1.0327 (St24)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Steels with Average C < 0,12% or Rm < 400 MPa |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Al, % |
P, % |
C, % |
S, % |
|
> 99.35 |
< 0.1 |
< 0.4 |
< 0.02 |
< 0.025 |
< 0.08 |
< 0.025 |
Information on suppliers
Properties
| Property |
| Density: 7.86 g / cm3 |
Analogues
| Germany |
CIS, Russia, Ukraine |
USA |
| DD 13 |
SAE 1006 |
SAE 1006 |