1.0070 (E360)
Method of deoxidation — FN = boiling steel is not allowed.
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Base Steels |
Chemical composition
| Standard | Fe, % | P, % | S, % | N, % |
|---|---|---|---|---|
| EN 10025 | > 99.898 | < 0.045 | < 0.045 | < 0.012 |
Information on suppliers
Mechanical properties at 20 °C
Properties
| Property |
|---|
| Density: 7.87 g / cm3 |
Analogues
| Germany | CIS, Russia, Ukraine | USA |
|---|---|---|
| 1.0070G | Fe690 | E360 |
Standards
| Standard | Description |
|---|---|
| EN 10025 | |
| DIN 1623 Part 2 | |
| DIN EN 10025-2:2004 | |
| DIN EN 10025-2:2019 | |
| DIN EN 10025:1990 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| P | % | Phosphorus |
| S | % | Sulfur |
| N | % | Nitrogen |
Description of mechanical properties
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\sigma_{Y}$$ | $$MPa$$ | Yield strength |
| $$\sigma_{0.2}$$ | $$MPa$$ | Tensile stress required to produce a total elongation of 0.2% |
| $$\sigma _{U}$$ | $$MPa$$ | Ultimate tensile strength |
| $$\epsilon_{P (L_0 = 5.65\sqrt{S_o})}$$ | % | Elongation at break (parallel) (for L0 = 5.65√So) |