1.1011 (RFe160)
Classification
| Country | Section | Category |
|---|---|---|
| Germany | Non-alloy Special Steels | Steels with Special Physical Properties |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Al, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|
| 98.45–99.28 | < 0.1 | 0.5–0.9 | 0.04–0.1 | < 0.08 | < 0.1 | 0.18–0.27 |
Information on suppliers
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |