1.0436 (P305GH)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Steels with Average 0,12% =< C < 0,25% or 400 MPa = < Rm < 500 MPa |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
P, % |
C, % |
S, % |
| EN 10222-2 |
97.76–98.95 |
< 0.4 |
0.9–1.6 |
< 0.025 |
0.15–0.2 |
< 0.015 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
$$\epsilon_L$$, % |
$$\epsilon_T$$, % |
$$KV_{L}$$, $$J$$ |
$$KV_{T}$$, $$J$$ |
Treatment |
|
|
|
|
normalization |
490–610 |
280–305 |
|
|
|
|
|
|
|
|
|
moderate hardening |
510–630 |
285 |
|
|
|
|
|
|
|
|
|
|
|
|
22 |
20 |
48 |
27 |
|
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_L$$ |
% |
Elongation at break (longitudinal) |
| $$\epsilon_T$$ |
% |
Elongation at break (transverse) |
| $$KV_{L}$$ |
$$J$$ |
Impact energy (longitudinal) |
| $$KV_{T}$$ |
$$J$$ |
Impact energy (transverse) |