1.0574 (H460)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Steels with Average 0,25% =< C < 0,55% or 500 MPa =< Rm < 700 MPa |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Ti, % | Al, % | P, % | C, % | S, % | Nb, % |
|---|---|---|---|---|---|---|---|---|---|
| > 97.015 | < 0.7 | < 1.8 | < 0.22 | < 0.015 | < 0.03 | < 0.1 | < 0.03 | < 0.09 |