1.0239
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Other Structural Steels (Not Intended for Heat Treatment with Rm < 500 MPa) |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
P, % |
C, % |
S, % |
| DIN EN 10346:2015 |
> 97.355 |
< 0.6 |
< 1.7 |
< 0.1 |
< 0.2 |
< 0.045 |
Information on suppliers
Properties
| Property |
| According to EN 10346 Thickness: < 0.35 mm ; yield strength: > 420 MPa |
| According to EN 10346 Thickness: < 0.35 mm ; tensile strength: > 480 MPa |
| According to EN 10346 Thickness: < 0.35 mm ; elongation: > 8 % |
| According to EN 10346 Thickness: 0.35 - 0.50 mm ; yield strength: > 420 MPa |
| According to EN 10346 Thickness: 0.35 - 0.50 mm ; tensile strength: > 480 MPa |
| According to EN 10346 Thickness: 0.35 - 0.50 mm ; elongation: > 11 % |
| According to EN 10346 Thickness: 0.5 - 0.7 mm ; yield strength: > 420 MPa |
| According to EN 10346 Thickness: 0.5 - 0.7 mm ; tensile strength: > 480 MPa |
| According to EN 10346 Thickness: 0.5 - 0.7 mm ; elongation: > 13 % |
| According to EN 10346 Thickness: > 0.7 mm ; yield strength: > 420 MPa |
| According to EN 10346 Thickness: > 0.7 mm ; tensile strength: > 480 MPa |
| According to EN 10346 Thickness: > 0.7 mm ; elongation: > 15 % |
| Density: 7.83 g / cm3 |
Analogues
| Germany |
CIS, Russia, Ukraine |
USA |
| S420GD |
420 |
A 792 SS Grade 60 [410] |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |