1.0205 (RSt 36)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Other Structural Steels (Not Intended for Heat Treatment with Rm < 500 MPa) |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
P, % |
C, % |
S, % |
| DIN 17111 |
98.96–99.75 |
< 0.3 |
0.25–0.5 |
< 0.05 |
< 0.14 |
< 0.05 |
Information on suppliers
Properties
| Property |
| Density: 7.85 g / cm3 |
Analogues
| Germany |
CIS, Russia, Ukraine |
| QSt 36-3 |
C10C |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |