1.0203 (Ust 36)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Other Structural Steels (Not Intended for Heat Treatment with Rm < 500 MPa) |
Chemical composition
| Standard | Fe, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|
| DIN 17111 | 99.26–99.75 | 0.25–0.5 | < 0.05 | < 0.14 | < 0.05 |
Information on suppliers
Properties
| Property |
|---|
| Density: 7.86 g / cm3 |
Analogues
| Germany |
|---|
| USt 36 |
Standards
| Standard | Description |
|---|---|
| DIN 17111 |