1.0967 (S940MC)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Alloy Steels | Steels for Other Applications |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| > 95.77 | < 0.8 | < 2.2 | < 1 | < 0.015 | < 0.025 | < 0.18 | < 0.01 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |