1.0428 (BSt420S)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Steels with Average 0,12% =< C < 0,25% or 400 MPa = < Rm < 500 MPa |
Chemical composition
| Standard | Fe, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|
| > 99.668 | < 0.05 | < 0.22 | < 0.05 | < 0.012 |
Information on suppliers
Analogues
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |