1.0169 (St 37-2 Cu3G)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Quality Steel (General Structural Steels with Rm < 500 MPa) |
Chemical composition
| Standard | Fe, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|
| DIN 5512 Part 2 | > 99.746 | < 0.04 | < 0.17 | < 0.035 | < 0.009 |
Information on suppliers
Properties
| Property |
|---|
| Density: 7.87 g / cm3 |
Analogues
| Germany |
|---|
| St 37-2 Cu 3 G |
Standards
| Standard | Description |
|---|---|
| DIN 5512 Part 2 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |