1.0344 (St12Cu3)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Steels with Average C < 0,12% or Rm < 400 MPa |
Chemical composition
| Standard |
Fe, % |
Mn, % |
Cu, % |
P, % |
C, % |
S, % |
N, % |
| DIN 5512 Part 2 |
98.992–99.55 |
0.2–0.45 |
0.25–0.35 |
< 0.05 |
< 0.1 |
< 0.05 |
< 0.008 |
Information on suppliers
Свойства
| Свойство |
| Плотность: 7.87 г/см3 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| N |
% |
Nitrogen |