1.0537 (C55Pb)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Steels with Average 0,25% =< C < 0,55% or 500 MPa =< Rm < 700 MPa |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Pb, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| 97.71–98.73 | < 0.4 | 0.6–0.9 | 0.15–0.3 | < 0.045 | 0.52–0.6 | < 0.045 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Pb | % | Lead |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |