Ferroalloys

An alloy of iron with components such as manganese, chromium, titanium, silicon, etc. with a minimum content of impurities. It is obtained by melting ore concentrates in electric or plasma furnaces. Ferroalloys are mainly used for deoxidizing and alloying steel.