1.0300 (C4D)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Steels with Average C < 0,12% or Rm < 400 MPa |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| EN 10016-2 |
98.16–99.7 |
< 0.3 |
0.3–0.6 |
< 0.2 |
< 0.3 |
< 0.25 |
< 0.01 |
< 0.035 |
< 0.06 |
< 0.035 |
< 0.05 |
Information on suppliers
Eigenschaften
| Eigenschaft |
| Nach EN 10016-2 Hinweis Mechanische Eigenschaften: nach Vereinbarung |
| Dichte: 7,86 g / cm³ |
Analogues
| Germany |
CIS, Russia, Ukraine |
| C4D |
C4D |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |