1.0037 (S235JR)
For thicknesses up to 25 mm.
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Base Steels |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|---|
| EN 10025 | > 98.031 | < 0.3 | < 1.4 | < 0.045 | < 0.17 | < 0.045 | < 0.009 |
Information on suppliers
Properties
| Property |
|---|
| Weldability In ISO/TR 20172 Group: 1.1 |
| Density: 7.86 g/cm3 |
| Note d > 16 and < 25 mm |
Analogues
| Germany | CIS, Russia, Ukraine | USA |
|---|---|---|
| St37k | Ст3пс-е | SAE 1010 |
Standards
| Standard | Description |
|---|---|
| EN 10025 | |
| DIN EN 10025:1990 |