1.0161 (UZSt 37-2)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Quality Steel (General Structural Steels with Rm < 500 MPa) |
Chemical composition
| Standard |
Fe, % |
Mn, % |
P, % |
C, % |
S, % |
N, % |
| DIN 1652 Part 2 |
99.223–99.8 |
0.2–0.5 |
< 0.05 |
< 0.17 |
< 0.05 |
< 0.007 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Dichte: 7,86 g / cm³ |