2FA
- 35HG2
- 35ХГФЛ (35HGF)
- 35HGN2
- 35HGSA
- 35HMFA
- 35HN1M2FA
- 35X
- 36G2S
- 36G2SR
- 36ХН1МФА (36H2N2MFA)
- 37G2S
- 37HN3A
- 38G2MF
- 38GST
- 38ХНМА (38H2N2MA)
- 38H2N2VA
- 38H2N3M
- 38H2NM
- 38H2NMF
- 38ХЮ (38H2YU)
- 38HA
- 38HGM
- 38HGN
- 38HGNM
- 42ХМ (38HM)
- 38HMA
- 38HN3MA
- ОХН3МФА (38HN3MFA)
- 38HN3VA
- 38HNM
- 38HS
- 38HV
- 40g
- 40G2
- 40gr
- 40H2G2M
- 40Х1НВА (40H2N2MA)
- 40H2N2VA
- 40H3G2MF
- 40ХФ (40HFA)
- 40HGNM
- 40HGTR
- 40ХМФ (40HMFA)
- 40ХНМА (40HN2MA)
- ЭИ643-ВД (40HN2SMA-VD)
- 40ХНВА (40HN2VA)
- 40HS
- 40HSN2MA
- 40KhN
- 40X
- 45G
- 45G2
- 45H
- 45H4V3GF
- 45HN
- 45ХНМФА (45HN2MFA)
- 47GT
- 50G
- 50G2
- 50H3V10F
- 50H6FMS
- 50HN
- 50HNM
- 50X
- G13A
- H6F1
-
Bearing structural steel
-
Carbonaceous quality structural steel
-
Carbonaceous structural steel of ordinary quality
- St0
- St1
- St1kp
- St1ps
- St1sp
- ВСт2кп (St2kp)
- ВСт2пс (St2ps)
- ВСт2сп (St2sp)
- ВСт3Гпс (St3Gps)
- ВСт3Гсп (St3Gsp)
- ВСт3кп (St3kp)
- ВСт3пс (St3ps)
- ВСт3сп (St3sp)
- ВСт4кп (St4kp)
- ВСт4пс (St4ps)
- ВСт4сп (St4sp)
- St5Gps
- St5ps
- St5sp
- St6ps
- ВСт6сп (St6sp)
- Ст2кп (VSt2kp)
- Ст2пс (VSt2ps)
- Ст2сп (VSt2sp)
- Ст3Гпс (VSt3Gps)
- Ст3кп (VSt3kp)
- Ст3пс (VSt3ps)
- Ст3сп (VSt3sp)
- Ст4кп (VSt4kp)
- Ст4пс (VSt4ps)
- VSt5ps
- VSt5sp
- Ст6пс (VSt6ps)
- Ст6сп (VSt6sp)
-
Cryogenic structural steel
-
High strength high alloy structural steel
- N12K12M10TYU
- N12K12M7V7
- N12K15M10
- N12K16M12
- N12K8M3G2
- N12K8M4G2
- N13K15M10
- N13K16M10
- N15K9M5TYU
- N16K11M3T2
- N16K15V9M2
- N16K4M5T2YU
- N17K10M2V10T
- N17K11M4T2YU
- ЭП845-ИЛ (N17K12M5T)
- N18F6M3
- N18F6M6
- N18K12M3T2
- N18K12M4T2
- N18K14M5T
- N18K3M4T
- N18K4M7TS
- N18K7M5T
- N18K8M3T
- N18K8M5T
- N18K9M5T
- N8K18M14
- Steel 30H23N7SL
-
Improved machinability structural steel
-
Low alloy structural steel for welded structures
- 06G2SYU
- 06HGSYU
- 07GFB
- 07GFB-1
- 08G2S
- 08GBYU
- 08HMFCHAA
- 09 SFFS
- 10Г2 (09G2)
- 09G2D
- 09G2FB
- 09G2FB-1
- 09Г2 (09G2S)
- 09G2S-1
- 09G2SD
- 09G2SD-1
- 09GBYU
- 09Г2-1
- 09Г2Д-1
- 10G2B
- 10G2B-1
- 10G2BD
- 10G2BD-1
- 10G2FB
- 10G2FBYU
- 10G2FBYU-1
- 10G2S1
- 10G2S1D
- 10G2SB
- 10G2SFB
- 10GS2
- 10GT
- 10H2M1
- СХЛ-45 (10HGSN1D)
- 10HNDP
- 10ХСНД-Ш (10HSND)
- 12G2A
- 12G2B
- 12G2B-1
- 12G2F
- 12G2F-1
- 12G2FD-1
- 12G2S
- 12G2S-1
- 12G2SB
- 12G2SD
- 12G2SD-1
- 12G2SMF
- 12ГФ (12GF-W)
- 12GN2MFAYU
- Св-12ГС (12GS)
- 12GS-1
- 12GSB
- 12GSB
- 12GSBYU-1
- 12HGN2MFBAYU
- 12x8
- 12Г2ФД
- 13Г1С (13G1S-U)
- 13Г1СБ (13G1SB-U)
- 13G2AF
- 13GS
- 13HFU
- 14G2
- 14G2-1
- 14G2AF
