1.0588 (C52D)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Steels |
Steels with Average 0,25% =< C < 0,55% or 500 MPa =< Rm < 700 MPa |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| EN 10016-2 |
97.62–98.9 |
0.1–0.3 |
0.5–0.8 |
< 0.15 |
< 0.25 |
< 0.2 |
< 0.01 |
< 0.035 |
0.5–0.55 |
< 0.035 |
< 0.05 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |