1.0584 (GL-D36)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Steels | Steels with Average 0,25% =< C < 0,55% or 500 MPa =< Rm < 700 MPa |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Cu, % | Ni, % | V, % | Al, % | P, % | C, % | S, % | Nb, % | Mo, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 96.44–99.03 | < 0.5 | 0.9–1.6 | < 0.2 | < 0.35 | < 0.4 | 0.05–0.1 | < 0.02 | < 0.04 | < 0.18 | < 0.04 | 0.02–0.05 | < 0.08 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Cu | % | Copper |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| Mo | % | Molybdenum |