- 14G2AF-1
- 14G2AFD
- 14G2AFD-1
- 14HGS
- 15Г2АФДпс (15G2AFD)
- 15G2AFD-1
- 15Г2АФД (15G2AFDps)
- 15G2SF
- 15G2SF-1
- 15G2SFD
- 15G2SFD-1
- 15GF
- 15GFD
- 15GFD-1
- 15ГС-Ш (15GS)
- 15ХСНД-Ш (15HSND)
- 15ГФ-1
- 16Д-Ш (16D)
- 16G2AF
- 16G2AF-1
- 16G2AFD
- 16G2AFD-1
- 16G2SAF
- 16G2SF
- 16GS
- 16GS-1
- 16GS-W
- 16H2GSB
- 17G1S
- 17G1S-1
- 17G1S-U
- 17G1S-U-1
- 17GS
- 17GS-1
- 18Г2АФпс (18G2AF)
- 18G2AF-1
- 18Г2АФДпс (18G2AFD)
- 18G2AFD-1
- 18Г2АФД (18G2AFDps)
- 18Г2АФ (18G2AFps)
- 18G2S
- 18Г2
- 1H2M1
- 20fyu
- 20GS
- 20GS2
- 20H2G2SR
- 20HG2T
- 20HG2TS
- 20HGS2
- 22C
- 22GYU
- 22H2G2AYU
- 22H2G2R
- 23H2G2T
- 23Х2Г2Т (23H2G2TS)
- 25G2S
- 25GS
- 25S2R
- 27GS
- 28C
- 30HS2
- 32G2Rps
- 35GS
- 6G2AF
- 80C
- Steel 20C
-
Spring-spring structural steel
-
-
Tin, lead, babity
-
calcium babbit
-
Lead
-
Lead antimony alloys
-
lead babbit
-
Tin
-
Tin babbitt
-
Tin-lead solder
- 50S
- 55S
- 60S
- POM2
- POS10
- POS30
- POS40
- POS61
- sn60pb38cu2 (POS61M)
- POS63
- POS90
- POSK2-18
- POSK50-18
- POSSu10-2
- POSSu15-2
- POSSu18-0.5
- POSSu18-2
- POSSu25-0.5
- POSSu25-2
- POSSu30-0.5
- POSSu30-2
- POSSu35-0.5
- POSSu35-2
- POSSu4-4
- POSSu4-6
- POSSu40-0.5
- POSSu40-2
- POSSu5-1
- POSSu50-0.5
- POSSu61-0.5
- POSSu8-3
- POSSu95-5
- Alloy / solder 30C
- ZHLSn20PbС
- ZHLSn25PbС
- ZHLSn30PbС
- ZHLSn35PbС
- ZHLSn40PbС
- ZHLSn45PbС
- ZHLSn50PbС
- ZHLSn55PbС
- ZHLSn60PbС
-
-
Titanium, titanium alloys
-
Foundry titanium alloys
-
Sponge titanium
-
Technical Titan
-
Wrought Titanium Alloys
- Alloy 3M
- 40 (dubl)
- 5B
- 5VB
- AT-6
- AT3
- BT20
- BT41
- Alloy 2WB
- Alloy 19B
- ET2
- ET3
- ET5
- OT4
- OT4-0
- OT4-1
- OT4-1sv
- OT4sv
- PT-1M
- PT-7Msv
- PT3V
- PT7M
- SPT-2
- TC6
- Alloy 27B
- Alloy 30BTC-VI
- Alloy 2B
- VT14
- VT15
- VT16
- VT18
- VT18U
- VT20-1sv
- VT20-2sv
- VT22
- VT22I
- VT23
- VT25U
- VT2sv
- VT3-1
- VT5
- VT5-1
- VT6
- VT6ch
- VT6S
- VT6sv
- VT8
- VT8-1
- VT8M-1
- VT9
-
-
Tool steel
-
Alloy tool steel
-
Carbon Tool Steel
-
Die tool steel
- 27H2N2M1F
- ЭП745 (2H6V8M2K8)
- 3H2N2MVF
- 3H2V8F
- 3H3M3F
- 3Х2В8Ф (40H5MF)
- 4H2NMF
- ЭИ959 (4H2V5MF)
- ЭИ2 (4H3VMF)
- ДИ22 (4H4VMFS)
- ЭП572 (4H5MF1S)
- 4Х5МФ1С (4H5MFS)
- ЭИ958 (4H5V2FS)
- 40ХСМФ (4HMFS)
- 4Х5В2ФС (4HV2S)
- ДИ32 (5H2MNF)
- ДИ23 (5H3V3MFS)
- 5ХНМ (5HGM)
- 5ХГМ (5HNM)
- 6ХВ2С (5HV2S)
- ЭИ325 (6HS)
- 6Х3ФС (6HV2S)
- 6HVG
- 8Х3 (7H3)
- ЭП472 (7HG2VM)
- 7HG2VMF
- ЭП570 (8H4V3M3F2)
- 8x3
- Х6В3ФМ (H12F1)
- Х6ВФ (H12MF)
- Х12М (H12VM)
- H12VMF
- ЭП770 (H6F4M)
- 9Х5Ф (H6VF)
- X12
- X12M
-
High speed tool steel
-
Roll tool steel
-