1.1004 (C2E)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Special Steels | Steels with Special Physical Properties |
Chemical composition
| Standard | Fe, % | Mn, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|
| 99.54–99.95 | < 0.2 | 0.05–0.15 | < 0.035 | < 0.04 | < 0.035 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Mn | % | Manganese |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |