1.1152 (Cq22)
Classification
| Country |
Section |
Category |
| Germany |
Non-alloy Special Steels |
Structural Pressure Vessel and Engineering Steels with C < 0,5% |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cu, % |
P, % |
C, % |
S, % |
| EN 10263-3 |
98.58–99.52 |
< 0.3 |
0.3–0.6 |
< 0.25 |
< 0.025 |
0.18–0.22 |
< 0.025 |
Information on suppliers
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\psi$$, % |
Treatment |
|
|
|
|
|
450–640 |
56–67 |
|
Analogues
| CIS, Russia, Ukraine |
| 20kp |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
| $$\psi$$ |
% |
Reduction in cross section on fracture |