1.0164
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Quality Steel (General Structural Steels with Rm < 500 MPa) |
Chemical composition
| Standard | Fe, % | Mn, % | Cu, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|---|
| DIN 5512 Part 1 | 98.873–99.55 | 0.2–0.5 | 0.25–0.35 | < 0.05 | < 0.17 | < 0.05 | < 0.007 |
Note: Depending on the content of the P: N < 0.012%
Note: For thicknesses > 16 mm: C < 0.2%
Note: Si - traces
Information on suppliers
Properties
| Property |
|---|
| Density: 7.86 g/cm3 |
Analogues
| Germany |
|---|
| UQST 37-2 Cu3 |
Standards
| Standard | Description |
|---|---|
| DIN 5512 Part 1 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mn | % | Manganese |
| Cu | % | Copper |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |