1.0965 (S900MC)
Classification
| Country |
Section |
Category |
| Germany |
Alloy Steels |
Steels for Other Applications |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
V, % |
Al, % |
P, % |
C, % |
S, % |
|
> 94.65 |
< 0.8 |
< 0.005 |
< 2 |
< 0.22 |
< 2 |
< 0.06 |
< 0.25 |
< 0.015 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{0.2}$$, $$MPa$$ |
$$\epsilon_{L (L_0 = 80 mm)}$$, % |
Treatment |
|
|
|
|
|
1200 |
900–1150 |
5 |
|
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma_{0.2}$$ |
$$MPa$$ |
Tensile stress required to produce a total elongation of 0.2% |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\epsilon_{L (L_0 = 80 mm)}$$ |
% |
Elongation at break (longitudinal) (for L0 = 80 mm) |