1.0375
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Steels with Average C < 0,12% or Rm < 400 MPa |
Chemical composition
| Standard |
Fe, % |
Si, % |
Sn, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Al, % |
As, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
|
99.112–99.76 |
< 0.03 |
< 0.02 |
0.18–0.35 |
< 0.08 |
< 0.08 |
< 0.08 |
0.02–0.08 |
< 0.02 |
< 0.02 |
0.04–0.08 |
< 0.02 |
< 0.02 |
< 0.008 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{0.2}$$, $$MPa$$ |
Treatment |
|
|
|
|
|
375 |
275 |
|
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Sn |
% |
Tin |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{0.2}$$ |
$$MPa$$ |
Tensile stress required to produce a total elongation of 0.2% |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |